预变形温度对纳米贝氏体相变动力学及组织的影响 |
徐士新1,2,3( ), 余伟2, 李舒笳1, 王坤1, 孙齐松1 |
1 首钢集团有限公司技术研究院 北京 100043 2 北京科技大学工程技术研究院 北京 100083 3 首钢集团有限公司绿色可循环钢铁流程北京市重点实验室 北京 100043 |
|
Effects of Pre-Deformation Temperature on Nanobainite Transformation Kinetics and Microstructure |
Shixin XU1,2,3( ), Wei YU2, Shujia LI1, Kun WANG1, Qisong SUN1 |
1 Research Institute of Technology, Shougang Group Co., Ltd., Beijing 100043, China 2 Engineering Research Institute, University of Science and Technology Beijing, Beijing 100083, China 3 Beijing Key Laboratory of Green Recyclable Process for Iron and Steel Production, Shougang Group Co., Ltd., Beijing 100043, China |
引用本文:
徐士新, 余伟, 李舒笳, 王坤, 孙齐松. 预变形温度对纳米贝氏体相变动力学及组织的影响[J]. 金属学报, 2018, 54(8): 1113-1121.
Shixin XU,
Wei YU,
Shujia LI,
Kun WANG,
Qisong SUN.
Effects of Pre-Deformation Temperature on Nanobainite Transformation Kinetics and Microstructure[J]. Acta Metall Sin, 2018, 54(8): 1113-1121.
[1] | Caballero F G, Bhadeshia H K D H, Mawella K J A, et al. Design of novel high-strength bainitic steels: Part 1[J]. Mater. Sci. Technol., 2001, 17: 512 | [2] | Caballero F G, Bhadeshia H K D H, Mawella K J A, et al. Design of novel high-strength bainitic steels: Part 2[J]. Mater. Sci. Technol., 2001, 17: 517 | [3] | Caballero F G, Bhadeshia H K D H, Mawella K J A, et al. Very strong low temperature bainite[J]. Mater. Sci. Technol., 2002, 18: 279 | [4] | Caballero F G, Bhadeshia H K D H. Very strong bainite[J]. Curr. Opin. Solid State Mater. Sci., 2004, 8: 251 | [5] | García-Mateo C, Caballero F G, Bhadeshia H K D H. Mechanical properties of low-temperature bainite [J]. Mater. Sci. Forum, 2005, 500-501: 285 | [6] | García-Mateo C, Caballero F G, Bhadeshia H K D H. Development of hard bainite[J]. ISIJ Int., 2003, 43: 1238 | [7] | García-Mateo C, Caballero F G, Bhadeshia H K D H. Acceleration of low-temperature bainite[J]. ISIJ Int., 2003, 43: 1821 | [8] | Umemoto M, Furuhara T, Tamura I.Effects of austenitizing temperature on the kinetics of bainite reaction at constant austenite grain size in Fe-C and Fe-Ni-C alloys[J]. Acta Metall., 1986, 34: 2235 | [9] | Bhadeshia H K D H. Nanostructured bainite[J]. Proc. R. Soc., 2010, 466A: 3 | [10] | Yoozbashi M N, Yazdani S, Wang T S.Design of a new nanostructured, high-Si bainitic steel with lower cost production[J]. Mater. Des., 2011, 32: 3248 | [11] | Bhadeshia H K D H, David S A, Vitek J M, et al. Stress induced transformation to bainite in Fe-Cr-Mo-C pressure vessel steel[J]. Mater. Sci. Technol., 1991, 7: 686 | [12] | Matsuzaki A, Bhadeshia H K D H, Harade H. Stress affected bainitic transformation in a Fe-C-Si-Mn alloy[J]. Acta Metall. Mater., 1994, 42: 1081 | [13] | Shipway P H, Bhadeshia H K D H. The effect of small stresses on the kinetics of the bainite transformation[J]. Mater. Sci. Eng., 1995, A201: 143 | [14] | Xu Z Y.Effect of stress on bainitic transformation in steel[J]. Acta. Metall. Sin., 2004, 40: 113(徐祖耀. 应力对钢中贝氏体相变的影响[J]. 