Abstract As-cast Ti-43Al-9V-0.3Y alloy is mainly comprised of γ phase, besides minor α2, B2 and YAl2. The alloy is fine-grained and mainly consists of lamellar structure (approximately 85 vol%). The mean colony size is about 80 μm. There is evidence of the β phase and γ phase along colony boundaries and disperse fine YAl2 particles. There exist some B2 precipitations within the lamellar colonies. As-forged Ti-43Al-9V-0.3Y alloy has the streamline near gamma (NG) microstructure drastically refined with DRX γ grains of 1~5μm. The B2 and YAl2 phases are broken and elongated and the lamellar colonies diminish. As-rolled Ti-43Al-9V-0.3Y alloy has the fine NG microstructure with γ grains of about 20μm. The streamline structure vanishes. The B2 phases with size of 8μm are distributed in the network shape along γ grains and the YAl2 particles are disperse. As-cast Ti-43Al-9V-0.3Y alloy has the ultimate tensile strength of about 510.6 and 425.8MPa, the elongation of 0.5% and 5.7%, at room temperature and 700℃, respectively. After forging and rolling, the tensile properties are greatly improved. At room temperature, the strength of as-forged and as-rolled material increases about 89~132MPa, and the elongation increases from 0.5% to 1% and 1.2%, respectively. At 700℃, the strength as-rolled material increases about 63~72MPa and the elongation increases from 5.7% to 7.9%. The improvement of the tensile properties is attributed to the microstructural refinement and higher density induced by forging and rolling process.
[1]Husng Z H.Trans Nonferrous Met Soc China,2003;13: 1325 [2]Maziasz P J,Liu C T.Metall Mater Trans,1998;29A:105 [3]Edward A L.Intermetallics,2000;8:1339 [4]Appel F,Oehring M,Paul J D H,Klinkenberg C,Cameiro T.Intermetallics,2004;12:791 [5]Semiatin S L,Seetharaman V,Weiss I.Mater Sci Eng, 1998;A243:1 [6]Oh J,Pyo S G,Lee S.J Mater Sci,2003;38:3647 [7]Bartels A,Kestler H,Clemens H.Mater Sci Eng,2002; A329-331:153 [8]Gerling R,Bartels A,Clements H,Kestler H.Inter- metallics,2004;12:275 [9]Chen Y Y,Kong F T,Hart J C,Chen Z Y,Tian J.Inter- metallics,2005;13:263