静水压力对金属腐蚀热力学及动力学的影响 |
马荣耀1,2, 赵林1, 王长罡1, 穆鑫1, 魏欣1, 董俊华1, 柯伟1 |
1 中国科学院金属研究所 沈阳 110016 2 中国科学院大学 北京 100049 |
|
Influence of Hydrostatic Pressure on the Thermodynamics and Kinetics of Metal Corrosion |
Rongyao MA1,2, Lin ZHAO1, Changgang WANG1, Xin MU1, Xin WEI1, Junhua DONG1, Wei KE1 |
1 Institute of Metal Research, Chinese Academy of Sciences, Shenyang 110016, China 2 University of Chinese Academy of Sciences, Beijing 100049, China |
引用本文:
马荣耀, 赵林, 王长罡, 穆鑫, 魏欣, 董俊华, 柯伟. 静水压力对金属腐蚀热力学及动力学的影响[J]. 金属学报, 2019, 55(2): 281-290.
Rongyao MA,
Lin ZHAO,
Changgang WANG,
Xin MU,
Xin WEI,
Junhua DONG,
Wei KE.
Influence of Hydrostatic Pressure on the Thermodynamics and Kinetics of Metal Corrosion[J]. Acta Metall Sin, 2019, 55(2): 281-290.
[1] | Zhou J L, Li X G, Cheng X Q, et al.Research progress on corrosion of metallic materials in deep sea environment[J]. Corros. Sci. Prot. Technol., 2010, 22: 47(周建龙, 李晓刚, 程学群等. 深海环境下金属及合金材料腐蚀研究进展[J]. 腐蚀科学与防护技术, 2010, 22: 47) | [2] | Fan L, Ding K K, Guo W M, et al.Effect of hydrostatic pressure and pre-stress on corrosion behavior of a new type Ni-Cr-Mo-V high strength steel[J]. Acta Metal. Sin., 2016, 52: 679(范林, 丁康康, 郭为民等. 静水压力和预应力对新型Ni-Cr-Mo-V高强钢腐蚀行为的影响[J]. 金属学报, 2016, 52: 679) | [3] | Liu J, Li X B, Wang J.Effect of hydrostatic pressure on the corrosion behaviors of two low alloy steels[J]. Acta Metal. Sin., 2011, 47: 695(刘杰, 李相波, 王佳. 模拟深海压力对2种低合金钢腐蚀行为的影响[J]. 金属学报, 2011, 47: 695) | [4] | Traverso P, Canepa E.A review of studies on corrosion of metals and alloys in deep-sea environment[J]. Ocean Eng., 2014, 87: 10 | [5] | Beccaria A M, Poggi G.Influence of hydrostatic pressure on pitting of aluminium in sea water[J]. Br. Corros. J., 1985, 20: 183 | [6] | Beccaria A M, Poggi G, Gingaud D, et al.Effect of hydrostatic pressure on passivating power of corrosion layers formed on 6061 T6 aluminium alloy in sea water[J]. Br. Corros. J., 1994, 29: 65 | [7] | Beccaria A M, Poggi G.Influence of hydrostatic pressure and salt concentration on aluminum corrosion in NaCl solutions[J]. Corrosion, 1986, 42: 470 | [8] | Beccaria A M, Poggi G.Aluminum corrosion in slightly alkaline sodium sulfate solutions at different hydrostatic pressures[J]. Corrosion, 1987, 43: 153 | [9] | Beccaria A M, Ltraverso P, Poggi G, et al.Effect of hydrostatic pressure on corrosion behaviour of 5086 Al-alloy in sea water[J]. High Pressure Res., 1991, 7: 347 | [10] | Beccaria A M, Poggi G.Effect of some surface treatments on kinetics of aluminium corrosion in NaCl solutions at various hydrostatic pressures[J]. Br. Corros. J., 1986, 21: 19 | [11] | Beccaria A M, Fiordiponti P, Mattogno G.The effect of hydrostatic pressure on the corrosion of nickel in slightly alkaline solutions containing Cl- ions[J]. Corros. Sci., 1989, 29: 403 | [12] | Beccaria A M, Poggi G, Arfelli M, et al.The effect of salt concentration on nickel corrosion behaviour in slightly alkaline solutions at different hydrostatic pressures[J]. Corros. Sci., 1993, 34: 989 | [13] | Beccaria A M, Poggi G, Castello G.Influence of passive film composition and sea water pressure on resistance to localised corrosion of some stainless steels in sea water[J]. Br. Corros. J., 1995, 30: 283 | [14] | Zhang T, Yang Y E, Shao Y W, et al.A stochastic analysis of the effect of hydrostatic pressure on the pit corrosion of Fe-20Cr alloy[J]. Electrochim. Acta, 2009, 54: 3915 | [15] | Liu B.Effect of hydrostatic pressure on the corrosion behavior of pure nickel [D]. Harbin: Harbin Engineering University, 2009(刘斌. 