RECENT RESEARCH PROGRESS ON NANOCRYSTALLINE MATERIALS
LU Ke; ZHOU Fei (State Key Laboratory for RSA; Institute of Metal Research;Chinese Academy of Sciences; Shenyang 110015)
Cite this article: 

LU Ke; ZHOU Fei (State Key Laboratory for RSA; Institute of Metal Research;Chinese Academy of Sciences; Shenyang 110015). RECENT RESEARCH PROGRESS ON NANOCRYSTALLINE MATERIALS. Acta Metall Sin, 1997, 33(1): 99-106.

Download:  PDF(868KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  Polycrystalline materials with grains sizes in the nanometer region (typically less than 100 nm), termed nanocrystalline materials, have been intensively investigated in the past several years. Much improvement has been made in the field of both fundamental understanding and practical applications of this type of materials. This article reviews the present state of the art in this field. The current status of research and development on the synthesis,microstructure, structural instability, and properties of nanocrystalline materials will be summarized. Further consideations of the development and applications of this new class of materials will also be presented.
Key words:  nanocrystalline materials      synthesis      microstructure      properties     
Received:  18 January 1997     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1997/V33/I1/99

1Gleiter H Prog Mater Sci,1989; 33: 223
2Suryanarayana C Inter Mater Rev,1995;40: 41
3 Lu K Mater Sci Eng Roports,1996;16;161
4Koch C C. Nanostr Marer,1993;2:109
5Erb U, El-Sherik A M,Palumbo G,AustK T. Nanostr Mater,1993; 2: 383
6 Oehring M,Appel F,Pfullmann Th Bormann R.Appl Phys Lett,1995;66:941
7 He L,Ma E J M ater Res, 1996;11:72
8 He L,Ma E.Nanostr Mater,1996;7 347
9Zhou F, Sheng H W,Lu K to be published
10 Rittner M N,Sanders P G,Weertman J R.Nanostr Mater,1997 to be published
11 Erb U.Nanostr Mater 1995 6: 533
12 Inoue A Zhang T,Nishiyama N,Ohba K,Masumoto T.Mater Sci Eng,1994;A179/A180:210
13 Kawamura Y,Kato H,Inoue A.Appl Phys Lett,1995;67:2008
14 Thomas G J,Siegel R W,Eastman J A Scr Metall Mater,1990;24:201
15 Ganapathi S K,Rigney D AScr Metall Mater,1990;24:1675
16 Li D X Ping D H,Ye H Q,Qin X Y,Wu X J.Mater Letters,1993;18:29
17 Wang J,Wolf D,Phillpot S R Phil Mng A,1996;73:517
18 Keblinsxi P Phillpot S R,Wolf D Nanostr,1997;to be published
19 Lu K,Luck R,Predel B Scr Metall Mater,1993;28:1387
20 Lu K,et al.to be published
21 Terwillinger C D,Chiang Y M MRS Symp Proc,1993;289:15
22 Birringer R,Krill C E,Klingel M Phil Mag Letters,1995;72:71
23 Zhang H Y,Hu Z Q,Lu K J Phys:Condens Matter,1995; 7: 5327
24 Zhao Y H,Lu K to be published
25 Zhang K,Alexandrov I V, Valiev R Z, Lu K J Appl Phys 1996;in print
26 Gunther B,Kumpmann A Kunze H D.Scr Metall Mater,1992;27 83
27 Lu K Nanostr Mater,1993; 2A: 643
28 Lu K,Dong Z F,Lang D Luck R Acta Mater, 1997 to be published
29 Sun N X Lu K Phys Rev B 1996;in print
30 Erb U.(Private Communication)
31 Shen T D,Koch C C,Tsui T Y,Pharr G M J Mater Res,1995;10:2892
32 Lu K,Sui M L Acta Metall Mater,1995;43:3325
33 Siegel R W,Fougere G E Nanostr Mater,1995; 6 205
34卢柯,刘学东,胡壮麒。材料研究学报,1994 8: 385
35 Zhang H Y,Hu Z Q,Lu K.J App Phys,1995;772811,J Mater Res,1997;in print
36 Yan D S, Shi J L,Qin H B,Zheng Y S Gao L.Nanostr Mater,1997;to be published
