| Inconel 718高温合金中析出相演变研究进展* |
刘永长( ),郭倩颖,李冲,梅云鹏,周晓胜,黄远,李会军 |
| 天津大学材料科学与工程学院水利安全与仿真国家重点实验室, 天津 300354 |
|
| RECENT PROGRESS ON EVOLUTION OF PRECIPI-TATES IN INCONEL 718 SUPERALLOY |
Yongchang LIU( ),Qianying GUO,Chong LI,Yunpeng MEI,Xiaosheng ZHOU,Yuan HUANG,Huijun LI |
| State Key Lab of Hydraulic Engineering Simulation and Safety, School of Materials Science & Engineering, Tianjin University, Tianjin 300354, China |
引用本文:
刘永长, 郭倩颖, 李冲, 梅云鹏, 周晓胜, 黄远, 李会军. Inconel 718高温合金中析出相演变研究进展*[J]. 金属学报, 2016, 52(10): 1259-1266.
Yongchang LIU,
Qianying GUO,
Chong LI,
Yunpeng MEI,
Xiaosheng ZHOU,
Yuan HUANG,
Huijun LI.
RECENT PROGRESS ON EVOLUTION OF PRECIPI-TATES IN INCONEL 718 SUPERALLOY[J]. Acta Metall Sin, 2016, 52(10): 1259-1266.
| [1] | Guan Y S, Liu E Z, Guan X R, Liu Z.J Mater Sci Technol, 2016; 32: 271 | | [2] | Dong J X, Liu X B, Tang B, Hu Y H, Xu Z C, Xie X S.Acta Metall Sin, 1996; 32: 241 | | [2] | (董建新, 刘兴博, 唐宾, 胡尧和, 徐志超, 谢锡善. 金属学报, 1996; 32: 241) | | [3] | Zhang Y W, Hu B F.Acta Metall Sin, 2015; 51: 967 | | [3] | (张义文, 胡本芙. 金属学报, 2015; 51: 967) | | [4] | Rao G A, Kumar M, Srinivas M, Sarma D S.Mater Sci Eng, 2003; A355: 114 | | [5] | Dong X M, Zhang X L, Du K, Zhou Y Z, Jin T, Ye H Q.J Mater Sci Technol, 2012; 28: 1031 | | [6] | Tiley J, Viswanathan G B, Srinivasan R, Banerjee R, Dimiduk D M, Fraser H L.Acta Mater, 2009; 57: 2538 | | [7] | Li X W, Wang L, Dong J S, Lou L H.J Mater Sci Technol, 2014; 30: 1296 | | [8] | Ma D X.Acta Metall Sin, 2015; 51: 1179 | | [8] | (马德新. 金属学报, 2015; 51: 1179) | | [9] | Liu T, Dong J S, Wang L, Li Z J, Zhou X T, Lou L H, Zhang J.J Mater Sci Technol, 2015; 31: 269 | | [10] | Xu Z H, Wang Z K, Niu J, Dai J W, He L M, Mu R D.J Alloys Compd, 2016; 676: 231 | | [11] | Bai M W, Jiang H B, Chen Y, Chen Y Q, Grovenor C, Zhao X F, Xiao P.Mater Des, 2016; 97: 364 | | [12] | Song K, Yu K, Lin X, Yang J, Hu H O, Huang W D.Acta Metall Sin, 2015; 51: 935 | | [12] | (宋衎, 喻恺, 林鑫, 杨静, 胡海鸥, 黄卫东. 金属学报, 2015; 51: 935) | | [13] | Kirman I, Warrington D H.Metall Trans, 1970; 1A: 2667 | | [14] | Zhao X B, Gu Y F, Lu J T, Yan J B, Yin H F.Rare Met Mater Eng, 2015; 44: 768 | | [14] | (赵新宝, 谷月峰, 鲁金涛, 严靖博, 尹宏飞. 