Please wait a minute...
Acta Metall Sin  2008, Vol. 44 Issue (7): 826-830     DOI:
Research Articles Current Issue | Archive | Adv Search |
The graded material of 316L stainless steel-Ni-based alloy-Ti6Al4V formed by laser rapid forming process
北京有色金属研究总院
Cite this article: 

. The graded material of 316L stainless steel-Ni-based alloy-Ti6Al4V formed by laser rapid forming process. Acta Metall Sin, 2008, 44(7): 826-830 .

Download:  PDF(2334KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  The graded material of 316L stainless steel/Ni-based alloy/Ti6Al4V was fabricated from metal powders using laser rapid forming process. The as-formed graded material is fully dense and free of cracks. The microstructure of the graded segment of 316L stainless steel to Ni-based alloy consists of γphase and the hardness values increase with the increment of the content of Ni-based alloy. A series of phase evolutions, , along the graded segment of Ni-based alloy to Ti6Al4V have occurred. The maximum hardness value (HV10830) was measured at the weight ratio of 80% Ni-based alloy to 20% Ti6Al4V, then the hardness values decrease with the increment of the content of Ti6Al4V.
Key words:       
Received:  05 November 2007     
ZTFLH:  TF777.1  
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y2008/V44/I7/826

[1]Lin X,Yue T M,Yang H O,Huang W D.Metall Mater Trans,2007;38A:127
[2]Lin X,Yue T M,Yang H O,Huang W D.Acta Mater, 2006;54:1901
[3]Lin X,Yue T M,Yang H O,Huang W D.Mater Sci Eng, 2005;A391:325
[4]Lin X,Yue T M.Mater Sci Eng,2005;A402:294
[5]Yakovlev A,Trunova E ,Grevey D,Pilloz M.Surf Coat Technol,2005;190:15
[6]Banerjee R,Collins P C,Bhattacharyya D,Banerjee S. Acta Mater,2003;51:3277
[7]Collins P C,Banerjee R,Banerjee S.Mater Sci Eng,2003; A352:118
[8]Shin K H,Natu H,Dutta D,Mazumder J.Mater Des, 2003;24:339
[9]Lewis G K,Schlienger E.Mater Des,2000;21:417
[10]Yadroitsev I,Bertrand Ph,Laget B,Smurov I.J Nucl Mater,2007;362:189
[1] WANG Luning, LIU Lijun, YAN Yu, YANG Kun, LU Lili. Influences of Protein Adsorption on the in vitro Corrosion of Biomedical Metals[J]. 金属学报, 2021, 57(1): 1-15.
[2] TUNG Feng'en;WANG Yuming Institute of Materials Science; Jilin University; Changchun. X-RAY ANALYSIS OF WORK-HARDENING PROCESS FOR POLYCRYSTALLINE а-BRASS DURING UNIAXIAL TENSILE TEST[J]. 金属学报, 1989, 25(2): 82-84.
[3] WANG Jinliang, WANG Chenchong, HUANG Minghao, HU Jun, XU Wei. The Effects and Mechanisms of Pre-Deformation with Low Strain on Temperature-Induced Martensitic Transformation[J]. 金属学报, 2021, 57(5): 575-585.
[4] DU Hegui;LIU Xin Northeast University of Technology; Shenyang. KINETICS OF CARBON COMBUSTION IN PLASMA AIR[J]. 金属学报, 1989, 25(2): 85-88.
[5] . [J]. 金属学报, 2001, 37(1): 42-46 .
[6] . [J]. 金属学报, 1999, 35(3): 320-324 .
[7] . [J]. 金属学报, 2000, 36(1): 72-76 .
[8] . [J]. 金属学报, 1999, 35(3): 330-333 .
[9] . [J]. 金属学报, 1999, 35(3): 334-336 .
[10] . [J]. 金属学报, 2000, 36(6): 647-650 .
[11] . [J]. 金属学报, 2000, 36(6): 655-658 .
[12] No Author. ACTA METALLURGLCA SLNLCA Volume 28 Series A 1992 SUBJECT INDEX[J]. 金属学报, 1992, 28(12): 63-90.
[13] . [J]. 金属学报, 2000, 36(7): 780-784 .
[14] No Author. ACTA METALLURGICA SINICA(JINSHU XUEBAO) Volume 28 1992 AUTHOR INDEX[J]. 金属学报, 1992, 28(12): 71-94.
[15] Хань Яо-вэнь Инсмцмум мемаддов АН КНР;Г.н.Ойкс Московскц цнсмцмум смадц. НЗУЧЕНИЕ ПРОЦЕССОВ ДЕСУЛЬФУРАЦИИ ХНДКОΓО МЕТАЛЛА В ВАКУУМЕ[J]. 金属学报, 1963, 6(2): 98-110.
No Suggested Reading articles found!