预变形对Al-Mg-Si-Cu合金时效硬化和显微结构的影响* |
顾媛,陈江华,刘春辉( ),朱东晖,刘力梅,陶冠辉 |
|
EFFECT OF PRE-DEFORMATION ON AGE- HARDENING AND MICROSTRUCTURE IN Al-Mg-Si-Cu ALLOY |
Yuan GU,Jianghua CHEN,Chunhui LIU( ),Donghui ZHU,Limei LIU,Guanhui TAO |
College of Materials Science and Engineering, Hunan University, Changsha 410082 |
引用本文:
顾媛,陈江华,刘春辉,朱东晖,刘力梅,陶冠辉. 预变形对Al-Mg-Si-Cu合金时效硬化和显微结构的影响*[J]. 金属学报, 2015, 51(11): 1400-1406.
Yuan GU,
Jianghua CHEN,
Chunhui LIU,
Donghui ZHU,
Limei LIU,
Guanhui TAO.
EFFECT OF PRE-DEFORMATION ON AGE- HARDENING AND MICROSTRUCTURE IN Al-Mg-Si-Cu ALLOY[J]. Acta Metall Sin, 2015, 51(11): 1400-1406.
[1] | Williams J C, Starke Jr E A. Acta Mater, 2003; 51: 5775 | [2] | Chen J H, Costan E, Van Huis M A, Xu Q, Zandbergen H W. Science, 2006; 312: 416 | [3] | Sabirov I, Murashkin Yu M, Valiev R Z. Mater Sci Eng, 2013; A560: 1 | [4] | Nageswara P, Jayaganthan R. Mater Des, 2012; 39: 226 | [5] | Zhang J W, Gao N, Starink M J. Mater Sci Eng, 2010; A527: 3472 | [6] | Wang Y M, Ma E. Acta Mater, 2004; 52: 1699 | [7] | Kang U G, Lee H J, Nam W J. J Mater Sci, 2012; 47: 7883 | [8] | Chen Y T, Wang D A, Uan J Y, Hsieh T H, Tsai T C. Mater Sci Eng, 2012; A551: 296 | [9] | Estrin Y, Vinogradov A. Acta Mater, 2013; 61: 782 | [10] | Liddicoat P V, Liao X Z, Zhao Y H, Zhu Y T, Murashkin M Y, Lavernia E J, Valiev R Z, Ringer S P. Nat Commun, 2010; 1: 1 | [11] | Cavaliere P. Inter J Fatigue, 2009; 31: 1476 | [12] | Yao Z Y, Liu Q, Godfrey A, Liu W. Acta Metall Sin, 2009; 45: 647 (姚宗勇, 刘 庆, Godfrey A, 刘 伟. 金属学报, 2009; 45: 647) | [13] | Eizadjou M, Manesh H D, Janghorban K. J Alloys Compd, 2009; 474: 406 | [14] | Zhao Y L, Yang Z Q, Zhang Z. Acta Mater, 2013; 61: 1624 | [15] | Djavanroodi F, Ebrahimi M, Rajabifar B, Akramizadeh S. Mater Sci Eng, 2010; A528: 745 | [16] | Rangaraju N, Raghuram T, Krishna V, Prasad R K, Venugopal P. Mater Sci Eng, 2005; A398: 246 | [17] | Cheng S, Zhao Y H, Zhu Y T, Ma E. Acta Mater, 2007; 55: 5822 | [18] | Zhao Y H, Liao X Z, Cheng S, Ma E, Zhu Y T. Adv Mater, 2006; 18: 2280 | [19] | Vaseghi M, Kim H S. Mater Des, 2012; 36: 735 | [20] | Liu C H, Li X L, Wang S H, Chen J H, Teng Q, Chen J, Gu Y. Mater Des, 2014; 54: 144 | [21] | Wang S H, Liu C H, Chen J H, Li X L, Zhu D H, Tao G H. Mater Sci Eng, 2013; A585: 233 | [22] | Engler O. Mater Sci Eng, 2012; A538: 69 | [23] | Valiev R Z, Islamgaliev R K, Alexandrov I V. Prog Mater Sci, 2000; 45: 103 | [24] | Chen J H, Liu C H. Trans Nonferrous Met Soc China, 2011; 21: 2352 (陈江华, 刘春辉. 中国有色金属学报, 2011; 21: 2352) | [25] | Li X L, Chen J H, Liu C H, Feng J N, Wang S H. Acta Metall Sin, 2013; 49: 243 (李祥亮, 陈江华, 刘春辉, 冯佳妮, 王时豪, 金属学报, 2013; 49: 243) |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
|
Shared |
|
|
|
|
|
Discussed |
|
|
|
|