| Research Progress on Alloying Regulation of Strengthening, Toughening, and Oxidation Resistance in Nb-Si-Based Ultrahigh-Temperature Alloys |
LI Yunlong1( ), ZHANG Zirun1, YU Jun2, ZHAO Zhanyong1, LIN Xin2( ), BAI Peikang1 |
1 Provincial Key Laboratory of Metal Solidification Control and Additive Manufacturing, North University of China, Taiyuan 030051, China 2 State Key Laboratory of Solidification Processing, Northwestern Polytechnical University, Xi'an 710072, China |
|
Cite this article:
LI Yunlong, ZHANG Zirun, YU Jun, ZHAO Zhanyong, LIN Xin, BAI Peikang. Research Progress on Alloying Regulation of Strengthening, Toughening, and Oxidation Resistance in Nb-Si-Based Ultrahigh-Temperature Alloys. Acta Metall Sin, 2026, 62(10): 1635-1654.
|
|
|
Abstract Nb-Si-based ultrahigh-temperature alloys are considered promising candidates to replace conventional Ni-based superalloys in hot-end aerospace components operating at 1200-1400 oC owing to their high melting point, low density, high-temperature strength, and creep resistance. Their microstructures generally comprise a niobium solid solution (Nbss) and silicide phases, with the Nbss providing room-temperature toughness and the silicides imparting high-temperature strength and thermal stability. However, the inherent brittleness of the silicides, insufficient continuity of the Nbss phase, and the difficulty of forming a stable protective oxide scale at elevated temperatures create a long-standing trade-off between room-temperature fracture toughness and high-temperature oxidation resistance, thereby severely limiting the engineering applications of these alloys. This review focuses on the relationships among processing technology, microstructure, and properties in Nb-Si-based alloys. The effects of directional solidification, arc melting, powder metallurgy, and additive manufacturing on phase constitution, microstructural characteristics, and properties are systematically summarized. Particular attention is given to the roles of Ti, Zr, Mo, Cr, Al, B, Ta, Hf, and rare-earth elements in phase stabilization, microstructure optimization, strengthening, toughening, and oxidation resistance. In addition, the synergistic and antagonistic effects of multi-element alloying are discussed in terms of suppressing Nb3Si formation, stabilizing beneficial silicides, maintaining Nbss continuity, and promoting the formation of protective oxide scales. Finally, current challenges, including the lack of unified performance evaluation criteria, insufficient understanding of composition-process coupling, and limited design strategies for simultaneously enhancing toughness and oxidation resistance, are highlighted. Future directions for the design and development of high-performance Nb-Si-based ultrahigh-temperature alloys for extreme service environments are also proposed.
|
|
Received: 16 April 2026
|
|
|
| Fund: National Natural Science Foundation of China(52405433);Fundamental Research Program of Shanxi Province(202403021212119) |
Corresponding Authors:
LI Yunlong, associate professor, Tel: 15702962668, E-mail: lyunlong@nuc.edu.cn; LIN Xin, professor, Tel: (029)88494001, E-mail: xlin@nwpu.edu.cn
|
| [1] |
Bewlay B P, Lewandowksi J J, Jackson M R. Refractory metal-intermetallic in-situ composites for aircraft engines[J]. JOM, 1997, 49(8): 44