37 Cheung C, Wood D Erb U In:sufyanarayana C, singh J,Froes F H eds, Processing and Properties of Nanocrystalline Materials,The Minerals,Metals & Materials Society,1996
[1] ZHANG Leilei, CHEN Jingyang, TANG Xin, XIAO Chengbo, ZHANG Mingjun, YANG Qing. Evolution of Microstructures and Mechanical Properties of K439B Superalloy During Long-Term Aging at 800oC[J]. 金属学报, 2023, 59(9): 1253-1264.
[2] LU Nannan, GUO Yimo, YANG Shulin, LIANG Jingjing, ZHOU Yizhou, SUN Xiaofeng, LI Jinguo. Formation Mechanisms of Hot Cracks in Laser Additive Repairing Single Crystal Superalloys[J]. 金属学报, 2023, 59(9): 1243-1252.
[3] GONG Shengkai, LIU Yuan, GENG Lilun, RU Yi, ZHAO Wenyue, PEI Yanling, LI Shusuo. Advances in the Regulation and Interfacial Behavior of Coatings/Superalloys[J]. 金属学报, 2023, 59(9): 1097-1108.
[4] WANG Lei, LIU Mengya, LIU Yang, SONG Xiu, MENG Fanqiang. Research Progress on Surface Impact Strengthening Mechanisms and Application of Nickel-Based Superalloys[J]. 金属学报, 2023, 59(9): 1173-1189.
[5] LI Jingren, XIE Dongsheng, ZHANG Dongdong, XIE Hongbo, PAN Hucheng, REN Yuping, QIN Gaowu. Microstructure Evolution Mechanism of New Low-Alloyed High-Strength Mg-0.2Ce-0.2Ca Alloy During Extrusion[J]. 金属学报, 2023, 59(8): 1087-1096.
[6] LIU Xingjun, WEI Zhenbang, LU Yong, HAN Jiajia, SHI Rongpei, WANG Cuiping. Progress on the Diffusion Kinetics of Novel Co-based and Nb-Si-based Superalloys[J]. 金属学报, 2023, 59(8): 969-985.
[7] CHEN Liqing, LI Xing, ZHAO Yang, WANG Shuai, FENG Yang. Overview of Research and Development of High-Manganese Damping Steel with Integrated Structure and Function[J]. 金属学报, 2023, 59(8): 1015-1026.
[8] SUN Rongrong, YAO Meiyi, WANG Haoyu, ZHANG Wenhuai, HU Lijuan, QIU Yunlong, LIN Xiaodong, XIE Yaoping, YANG Jian, DONG Jianxin, CHENG Guoguang. High-Temperature Steam Oxidation Behavior of Fe22Cr5Al3Mo-xY Alloy Under Simulated LOCA Condition[J]. 金属学报, 2023, 59(7): 915-925.
[9] ZHANG Deyin, HAO Xu, JIA Baorui, WU Haoyang, QIN Mingli, QU Xuanhui. Effects of Y2O3 Content on Properties of Fe-Y2O3 Nanocomposite Powders Synthesized by a Combustion-Based Route[J]. 金属学报, 2023, 59(6): 757-766.
[10] WANG Fa, JIANG He, DONG Jianxin. Evolution Behavior of Complex Precipitation Phases in Highly Alloyed GH4151 Superalloy[J]. 金属学报, 2023, 59(6): 787-796.
[11] WU Dongjiang, LIU Dehua, ZHANG Ziao, ZHANG Yilun, NIU Fangyong, MA Guangyi. Microstructure and Mechanical Properties of 2024 Aluminum Alloy Prepared by Wire Arc Additive Manufacturing[J]. 金属学报, 2023, 59(6): 767-776.
[12] GUO Fu, DU Yihui, JI Xiaoliang, WANG Yishu. Recent Progress on Thermo-Mechanical Reliability of Sn-Based Alloys and Composite Solder for Microelectronic Interconnection[J]. 金属学报, 2023, 59(6): 744-756.
[13] FENG Aihan, CHEN Qiang, WANG Jian, WANG Hao, QU Shoujiang, CHEN Daolun. Thermal Stability of Microstructures in Low-Density Ti2AlNb-Based Alloy Hot Rolled Plate[J]. 金属学报, 2023, 59(6): 777-786.
[14] WANG Changsheng, FU Huadong, ZHANG Hongtao, XIE Jianxin. Effect of Cold-Rolling Deformation on Microstructure, Properties, and Precipitation Behavior of High-Performance Cu-Ni-Si Alloys[J]. 金属学报, 2023, 59(5): 585-598.
[15] ZHANG Dongyang, ZHANG Jun, LI Shujun, REN Dechun, MA Yingjie, YANG Rui. Effect of Heat Treatment on Mechanical Properties of Porous Ti55531 Alloy Prepared by Selective Laser Melting[J]. 金属学报, 2023, 59(5): 647-656.
No Suggested Reading articles found!