THE ROLE OF INTERFACE IN THE DEFORMATION PROCESS OF MULTIPHASE INTERMETALLICS |
YANG Rui (Institute of Metal Research; Chinese Academy of Sciences; Shenyang 110015) |
|
Cite this article:
YANG Rui (Institute of Metal Research; Chinese Academy of Sciences; Shenyang 110015). THE ROLE OF INTERFACE IN THE DEFORMATION PROCESS OF MULTIPHASE INTERMETALLICS. Acta Metall Sin, 1997, 33(1): 107-112.
|
Abstract Recent developments in multiphase intermetallics are reviewed in this paper.The emphasis is placed upon the role various interfaces play in influencing the deformationprocess and mechanical behaviour of the multiphase alloys. The examples are taken fromTiAl based and (Ni,Fe,Co)Al based materials. It is shown that the operation of interface-related dislocation sources can improve the deformability of the brittle phases. A better balanceof mechanical properties can be obtained when the beneficial effects of the interfaces are manifested by a proper choice of constituent phases and conditions of material preparation andprocessing.
|
Received: 18 January 1997
|
1Cahn R W.Phil Trans R Soc Lond A,1995;351:497 2Nabarro F R N.Mater Sci Eng A,1994:184;167 3Noebe R D Bowman R R, Kim J T, Larsen M Gibala R.In:Whang S H,Liu C T,Pope D P,Stiegler J O eds,High Temperature Alumidides Intermetallic,Warrendale:TMS 1990:271 4Kim Y-W, Dimiduk D M JOM,1991(8);43:40 5Fujiwara T,Nakamura A,Hosomi M,Nishitani S R,Shirai Y,Yamaguchi M.Philos Mag A,1990;61:591 6Inui H,Oh M H,Nakamura A Yamaguchi M.Acta Metall Mater,1992;40:30954 7Reviere R D,Oliver B F,Bruns D D.Mater Manuf Proc,1989;4:103 8Minonishi Y.Philos Mag A,1991; 63:1085 9Kad B K,Hazzledine P M,Fraser H L.Mater Res Soc Symp Proc,1993;288:495 10Kad B K,Hazzledine P M.Philos Mag Lett, 1992; 66: 133 11Appel F,Beaven P A, Wagner R.Acta Metall Mater,1993;41:1721 12Christoph U Sparka U,Appel F, Wagner R. Acta Metall Sin(Eng Lett),1995 8:349 13Russell K C,Edington J W.Met Sci J 1972;6:20 14Moskovic R.J Mater Sci,1978;13:1901 15Noebe R D,Misra A Gibala R.ISIJ Int,1991;31:1172 16Misra A Noebe R D,Gibala R.Mater Res Soc Symp Proc,1993;288:483 17Jung I,Sauthoff G.Z Metallkd 1989:80;484 18Guha S,Munroe P R,Baker I.Mater Sci Eng A,1991; 131:27 19Strutt P R, Polvani R S Ingram J C. Metall Trans A, 1976; 7 23 20Polvani R S,Tzeng W S,Strutt P R.Metall Trans A,1976; 7:33 21Nash P G,Liang W W.Metall Trans A,1985;16:319 22Yang R Saunders N,Leake J A, Cahn R W.Acta Metall Mater,1992;40:1553 23Yang R,Parker S V,Leake J A Cahn R W In Stocks G M,Turchi P eds. Alloy Modelling and Design,Proc of TMS Symp,Pittsburgh:TMS,1994:303 24Yang R,Leake J A Cahn R W.J Mater Res,1991;6:343 25Yang R, Leake J A, Cahn R W.Mater Sci Eng,1992;A152:227 26Yang R.PhD Thesis,University of Cambridge,1992 27Yang R,Leake J A Cahn R W.Mater Res Soc Symp Proc, 1993; 288:489 28Hsiung L C,Bhadeshia H K D H.Metall Trans A,1995;26:1895 29Pank D R,Nathal M V,Koss D A J Mater Res,1990; 5:942 30Ishida K,Kainuma R,Ueno N,Nishizawa T Melall Trans A,1991;22:411 31Mishima Y,Lee E H,Liu C T.Mater Trans JIM,1995;36:1031 32Mishima Y Acta Metall Sin (Eng Lett),1995;8:339 33Misnima Y,Kato M, Kimura Y,Hosoda H,Miura S Intermetallics,1996; 6:in pressi |
No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
|
Shared |
|
|
|
|
|
Discussed |
|
|
|
|