|
| [2] |
Busby J T, Leonard K J. Space fission reactor structural materials: Choices past, present, and future[J]. JOM, 2007, 59(4): 20
|
| [3] |
Bewlay B P, Jackson M R, Zhao J C, et al. A review of very-high-temperature Nb-silicide-based composites[J]. Metall. Mater. Trans., 2003, 34A: 2043
|
| [4] |
Bewlay B P, Jackson M R, Zhao J C, et al. Ultrahigh-temperature Nb-silicide-based composites[J]. MRS Bull., 2003, 28: 646
doi: 10.1557/mrs2003.192
|
| [5] |
Liu W, Huang S, Ye C T, et al. Progress in Nb-Si ultra-high temperature structural materials: A review[J]. J. Mater. Sci. Technol., 2023, 149:127
doi: 10.1016/j.jmst.2022.11.022
|
| [6] |
Qi C K, Li S R, Liu Y C, et al. Overview of powder forming research on Nb-Si-based ultra-high temperature alloys[J]. Mater. Today Adv., 2024, 24: 100537
|
| [7] |
Subramanian P R, Mendiratta M G, Dimiduk D M, et al. Advanced intermetallic alloys—Beyond gamma titanium aluminides[J]. Mater. Sci. Eng., 1997, A239-240: 1
|
| [8] |
Zhu F, Hu P, Ge S W, et al. Research progress of high temperature oxidation behavior of Nb-Si based alloys and their coatings[J]. Rare Met. Mater. Eng., 2023, 52: 4340
|
|
朱 飞, 胡 平, 葛松伟 等. Nb-Si基合金及其涂层的高温氧化行为研究进展[J]. 稀有金属材料与工程, 2023, 52: 4340
|
| [9] |
Li Z, Peng L M. Microstructural and mechanical characterization of Nb-based in situ composites from Nb-Si-Ti ternary system[J]. Acta Mater., 2007, 55: 6573
doi: 10.1016/j.actamat.2007.08.012
|
| [10] |
Ding H S, Nie G, Chen R R, et al. Directional solidification of TiAl-W-Si alloy by electromagnetic confinement of melt in cold crucible[J]. Intermetallics, 2012, 31: 264
doi: 10.1016/j.intermet.2012.07.018
|
| [11] |
Ma X, Guo X P, Fu M S, et al. Crystallographic characteristics of an integrally directionally solidified Nb-Ti-Si based in-situ composite[J]. Scr. Mater., 2017, 139: 108
doi: 10.1016/j.scriptamat.2017.06.035
|
| [12] |
He D D, Feng Q S, Fu Y X, et al. Erosion behaviors of BaZrO3 and BaZrO3/Y2O3 dual-phase refractories within Nb-Si melts during vacuum induction melting[J]. J. Mater. Res. Technol., 2024, 33: 9726
doi: 10.1016/j.jmrt.2024.12.005
|
| [13] |
Guo Y L, He J Y, Li Z M, et al. Tuning microstructures and improving oxidation resistance of Nb-Si based alloys via electron beam surface melting[J]. Corros. Sci., 2020, 163: 108281
doi: 10.1016/j.corsci.2019.108281
|
| [14] |
Orrù R, Licheri R, Locci A M, et al. Consolidation/synthesis of materials by electric current activated/assisted sintering[J]. Mater. Sci. Eng., 2009, R63: 127
|
| [15] |
Liu W, Sha J B. Failure mode transition of Nb phase from cleavage to dimple/tear in Nb-16Si-based alloys prepared via spark plasma sintering[J]. Mater. Des., 2016, 111: 301
doi: 10.1016/j.matdes.2016.08.087
|
| [16] |
Li Y L, Lin X, Hu Y L, et al. Microstructure and isothermal oxidation behavior of Nb-Ti-Si-based alloy additively manufactured by powder-feeding laser directed energy deposition[J]. Corros Sci., 2020, 173: 108757
doi: 10.1016/j.corsci.2020.108757
|
| [17] |
Guo Y L, Jia L N, Sun S B, et al. Rapid fabrication of Nb-Si based alloy by selective laser melting: Microstructure, hardness and initial oxidation behavior[J]. Mater. Des., 2016, 109: 37
doi: 10.1016/j.matdes.2016.07.048
|
| [18] |
Guo Y L, Jia L N, Kong B, et al. Improvement in the oxidation resistance of Nb-Si based alloy by selective laser melting[J]. Corros Sci., 2017, 127: 260