稀有金属材料与工程, 2015; 44: 768) | | [15] | Wlodek S T, Field R D.In: Loria E A ed., 3rd Int Symp on Superalloys 718, 625, 706 and Various Derivatives, Pittsburgh, PA: The Minerals, Metals & Materials Society, 1994: 659 | | [16] | Sundararaman M, Mukhopadhyay P, Banerjee S.Metall Trans, 1988; 19A: 453 | | [17] | Damodaram R, Raman S G S, Satyanarayana D V V, Madhusudhan R G, Prasad R K.Mater Sci Eng, 2014; A612: 414 | | [18] | Sundararaman M, Banerjee S.Metall Mater Trans, 1992; 23A: 2015 | | [19] | Sundararaman M, Mukhopadhyay P, Banerjee S.In: Loria E A ed., 3rd Int Symp on Superalloys 718, 625, 706 and Various Derivatives, Pittsburgh, PA: The Minerals, Metals & Materials Society, 1994: 419 | | [20] | Asadian S, Wei L Y, Warren R.Mater Charact, 2004; 53: 7 | | [21] | Wang W Q.Aviat Manuf Eng, 1995; (7): 15 | | [21] | (汪文迁. 航空制造工程, 1995; (7): 15) | | [22] | Zhou X H.Forging Technol, 2004; 29(5): 9 | | [22] | (周晓虎. 锻压技术, 2004; 29(5): 9) | | [23] | Cai D Y, Zhang W H, Liu W C.Trans Nonferrous Met Soc China, 2003; 13: 1338 | | [24] | Sellars C M, Tegart W J.Met Sci Rev Methods, 1996; 63: 731 | | [25] | Biswas S, Reddy G M, Mohandas T, Murthy V S.J Mater Sci, 2004; 39: 6813 | | [26] | Zhou N, Lv D C, Zhang H L, McAllister D, Zhang F.Acta Mater, 2014; 65: 270 | | [27] | Lin Y C, Wen D X, Deng J, Chen J.Mater Des, 2014; 59: 115 | | [28] | Findley K O, Evans J L, Saxena A.Int Mater Rev, 2011; 56: 49 | | [29] | Garcia C I, Wang G D, Camus D E, Loria E A, De Ardo A J. In: Loria E A ed., 3rd Int Symp on Superalloys 718, 626, 706, and Various Derivatives, Pittsburgh, PA: The Minerals, Metals & Materials Society, 1994: 293 | | [30] | Ning Y Q, Fu M W, Chen X.Mater Sci Eng, 2012; A540: 164 | | [31] | Wen D X, Lin Y C, Li H B, Chen X M, Deng J, Li L T.Mater Sci Eng, 2014; A591: 183 | | [32] | Wen D X, Lin Y C, Chen J, Chen X M, Zhang J L, He M.Mater Sci Eng, 2015; A620: 319 | | [33] | Thomas A, El-Wahabi M, Cabrera J M, Prad J M.J Mater Process Technol, 2006; 177: 469 | | [34] | Zhang H Y, Zhang S H, Cheng M, Li Z X.Mater Charact, 2010; 61: 49 | | [35] | Cheng M, Zhang H Y, Zhang S H.J Mater Sci, 2012; 47: 251 | | [36] | Wang Y, Zhen L, Shao W Z, Yang L, Zhang X M.J Alloys Compd, 2009; 474: 341 | | [37] | Nalawade S A, Sundararaman M, Singh J B, Verma A, Kishore R.Mater Sci Eng, 2010; A527: 2906 | | [38] | Lin Y C, Li K K, Li H B, Wen D X.Mater Des, 2015; 74: 108 | | [39] | Chen X M, Lin Y C, Wen D X, Zhang J L, He M.Mater Des, 2014; 57: 568 | | [40] | Lin Y C, Chen X M, Wen D X, Chen M S.Comp Mater Sci, 2014; 83: 282 | | [41] | Feng Y J.Master Thesis, Harbin Institute of Technology, 2012 | | [41] | (冯莹娟. 哈尔滨工业大学硕士学位论文, 2012) | | [42] | Liu W C, Xiao F R, Yao M.Scr Mater, 1997; 37: 53 | | [43] | Wei X P, Zheng W J, Song Z G, Lei T, Yong Q L, Xie Q C.J Iron Steel Res Int, 2014; 21: 375 | | [44] | Mei Y P, Liu Y C, Liu C X, Li C, Yu L M, Guo Q Y, Li H J.J Alloys Compd, 2015; 649: 949 | | [45] | Wang Y.Master Thesis, Harbin Institute of Technology, 2008 | | [45] | (王岩. 