Abstract In this paper, the morphology and structure change of fine copper powder during its oxidization process was observed by SEM and TEM. And their weight gain processes were measured by Thermal gravity Analyser(TGA). Based on the experiments and some classical theories, the course of the oxidation of fine copper powder was proposed. Then a new kinetics equation was deduced to simulate the course. The analog results agree well with the data gained from the oxidation of copper between 250-400℃.
[1]Tu H L,Zhao G Q,Guo Q W.Nonferrous Metals- Metallurgy,Material,Reproduct and Environmental Pro- teetion.Beijing:Chemical Industry Press,2003:14 (屠海令,赵国权,郭青蔚.有色金属——冶金、材料、再生与环保.北京:化学工业出版社,2003:14) [2]Patil S,Salnkar S It,Patti P P.Appl Surf Sci,2004;225: 204 [3]Han Z,Lu L,Zhang H W,Yang Z Q,Wang F H,Lu K. Oxid Met,2005;63:261 [4]Bridges D W,Baur J P,Baur G S,Fassell W M.J Elec- trochem Soc,1956;103:475 [5]Wallwork G R.,Smeltzer W W.Corros Sci,1969;9:561 [6]Mrowec S.Oxid Met,1973;6:178 [7]Garnaud G.Oxid Met,1977;11:127 [8]Hoar T P,Price L E.Trans Faraday Soc,1938;34:867 [9]Zhu R Z,He Y D,Qi H B.High-temperature Corro- sion and Resisting High-temperature Corrosion Materi- als.Shanghai:Shanghai Science and Technology Press, 1995:99 (朱日彰,何业东,齐慧滨.高温腐蚀及耐高温腐蚀材料.上海:上海科学技术出版社,1995:99) [10]Li T F.High Temperature Oxidation and Hot Corrosion of Metals.Beijing:Chemical Industry Press,2003:52 (李铁藩.金属高温氯化和热腐蚀.北京:化学工业出版社,2003:52) [11]Evans U R.The Corrosion and Oxidation of Metals.Lon- don:Edward Arnold Ltd,1968;696:701