LI Jianguo; Hu Dongping; MEI Jun; LIU Shi; LI Yiyi. Enhancing Adhesion Between Diamond Film and WC--Co Substrate. Acta Metall Sin, 2006, 42(7): 763-769 .
Abstract The effect of Murakami solution and H2 plasma treatment on the morphology and structure of tungsten carbide-cobalt has been investigated by the use of SEM and XRD. Then these pretreated tungsten carbide-cobalt tools were coated with multiple diamond film. Finally, the adhesion between diamond film and WC-Co substrate was evaluated with indentation method and drilling test. The Murakami solution treatment induced uniform corrugation on tungsten carbide-cobalt surface, as a result, the critical load of diamond film of this treatment is about 1.5kN examined with indentation method, but the diamond coated drill pretreated with Murakami solution has a bad cutting performance. H2 plasma treatment promoted WC grain more coarse and closed, thus, the critical load of diamond film of this treatment is more than 1.5kN and the diamond coated drill pretreated with H2 plasma demonstrated excellent cutting performance.
[1] Mallika K,Komanduri R. Wear, 1999; 224: 245 [2] Marinkovic S,Stankvic S,Rakocevic Z. Thin Solid Films, 1999; 354: 118 [3] Deuerler F,Pies M,van den Berg H,Tabersky R, Buck V. Phys Status Solidi, 1996; A154: 403 [4] Singh R K, Gilbert D R,Gerald F,Harkness S, Lee D G. Science, 1996; 272: 396 [5] Tsai C,Nelson J C,Gerberich W W,Heberlein J, Pfender E. Diamond Relat Mater, 1993; 2: 617 [6] Jagannadham K,Fan N D,Komanduri R,Narayanet J. J Vac Sci Tehnol, 1997; 15A: 2264 [7] Cremer R,Mertens R,Neuschutz D,Lemmer O,Frank M, Leyendecker T.Thin Solid Films, 1999; 355/356: 127 [8] Miao J Q, Song J H, Zhao Z Q, Yang Z W, Tong Y M, Tang W Z, Lu F X.Diamond Abrasives Eng, 2003; (4): 5 (苗晋琦,宋建华,赵中琴,杨志威,佟玉梅,唐伟忠,吕反修. 金刚石与磨料磨具工程,2003;(4):5) [9] Tsubota T, Ida S, Okada N, Nagata M,Matsumoto Y,Yatsushiro N. Surf Coat Technol, 2003; 169/170: 262 [10] Ostwald W, Leipzig Z. Phys Chem, 1900; 34: 495 [11] Lee D G, Fitz-Gerald J M, Singh R K. Surf Coat Technol,1998; 100/101: 187 [12] Miao J Q, Song J H, Xue R D, Tong Y M, Tang W Z, Lu F X. J Synth Cryst, 2003; 32: 371 (苗晋琦,宋建华,薛润东,佟玉梅,唐伟忠,吕反修.人工晶 体学报,2003;32:371)
LIU Changqing;JIN Zhujing;YU Li;YU Zhiming;WU Weitao Corrosion Science Laboratory; Institute of Corrsion and Protection of Metals; Academia Sinica; Shenyang. EVALUATION OF ADHESION AND PLASTICITY OF PVD FILMS[J]. 金属学报, 1992, 28(4): 77-82.