Please wait a minute...
Acta Metall Sin  1996, Vol. 32 Issue (11): 1130-1138    DOI:
Current Issue | Archive | Adv Search |
EFFECTS OF Si ON MECHANICAL PROPERTIES AND GRAIN BOUNDARY STRUCTURES IN HYPEREUTECTOID Mn STEELS
ZHU Xiaodong; LI Chengji; ZHANG Shouhua (University of Scicnce and Technol ogy Beijing; Beijing 100083); ZOU Ming; SU Shihuai (Panzhihua Iron and Steel [Group] Company; Panzhihua 617067)
Cite this article: 

ZHU Xiaodong; LI Chengji; ZHANG Shouhua (University of Scicnce and Technol ogy Beijing; Beijing 100083); ZOU Ming; SU Shihuai (Panzhihua Iron and Steel [Group] Company; Panzhihua 617067). EFFECTS OF Si ON MECHANICAL PROPERTIES AND GRAIN BOUNDARY STRUCTURES IN HYPEREUTECTOID Mn STEELS. Acta Metall Sin, 1996, 32(11): 1130-1138.

Download:  PDF(884KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  The effects of Si on the grain boundary structure and mechanical properties of hypereutectoid Mn steels austenitized at 950℃ and isothemially transformed at 560℃were studied by means of SEM and TEM. The experimental results showed that the impact toughness and elongation can be improved by Si additions. The observation of microstructure revealed that grain boundary cemetite networks can be inhibited and grain boundary ferrite formed in these hypereutectoid steels by Si addition. The formation mechanism of grain boundary ferrite has also been discussed. Correspondent: LI Chengji, Professor, Department of Materials Science and Engineering, University of Science and Technology Beijing, Beijing 100083
Key words:  grain boundary ferrite      hypereutetoid steel      pearlite      mechanical property     
Received:  18 November 1996     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1996/V32/I11/1130