金属学报, 2004, 40: 113) | [15] | Gong W, Tomota Y, Koo M S, et al.Effect of ausforming on nanobainite steel[J]. Scr. Mater., 2010, 63: 819 | [16] | Gong W, Tomota Y, Adachi Y, et al.Effects of ausforming temperature on bainite transformation, microstructure and variant selection in nanobainite steel[J]. Acta Mater., 2013, 61: 4142 | [17] | Ohtsuka H.Effects of strong magnetic fields on bainitic transformation[J]. Curr. Opin. Solid State Mater. Sci., 2004, 8: 279 | [18] | Bhadeshia H K D H, Edmonds D V. The bainite transformation in a silicon steel[J]. Metall. Trans., 1979, 10A: 895 | [19] | Xu Q K.A study of the incomplete phenomenon of bainite transformation in a low carbon Fe-C-Mo alloy[J]. J. Chongqing Univ., 1987, (3): 59(徐启昆. 铁碳钼合金贝氏体转变不完全现象的研究[J]. 重庆大学学报, 1987, (3): 59) | [20] | Johnson W A, Mehl R F.Reaction kinetics in process of nucleation and growth[J]. Trans. AIME, 1939, 135: 416 | [21] | Avrami M.Kinetics of phase change. I General theory[J]. J. Chem. Phys., 1939, 7: 1103 | [22] | Avrami M.Kinetics of phase change. II Transformation-time relations for random distribution of nuclei[J]. J. Chem. Phys., 1940, 8: 212 | [23] | Avrami M.Granulation, phase change, and microstructure kinetics of phase change. III[J]. J. Chem. Phys., 1941, 9: 177 | [24] | Sidel S M, Santos F A, Gordo V O, et al.Avrami exponent of crystallization in tellurite glasses[J]. J. Therm. Anal. Calorim., 2011, 106: 613 | [25] | Quidort D, Bréchet Y J M. The role of carbon on the kinetics of bainite transformation in steels[J]. Scr. Mater., 2002, 47: 151 | [26] | Liu F, Sommer F, Mittemeijer E J.An analytical model for isothermal and isochronal transformation kinetics[J]. J. Mater. Sci., 2004, 39: 1621 | [27] | Liu F, Sommer F, Bos C, et al.Analysis of solid state phase transformation kinetics: Models and recipes[J]. Int. Mater. Rev., 2007, 54: 193 | [28] | Liu F, Sommer F, Mittemeijer E J.Analysis of the kinetics of phase transformations; roles of nucleation index and temperature dependent site saturation, and recipes for the extraction of kinetic parameters[J]. J. Mater. Sci., 2007, 42: 573 | [29] | Christian J W.The Theory of Transformations in Metals and Alloys[M]. 3rd Ed., Oxford: Elsevier Ltd., 2002: 546 | [30] | Quidort D, Brechet Y J M. A model of isothermal and non isothermal transformation kinetics of bainite in 0.5% C steels[J]. ISIJ Int., 2002, 42: 1010 | [31] | Zhang Z M, Cai Q W, Yu W, et al.Continuous cooling transformation behavior and kinetic models of transformations for an ultra-low carbon bainitic steel[J]. J. Iron Steel Res. Int., 2012, 19: 73 | [32] | Wang Q C, Yang Z G, Li Z D.A theoretical analysis on effect of deformation above Ae3 to the nucleation of proeutectoid ferrite transformation[J]. Acta. Metall. Sin., 2007, 43: 344(王启超, 杨志刚, 李昭东. Ae3温度以上变形对先共析铁素体相变形核影响的理论分析[J]. 金属学报, 2007, 43: 344) | [33] | Bhadeshia H K D H, Honeycombe R W K. Steels: Microstructure and Properties[M]. 3rd Ed., Oxford: Elsevier Ltd., 2006: 129 | [34] | Legros M, Dehm G, Arzt E, et al.Observation of giant diffusivity along dislocation cores[J]. Science, 2008, 319: 1646 | [35] | Bhadeshia H K D H. Bainite in Steels [M]. 2nd Ed., Cambridge: Cambridge University Press, 2001: 124 | [36] | Singh S B, Bhadeshia H K D H. Estimation of bainite plate-thickness in low-alloy steels[J]. Mater. Sci. Eng., 1998, A245: 72 | [37] | Hase K, Garcia-Mateo C, Bhadeshia H K D H. Bainite formation influenced by large stress[J]. Mater. Sci. Technol., 2004, 20: 1499 |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
|
Shared |
|
|
|
|
|
Discussed |
|
|
|
|