静水压力对纯镍腐蚀行为的影响 [D]. 哈尔滨: 哈尔滨工程大学, 2009) | [16] | Liu B, Cong Y, Zhang T, et al.Influence of deep-sea environment on corrosion behavior of pure nickel: Influence of hydrostatic pressures on performance of passive film on pure nickel[J]. Corros. Sci. Prot. Technol., 2009, 21: 5(刘斌, 丛园, 张涛等. 深海环境下静水压力对纯镍腐蚀行为的影响[J]. 腐蚀科学与防护技术, 2009, 21: 5) | [17] | Liu B, Zhang J, Zhang T, et al.Influence of deep-sea environment on corrosion behavior of pure nickel-II—Stochastic analysis approaches to pitting of pure nickel under hydrostatic pressures[J]. Corros. Sci. Prot. Technol., 2010, 22: 85(刘斌, 张杰, 张涛等. 深海环境对纯镍腐蚀行为的影响II—利用随机分析方法研究纯镍在静水压力下的点蚀行为[J]. 腐蚀科学与防护技术, 2010, 22: 85) | [18] | Liu B, Zhang T, Shao Y W, et al.Influence of deep-sea environment on corrosion behavior of pure nickel III—Influence of hydrostatic pressures on pitting mechanism for pure nickel[J]. Corros. Sci. Prot. Technol., 2011, 23: 239(刘斌, 张涛, 邵亚薇等. 深海环境对纯镍腐蚀行为的影响III—静水压力对纯镍点蚀机制的影响[J]. 腐蚀科学与防护技术, 2011, 23: 239) | [19] | Liu B.Effect on corrosion behavior mechanism of pure nickel and NiCrMoV steel weld joint in deep sea environment [D]. Harbin: Harbin Engineering University, 2016(刘斌. 深海环境对纯Ni及NiCrMoV钢焊接接头腐蚀行为机制的影响 [D]. 哈尔滨: 哈尔滨工程大学, 2016) | [20] | Yang Y E, Zhang T, Shao Y W, et al.Effect of hydrostatic pressure on the corrosion behaviour of Ni-Cr-Mo-V high strength steel[J]. Corros. Sci., 2010, 52: 2697 | [21] | Yang Y E, Zhang T, Shao Y W, et al.New understanding of the effect of hydrostatic pressure on the corrosion of Ni-Cr-Mo-V high strength steel[J]. Corros. Sci., 2013, 73: 250 | [22] | Sun H J, Liu L, Li Y, et al.The performance of Al-Zn-In-Mg-Ti sacrificial anode in simulated deep water environment[J]. Corros. Sci., 2013, 77: 77 | [23] | Jin K X, Zhao C J, Ma P S.Chemical Thermodynamics [M]. Tianjin: Tianjin University Press, 1990: 128(金克新, 赵传钧, 马沛生. 化工热力学 [M]. 天津: 天津大学出版社, 1990: 128) | [24] | Jing F Q.Experimental Equation of State Equation [M]. Beijing: Science Press, 1986: 3(经福谦. 实验物态方程导引 [M]. 北京: 科学出版社, 1986: 3) | [25] | Zhang Z B, Liu L S.Marine Physical Chemistry [M]. Beijing: Science Press, 1989: 55(张正斌, 刘莲生. 海洋物理化学 [M]. 北京: 科学出版社, 1989: 55) | [26] | Millero F J, Kembro A, Lo Surdo A.Adiabatic partial molal compressibilities of electrolytes in 0.725 M sodium chloride solutions at 25.degree.C[J]. J. Phys. Chem., 1980, 84: 2728 | [27] | Owen B B, Brinkley S R.Calculation of the effect of pressure upon ionic equilibria in pure water and in salt solutions[J]. Chem. Rev., 1941, 29: 461 | [28] | Millero F J, Laferriere A L, Chetirkin P V.The partial molal volumes of electrolytes in 0.725 M sodium chloride solutions at 25.degree.C[J]. J. Phys. Chem., 1977, 81: 1737 | [29] | Oriani R A.The physical and metallurgical aspects of hydrogen in metals [A]. Proceedings of 4th International Conference on Cold Fusion[C]. Lahina, Maui, USA: Electric Power Research Institute, 1994 | [30] | Wan H X, Du C W, Liu Z Y, et al.The effect of hydrogen on stress corrosion behavior of X65 steel welded joint in simulated deep sea environment[J]. Ocean Eng., 2016, 114: 216 | [31] | Wan H X, Liu Z Y, Du C W, et al.Stress corrosion behavior of X65 steel welded joint in marine environment[J]. Int. J. Electrochem. Sci., 2015, 10: 8437 | [32] | Xiong X L, Tao X, Zhou Q J, et al.Hydrostatic pressure effects on hydrogen permeation in A514 steel during galvanostatic hydrogen charging[J]. Corros. Sci., 2016, 112: 86 | [33] | Xiong X L, Zhou Q J, Li J X, et al.Cathodic over-potential and hydrogen partial pressure coupling in hydrogen evolution reaction of marine steel under hydrostatic pressure[J]. Electrochim. Acta, 2017, 247: 1019 | [34] | Chen Z X, Gu F Y, Hu W M.Chemical Thermodynamics [M]. Beijing: Chemical Industry Press, 2012: 71(陈钟秀, 顾飞燕, 胡望明.化工热力学 [M]. 北京: 化学工业出版社, 2012: 71) | [35] | Prausnitz J M, Lichtenthaler R N,de Azevedo E G.Molecular Thermodynamics of Fluid-Phase Equilibria[M]. 3rd Ed., New Jersey: Prentice Hall PTR, 1999: 589 | [36] | Zhou T L, Battino R.Partial molar volumes of 13 gases in water at 298.15 K and 303.15 K[J]. J. Chem. Eng. Data, 2001, 46: 331 | [37] | Dexter S C.Effect of variations in sea water upon the corrosion of aluminum[J]. Corrosion, 1980, 36: 423 | [38] | Horne R A.Marine Chemistry: The Structure of Water and the Chemistry of the Hydrosphere[M]. New York, London, Sydney, Toronto: John Wiley & Sons Inc, 1969: 1 | [39] | Distèche A, Distèche S.The effect of pressure on the dissociation of carbonic acid from measurements with buffered glass electrode cells[J]. J. Electrochem. Soc., 1967, 114: 330 | [40] | Cramer S D, Covino B S.Corrosion: Environments and Industries[M]. Materials Park, Ohio: ASM International, 1990: 1 | [41] | Gutman E M.Mechanochemistry of Solid Surfaces [M]. Singapore: World Scientific Publishing Co Inc, 1994: 18 | [42] | Gutman E M.Mechanochemistry of Materials [M]. London: Cambridge International Science Publishing, 1998: 67 | [43] | Morild E,O?lmheim J E.Pressure dependence of the oxygen electrode[J]. J. Electrochem. Soc., 1980, 127: 2356 | [44] | Conway B E, Currie J C.Significance of effects of high pressure on kinetics of electrode reactions: II. The nature of solvent reorganization in the activation process of an electrochemical redox reaction[J]. J. Electrochem. Soc., 1978, 125: 257 | [45] | Conway B E, Currie J C.Significance of effects of high pressure on kinetics of electrode reactions: I. Applications to transition states in hydrogen evolution reaction mechanisms[J]. J. Electrochem. Soc., 1978, 125: 252 | [46] | Conway B E, Currie J C.Significance of effects of pressure on electrode reactions. Part III. Equilibrium processes at reference electrodes and the volume of H in Pd[J]. Can. J. Chem., 1978, 56: 915 | [47] | Conway B E, Currie J C.Temperature and pressure effects on surface processes at noble metal electrodes: Part 2. Volume of adsorbed H and oxygen species at Pt and Au[J]. J. Chem. Soc., Faraday Trans. 1, 1978, 74: 1390 | [48] | Hills G J, Kinnibrugh D R.The pressure coefficient of the hydrogen electrode reaction[J]. J. Electrochem. Soc., 1966, 113: 1111 |
|
|