| RECENT RESEARCH PROGRESS ON NANOCRYSTALLINE MATERIALS |
| LU Ke; ZHOU Fei (State Key Laboratory for RSA; Institute of Metal Research;Chinese Academy of Sciences; Shenyang 110015) |
|
Cite this article:
LU Ke; ZHOU Fei (State Key Laboratory for RSA; Institute of Metal Research;Chinese Academy of Sciences; Shenyang 110015). RECENT RESEARCH PROGRESS ON NANOCRYSTALLINE MATERIALS. Acta Metall Sin, 1997, 33(1): 99-106.
|
|
|
Abstract Polycrystalline materials with grains sizes in the nanometer region (typically less than 100 nm), termed nanocrystalline materials, have been intensively investigated in the past several years. Much improvement has been made in the field of both fundamental understanding and practical applications of this type of materials. This article reviews the present state of the art in this field. The current status of research and development on the synthesis,microstructure, structural instability, and properties of nanocrystalline materials will be summarized. Further consideations of the development and applications of this new class of materials will also be presented.
|
|
Received: 18 January 1997
|
1Gleiter H Prog Mater Sci,1989; 33: 223 2Suryanarayana C Inter Mater Rev,1995;40: 41 3 Lu K Mater Sci Eng Roports,1996;16;161 4Koch C C. Nanostr Marer,1993;2:109 5Erb U, El-Sherik A M,Palumbo G,AustK T. Nanostr Mater,1993; 2: 383 6 Oehring M,Appel F,Pfullmann Th Bormann R.Appl Phys Lett,1995;66:941 7 He L,Ma E J M ater Res, 1996;11:72 8 He L,Ma E.Nanostr Mater,1996;7 347 9Zhou F, Sheng H W,Lu K to be published 10 Rittner M N,Sanders P G,Weertman J R.Nanostr Mater,1997 to be published 11 Erb U.Nanostr Mater 1995 6: 533 12 Inoue A Zhang T,Nishiyama N,Ohba K,Masumoto T.Mater Sci Eng,1994;A179/A180:210 13 Kawamura Y,Kato H,Inoue A.Appl Phys Lett,1995;67:2008 14 Thomas G J,Siegel R W,Eastman J A Scr Metall Mater,1990;24:201 15 Ganapathi S K,Rigney D AScr Metall Mater,1990;24:1675 16 Li D X Ping D H,Ye H Q,Qin X Y,Wu X J.Mater Letters,1993;18:29 17 Wang J,Wolf D,Phillpot S R Phil Mng A,1996;73:517 18 Keblinsxi P Phillpot S R,Wolf D Nanostr,1997;to be published 19 Lu K,Luck R,Predel B Scr Metall Mater,1993;28:1387 20 Lu K,et al.to be published 21 Terwillinger C D,Chiang Y M MRS Symp Proc,1993;289:15 22 Birringer R,Krill C E,Klingel M Phil Mag Letters,1995;72:71 23 Zhang H Y,Hu Z Q,Lu K J Phys:Condens Matter,1995; 7: 5327 24 Zhao Y H,Lu K to be published 25 Zhang K,Alexandrov I V, Valiev R Z, Lu K J Appl Phys 1996;in print 26 Gunther B,Kumpmann A Kunze H D.Scr Metall Mater,1992;27 83 27 Lu K Nanostr Mater,1993; 2A: 643 28 Lu K,Dong Z F,Lang D Luck R Acta Mater, 1997 to be published 29 Sun N X Lu K Phys Rev B 1996;in print 30 Erb U.(Private Communication) 31 Shen T D,Koch C C,Tsui T Y,Pharr G M J Mater Res,1995;10:2892 32 Lu K,Sui M L Acta Metall Mater,1995;43:3325 33 Siegel R W,Fougere G E Nanostr Mater,1995; 6 205 34卢柯,刘学东,胡壮麒。材料研究学报,1994 8: 385 35 Zhang H Y,Hu Z Q,Lu K.J App Phys,1995;772811,J Mater Res,1997;in print 36 Yan D S, Shi J L,Qin H B,Zheng Y S Gao L.Nanostr Mater,1997;to be published 37 Cheung C, Wood D Erb U In:sufyanarayana C, singh J,Froes F H eds, Processing and Properties of Nanocrystalline Materials,The Minerals,Metals & Materials Society,1996 |
| No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|