1AlltenAG,PaysonP.TransASM,1953;45:4982ParkerER.MetallTrans,1977;8:10253胡光立,康沫狂等.航空材料,1985;5:14KangMokuang.In:LiuGuoxun,StuartH,ZhangHongtao,LiChengeds.HSLASteels'95ConfProc,Beijing:ChinaScience&TechnologyPress,1995:4955TsukataniI,HashimotoS,InoueT.In:TitherG,ZhangShouhuaeds.,HSLASteels:Processing,PropertiesandApplications,ProcoftheSecondInternationalConferenceonHSLASteels,USA:TMS,1990:2916王传雅.特殊钢,1994;15(6):547周富智主编.低合金钢性能手册.北京:冶金工业出版社,1986:3438HanK,SmithGDW,EdmondsDV.MetallMaterTrans,1995;26A:16179PickeringFB,GarbarzB.ScrMetall,1987;21:24910朱晓东,李承基,章守华等.北京科技大学学报,1996,6(待出版)11刘世楷,张筠.材料科学进展,1988;2:.2212SandvikBPJ.MetallTrans,1982;13A:77713LeHouillerR,BeginG,DubeA.MetallTrans,1971;2:264714李承基,胡梦怡.金属热处理学报,1981:1:1815HehemannRF,KinsmanKR,AaronsonHI.MetallTrans,1972;3A:107716李承基,高德春,曹凤豫,陆丰.金属学报,1993;29:A53517MemahonCJ.MetallTrans,1980;11A:53118李承基.贝氏体相变理论.北京:机械工业出版社,1995:52
[1] ZHANG Leilei, CHEN Jingyang, TANG Xin, XIAO Chengbo, ZHANG Mingjun, YANG Qing. Evolution of Microstructures and Mechanical Properties of K439B Superalloy During Long-Term Aging at 800oC[J]. 金属学报, 2023, 59(9): 1253-1264.
[2] ZHENG Liang, ZHANG Qiang, LI Zhou, ZHANG Guoqing. Effects of Oxygen Increasing/Decreasing Processes on Surface Characteristics of Superalloy Powders and Properties of Their Bulk Alloy Counterparts: Powders Storage and Degassing[J]. 金属学报, 2023, 59(9): 1265-1278.
[3] GONG Shengkai, LIU Yuan, GENG Lilun, RU Yi, ZHAO Wenyue, PEI Yanling, LI Shusuo. Advances in the Regulation and Interfacial Behavior of Coatings/Superalloys[J]. 金属学报, 2023, 59(9): 1097-1108.
[4] ZHANG Jian, WANG Li, XIE Guang, WANG Dong, SHEN Jian, LU Yuzhang, HUANG Yaqi, LI Yawei. Recent Progress in Research and Development of Nickel-Based Single Crystal Superalloys[J]. 金属学报, 2023, 59(9): 1109-1124.
[5] CHEN Liqing, LI Xing, ZHAO Yang, WANG Shuai, FENG Yang. Overview of Research and Development of High-Manganese Damping Steel with Integrated Structure and Function[J]. 金属学报, 2023, 59(8): 1015-1026.
[6] DING Hua, ZHANG Yu, CAI Minghui, TANG Zhengyou. Research Progress and Prospects of Austenite-Based Fe-Mn-Al-C Lightweight Steels[J]. 金属学报, 2023, 59(8): 1027-1041.
[7] LI Jingren, XIE Dongsheng, ZHANG Dongdong, XIE Hongbo, PAN Hucheng, REN Yuping, QIN Gaowu. Microstructure Evolution Mechanism of New Low-Alloyed High-Strength Mg-0.2Ce-0.2Ca Alloy During Extrusion[J]. 金属学报, 2023, 59(8): 1087-1096.
[8] YUAN Jianghuai, WANG Zhenyu, MA Guanshui, ZHOU Guangxue, CHENG Xiaoying, WANG Aiying. Effect of Phase-Structure Evolution on Mechanical Properties of Cr2AlC Coating[J]. 金属学报, 2023, 59(7): 961-968.
[9] WU Dongjiang, LIU Dehua, ZHANG Ziao, ZHANG Yilun, NIU Fangyong, MA Guangyi. Microstructure and Mechanical Properties of 2024 Aluminum Alloy Prepared by Wire Arc Additive Manufacturing[J]. 金属学报, 2023, 59(6): 767-776.
[10] HOU Juan, DAI Binbin, MIN Shiling, LIU Hui, JIANG Menglei, YANG Fan. Influence of Size Design on Microstructure and Properties of 304L Stainless Steel by Selective Laser Melting[J]. 金属学报, 2023, 59(5): 623-635.
[11] ZHANG Dongyang, ZHANG Jun, LI Shujun, REN Dechun, MA Yingjie, YANG Rui. Effect of Heat Treatment on Mechanical Properties of Porous Ti55531 Alloy Prepared by Selective Laser Melting[J]. 金属学报, 2023, 59(5): 647-656.
[12] LIU Manping, XUE Zhoulei, PENG Zhen, CHEN Yulin, DING Lipeng, JIA Zhihong. Effect of Post-Aging on Microstructure and Mechanical Properties of an Ultrafine-Grained 6061 Aluminum Alloy[J]. 金属学报, 2023, 59(5): 657-667.
[13] LI Shujun, HOU Wentao, HAO Yulin, YANG Rui. Research Progress on the Mechanical Properties of the Biomedical Titanium Alloy Porous Structures Fabricated by 3D Printing Technique[J]. 金属学报, 2023, 59(4): 478-488.
[14] WU Xinqiang, RONG Lijian, TAN Jibo, CHEN Shenghu, HU Xiaofeng, ZHANG Yangpeng, ZHANG Ziyu. Research Advance on Liquid Lead-Bismuth Eutectic Corrosion Resistant Si Enhanced Ferritic/Martensitic and Austenitic Stainless Steels[J]. 金属学报, 2023, 59(4): 502-512.
[15] WANG Hu, ZHAO Lin, PENG Yun, CAI Xiaotao, TIAN Zhiling. Microstructure and Mechanical Properties of TiB2 Reinforced TiAl-Based Alloy Coatings Prepared by Laser Melting Deposition[J]. 金属学报, 2023, 59(2): 226-236.
No Suggested Reading articles found!