| EFFECT OF ZIRCONIUM CONTENT ON PRECIPITATION OF SILICIDE IN TI-1100 ALLOY |
| XU Feng; LI Geping; YANG Rui M. Varlioglu; P. Nash |
| Institute of Metal Research; Chinese Academy of Sciences; Shenyang 110016 |
|
Cite this article:
XU Feng; LI Geping; YANG Rui M. Varlioglu; P. Nash. EFFECT OF ZIRCONIUM CONTENT ON PRECIPITATION OF SILICIDE IN TI-1100 ALLOY. Acta Metall Sin, 2006, 42(7): 770-776 .
|
|
|
Abstract Morphology and distribution of silicide in Ti-1100 alloy with different zirconium content were observed by TEM. Isopleths at 0.45wt %( 0.76at %) of the Ti–Zr–Si system for Ti-1100 alloy was deduced according to the TEM results, isothermal sections of Ti–Zr–Si system phase diagram and concerned references. Both the TEM observation and the Isopleths show that silicide resolve temperature increases as Zr content increase. Moreover, as Zr content increased, dissolvability of silicon in titanium declines. These changes result in silicide coarsening, silicide volume fraction increase and precipitation position change.
|
|
Received: 04 December 2005
|
|
|
[1] Lee D H,Nam S W,Choe S J. Scr Metall, 1999; 40: 265 [2] Weinem D, Kumpfert J, Peters M, Kaysser W A. Mater Sci Eng, 1996; A206: 55 [3]ьорисов E A ed., Translated by Chen S Q. Metallography of Titanium Alloys. Beijing: National Defence Industry Press, 1980: 4 (ьорисовE A著.陈石卿译.钛合金金相学.北京: 国防工业出版社,1980:4) [4] Yan Y, Han D, Cao M Z. Chin J Mater Res, 1996; 10:587 (颜 莹,韩 东,曹名洲.材料研究学报, 1996;10:587) [5] Chen W F, Shi Y F. Rare Mater Eng, 1999; 28: 323 [6] Rosenberger A H,Madsen A,Ghonem H. J Mater Eng Perform, 1995; 2: 182 [7] Madsen A, Ghonem H. Mater Sci Eng, 1994; A177: 63 [8] Boyer R, Weksch G, Collings E W. Materails Properties Handbook:Titanium Alloys.Materials Park,OH: AMS,1994: 411 [9] Cui W F,Liu C M, Zhou L,Luo G Z.Mater Sci Eng, 2002; A323: 192 [10] Singh A K,Ramachandra C.J Mater Sci,1997; 32: 229 [11] Ramachandra C, Singh V.Metall Trans,1992; 23A:689 [12] Bulanova M, Firstov S,Gornaya I,Miracle D. J Alloys Compd, 2004; 384: 106 [13] Weinem D,Kumpfert J,Peters M,Kaysser W A.Mater Sci Eng, 1996; A206: 55 [14] Lutjering G,Williams.Titaniu.Heidelberg:Springer-Verlag 2003: 232 [15] Cui Z Q. Metallurgy and Heat Treatment. Beijing: China Machine Press, 2000: 138 (崔忠圻.金属学与热处理.北京:机械工业出版社,2000:138) |