| HYDROGEN EMBRITTLEMENT SUSCEPTIBILITY OF 40CrNi3MoV STEELS WITH THE STRENGTH LEVEL OF 1500MPa |
| tian ye;WANG Mao-Qiu;Jinxu Li;;; |
| 北京科技大学材料科学与工程学院;钢铁研究总院先进钢铁材料技术国家工程研究中心 |
|
Cite this article:
tian ye; WANG Mao-Qiu; Jinxu Li. HYDROGEN EMBRITTLEMENT SUSCEPTIBILITY OF 40CrNi3MoV STEELS WITH THE STRENGTH LEVEL OF 1500MPa. Acta Metall Sin, 2008, 44(4): 403-408 .
|
|
|
Abstract Hydrogen embrittlement susceptibility of 40CrNi3MoV steels with Si contents of 0.25% and 1.16% and the strength level of 1500 MPa was investigated by means of slow strain rate tests. The reduction of notch tensile strength after introduction of hydrogen was used to characterize hydrogen embrittlement susceptibility and compact specimens were used to investigate hydrogen-induced crack propagation. Results show that the higher Si content 40CrNi3MoV steel was less susceptible to hydrogen embrittlement than the lower Si content 40CrNi3MoV steel with the same strength level of 1500 MPa, resulting from more and finer carbides which may act as hydrogen trapping sites and prevent hydrogen from diffusing to fracture process zone.
|
|
Received: 27 September 2007
|
|
|
[1]Zhang R S.Ordnance Mater Sci Eng,1995;18(3):3 (张锐生.兵器材料科学与工程,1995;18(3):3) [2]Wang M Q,Dong H,Wang Q,Li J X,Zhao L.Ordnance Mater Sci Eng,2003;26(2):7 (王毛球,董瀚,王琪,李建新,赵隆.兵器材料科学与工程,2003;26(2):7) [3]Shi C X,Averbach B L,Cohen M.Trans ASM,1956;48: 86 [4]Bandyopadhyay N,Kameda J,McMahon J C.Metall Trans,1983;14A:881 [5]Li H L,Hui W J,Wang Y B,Dong H,Weng Y Q,Chu W Y.Acta Metall Sin,2001;37:512 (李会录,惠卫军,王燕斌,董瀚,翁宇庆,褚武扬.金属学报,2001;37:512) [6]Nisitani H,Noda N.JSME,1985;51(461)A:54 (西谷宏信,野田尚昭.日本机械协会论文集,1985:51(461)A:54) [7]Wang M Q,Akiyama E,Tsuzaki K.Corros Sci,2006;48: 2189 [8]Chu W Y,Yu G H,Qiao L J,Cheng Y H.Sci Chin,1996; 26E:411 (褚武扬,于广华,乔利杰,程以环.中国科学,1996;26E:411) [9]Takai K,Seki J,Saktta E,Takayama K.Tetsu Hagané, 1993;79(5):67 (高井健一,关纯一,崎田荣一,高山康一.铁钢,1993;79(5):67) [10]Kushida T,Matsumoto H,Kuratomi N,Tsumupa T, Nakasato F,Kudo T.Tetsu Hagané,1996;82(4):37 (栉田隆弘,松本齐,仓富直行,津村辉隆,中里福和,工藤赳夫.铁钢,1996;82(4):37) [11]Guo H D,Tian X T.Corros Sci Prot Technol,1995;7(1): 47 (郭海丁,田锡唐.腐蚀科学与防护技术,1995;7(1):47) [12]Tarui T,Yamasaki S.Tetsu Hagané,2002;88(10):26 (樽井敏三,山﨑真吾.铁钢,2002;88(10):26) [13]Yu G H,Cheng Y H,Chen L,Qiao L J,Chu W Y.Acta Metall Sin,1995;31:A444 (于广华,程以环,陈廉,乔利杰,褚武扬.金属学报,1995;31:A444) [14]Snape E.Corrosion,1968;24:261 [15]Craig B D,Krauss G.Manuscr Submitted February,1980; 22A:1799 [16]Li G F,Wu R G,Lei T Q,Chu W Y.J Astronaut,1996; 17(3):58 (李光福,吴忍耕,雷廷权,褚武扬.宇航学报,1996;17(3):58) [17]Wu C J,Chen G L,Qiang W J.Metallic Materials.Bei- jing:Metallurgical Industry Press,2005:21 (吴承建,陈国良,强文江.金属材料学.北京:冶金工业出版社,2005:21) [18]Zhao J S,Zhang L M.J Beijing Univ Aeronaut Astronaut, 1991;(1):14 (赵敬世,张利民.北京航空航天大学学报,1991;(1):14) [19]Chu W Y,Xiao J M,Li S Q.Acta Metall Sin,1981;17: 10 (褚武扬,肖纪美,李世琼.金属学报,1981;17:10) |
| No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|