哈尔滨工业大学硕士学位论文, 2008) | | [46] | Lin Y C, Deng J, Jiang Y Q, Liu G.Mater Des, 2014; 55: 949 | | [47] | Kashyap B P, Chaturvedi M C. Mater Sci Eng, 2007; A445-446: 364 | | [48] | Huang Y, Langdon T G.J Mater Sci, 2007; 42: 421 | | [49] | Ning Y Q, Huang S B, Fu M W, Dong J.Mater Charact, 2015; 109: 36 | | [50] | Deng G J, Tu S T, Zhang X C, Wang J, Zhang C C, Qian X Y, Wang Y N.Eng Fract Mech, 2016; 153: 35 | | [51] | Hu D Y, Mao J X, Song J, Meng F C, Shan X M, Wang R Q.Mater Sci Eng, 2016; A669: 318 | | [52] | Ding T S, Zhang X C, Tu S D, Xuan F Z.Trans Mater Heat Treat, 2016; 37(4): 69 | | [52] | (丁天胜, 张显程, 涂善东, 轩福贞. 材料热处理学报, 2016; 37(4): 69) | | [53] | Wang R Z, Zhang X C, Liu F, Yao L L, Tu S T.Procedia Eng, 2015; 130: 1088 | | [54] | Chen G, Zhang Y, Xu D K, Chen X.Mater Sci Eng, 2016; A655: 175 | | [55] | Xiao L, Chen D L, Chaturvedi M C.Mater Sci Eng, 2008; A483: 369 | | [56] | Xiao L, Chen D L, Chaturvedi M C.Scr Mater, 2005; 52: 603 | | [57] | Tian S G, Li Z R, Zhao Z G, Chen L Q, Sun W R, Liu X H.Rare Met Mater Eng, 2012; 41: 1651 | | [57] | (田素贵, 李振荣, 赵中刚, 陈礼清, 孙文儒, 刘相华. 稀有金属材料与工程, 2012; 41: 1651) | | [58] | Tian S G, Li Z R, Zhao Z G, Chen L Q, Sun W R, Liu X F.Mater Sci Eng, 2012; A550: 235 | | [59] | Caliari F R, Candioto K C G, Couto A A, Nunes C ?, Reis D A P.J Mater Eng Perform, 2016; 25: 2307 | | [60] | Kuo C M, Yang Y T, Bor H Y, Wei C N, Tai C C. Mater Sci Eng, 2009; A510-511: 289 | | [61] | Song H W, Guo S R, Hu Z Q.Scr Mater, 1999; 41: 215 | | [62] | Yeh A C, Lu K W, Kuo C M, Borc H Y, Wei C N.Mater Sci Eng, 2011; A530: 525 | | [63] | Richards N L, Chaturvedi M C.Int Mater Rev, 2000; 45: 109 | | [64] | Damodaram R, Raman S G S, Rao K P.Mater Sci Eng, 2013; A560: 781 | | [65] | Damodaram R, Raman S G S, Rao K P.Mater Des, 2014; 53: 954 | | [66] | Idowu O A, Ojo O A, Chaturvedi M C.Mater Sci Eng, 2007; A454: 389 | | [67] | Manikandan S G K, Sivakumar D, Kamaraj M, Prasad K.Mater Sci Forum, 2012; 710: 614 | | [68] | Ramkumar K D, Sridhar R, Periwal S, Oza S, Saxena V.Mater Des, 2015; 68: 158 | | [69] | Koleva E G, Mladenov G M, Trushnikov D N, Belenkiy V Y.J Mater Process Technol, 2014; 214: 1812 | | [70] | Khodir S, Shibayanagi T, Takahashi M, Abdel-Aleem H, Ikeuchi K, Hidad P, Arivazhagan N.Mater Des, 2014; 60: 391 | | [71] | Mei Y P, Liu Y C, Liu C X, Li C, Yu L M, Guo Q Y, Li H J.Mater Des, 2016; 89: 964 |
|
|