Microstructure and performance of AZ4.51-Ca magnesium alloy sheets
Chen Hongmei;Suk-Bong Kang;Huashun Yu;Guanghui Min
山东大学
Cite this article:
Chen Hongmei; Suk-Bong Kang; Huashun Yu; Guanghui Min. Microstructure and performance of AZ4.51-Ca magnesium alloy sheets. Acta Metall Sin, 2008, 44(4): 397-402 .
Abstract Magnesium sheets produced by different process were studied in this paper. The microstructure and mechanical properties of the alloys were analyzed by optical microscope (OM)、scanning electron microscope (SEM)、transmission electron microscope (TEM) 、digital microhardness tester and electron test equipment. The conventional casting ingot and twin rolling casting strip were all can be hot rolled at certain temperature and get magnesium sheets with 1mm thickness had refined and uniform deformation microstructure, the alloys were recrystallized after heat treatment and got equiaxed structure. The alloys had good mechanical properties after hot rolling, the strength and the elongation of twin roll casting alloy were evident higher than those of the conventional casting alloy. The tensile strength, yield strength and elongation of twin roll casting alloy and conventional casting alloy after hot rolling and 350℃×10min annealing were 334.4MPa, 229.3MPa, 23.8%, and 270.8MPa, 174.4MPa, 10.8%, respectively. The fracture surface of the alloys all took on ductile fracture contains lacerated ridge and ductile sockets, but the twin roll casting alloy had more evidence and smaller ductile sockets, this because the grain size of twin roll casting alloy was finer than that of conventioanal casting alloy.
[1]Park S S,Lee J G,Park Y S,Kim N J.Mater Sci Forum, 2003;419-422:599 [2]Alien R V,East D R,Johnson T J,Borbidge W E,Liang D.In:Hryn J N,ed.,Magnesium Technology 2001,War- rendale,Pennsylvania:TMS,2001:75 [3]Armstrong R W.Acta Metall,1968;16:347 [4]Barnett M R,Keshavarz Z,Beer A G,Atwell D.Acta Mater,2004;52:5093 [5]Jain A,Duygulu O,Brown D W,ToméC N,Agnew S R. Mater Sci Eng,in press [6]Chang T C,Wang J Y,Chia-Ming O,Lee S.J Mater Process Technol,2003;140:588 [7]Luo A A.Int Mater Rev,2004;49(1):13 [8]Suzuki A,Saddock N D,Jones J W,Pollock T M.Scr Mater,2004;51:1005 [9]Ninomiya R,Ojiro T,Kubota K.Acta Metall Mater,1995; 43:669 [10]Terada Y,Ishimatsu N,Sota R,Sato T,Ohori K.Mater Sci Forum,2003;419-422:459 [11]Mural T,Oguri H,Matsuoka S.Mater Sci Forum,2005; 488-489:515 [12]Seale G,Carter J,Verma R,Krajewski P,Essadiqi E, Javaid A,Galvani C,Zarandi F,Yue S.In:Beals R S, ed.,Magnesium Technology 2007,Warrendale,Pennsyl- vania:TMS,2007:17 [13]Yang P,Meng L,Mao W M,Cai Q W.Trans Mater Heat Treat,2005;26(2):34 (杨平,孟利,毛卫民,蔡庆武.材料热处理学报,2005;26(2):34) [14]Yu K,Li W X.Met Heat Treat,2002;27(5):8 (余琨,黎文献.金属热处理,2002;27(5):8) [15]Fu D F,Xu F Y,Xia W J,Liu T X,Chen Z H.Nat Sci J Xiangtan Univ,2005;27(4):57 (傅定发,许芳艳,夏伟军,刘天喜,陈振华.湘潭大学自然科学学报,2005;27(4):57) [16]Pan F S,Han E H.High Properties Wrought Magnesium Alloy and Processing Technology.Beijing:Science Press, 2007:18 (潘复生,韩恩厚.高性能变形镁合金及加工技术.北京:科学出版社,2007:18) [17]Bae G T,Park S S,Kang D H,Bae J H,Kim N J.In: Beals R S,ed.,Magnesium Technology 2007,Warrendale, Pennsylvania:TMS,2007:89 [18]Park S S,Oh Y S,Kang D H,Kim N J.Mater Sci Eng, 2007;A449-451:352 [19]Ninomiya R,Ojiro T,Kubota K.Acta Metall Mater,1995; 43:669 [20]Yang G Y,Hao Q T,Jie W Q,Jia W P,He Z.Acta Metall Sin,2005;41:933 (杨光昱,郝启堂,介万奇,贾文平,何志.金属学报,2005;41:933)