doi: 10.1016/j.corsci.2017.08.022
|
| [19] |
Guo H S, Guo X P. Microstructure and microhardness of directionally solidified and heat-treated Nb-Ti-Si based ultrahigh temperature alloy[J]. Trans. Nonferrous Met. Soc. China, 2011, 21: 1283
doi: 10.1016/S1003-6326(11)60854-6
|
| [20] |
Wang J Y, Jia L N, Ma L M, et al. Microstructure optimization of directionally solidified hypereutectic Nb-Si alloy[J]. Trans. Nonferrous Met. Soc. China, 2013, 23: 2874
doi: 10.1016/S1003-6326(13)62809-5
|
| [21] |
Liu T, Li T J, Cao Y K, et al. Improvement in the oxidation resistance of Nb-16Si-24Ti-2Al-2Cr alloy by hot pressing[J]. Int. J. Refract. Met. Hard Mater., 2024, 120: 106605
doi: 10.1016/j.ijrmhm.2024.106605
|
| [22] |
Kumar M D B, Madesh R, Adarsh S J, et al. Recent developments and future perspectives in metal additive manufacturing: Techniques, challenges, and functional performance[J]. J Alloys Compd., 2026, 1064: 187718
doi: 10.1016/j.jallcom.2026.187718
|
| [23] |
Liu W, Ren X Y, Li N, et al. Rapid directionally solidified microstructure characteristic and fracture behaviour of laser melting deposited Nb-Si-Ti alloy[J]. Prog. Nat. Sci. Mater. Int., 2021, 31: 113
doi: 10.1016/j.pnsc.2020.12.003
|
| [24] |
Li M, Kang Y W, Guo F W. Research progress in manufacturing technology of Nb-Si based ultra-high temperature structural materials[J]. J. Mater. Eng., 2020, 48: 58
doi: 10.11868/j.issn.1001-4381.2020.000284
|
| [25] |
Sha J B, Hirai H, Tabaru T, et al. High-temperature strength and room-temperature toughness of Nb-W-Si-B alloys prepared by arc-melting[J]. Mater. Sci. Eng., 2004, A364: 151
|
| [26] |
Sun Z P, Guo X P, He Y S, et al. Investigation on the as-cast microstructure of Nb-Nb silicide based multicomponent alloys[J]. Intermetallics, 2010, 18: 992
doi: 10.1016/j.intermet.2010.01.024
|
| [27] |
Sala K, Mitra R. Effect of Ti addition and microstructural evolution on toughening and strengthening behavior of as cast or annealed Nb-Si-Mo based hypoeutectic and hypereutectic alloys[J]. Metall. Mater. Trans., 2021, 52A: 3436
|
| [28] |
Li Y L, Lin X, Hu Y L, et al. Precipitation behavior of Nb-Si-based in-situ composite manufactured by laser directed energy deposition[J]. Scr. Mater., 2022, 207: 114288
doi: 10.1016/j.scriptamat.2021.114288
|
| [29] |
Li Y L, Lin X, Hu Y L, et al. Zirconium modified Nb-22Ti-16Si alloys fabricated by laser additive manufacturing: Microstructure and fracture toughness[J]. J. Alloys Compd., 2019, 783: 66
doi: 10.1016/j.jallcom.2018.12.280
|
| [30] |
Sankar M, Phanikumar G, Satya Prasad V V. Effect of Zr addition on the mechanical properties of Nb-Si based alloys[J]. Mater. Sci. Eng., 2019, A754: 224
|
| [31] |
Zhang S N, Jia L N, Guo Y L, et al. Improvement in the oxidation resistance of Nb-Si-Ti based alloys containing zirconium[J]. Corros. Sci., 2020, 163: 108294
doi: 10.1016/j.corsci.2019.108294
|
| [32] |
Xu Q, Ma X H, Wang Q, et al. Formation of (Nb, X)ss/β-(Nb, X)5Si3 eutectic and its effect on mechanical properties of Nb-Si-Ti alloys by addition of Mo[J]. Mater. Today Commun., 2025, 42: 111556
|
| [33] |
Ma R, Guo X P. Influence of molybdenum contents on the microstructure, mechanical properties and oxidation behavior of multi-elemental Nb-Si based ultrahigh temperature alloys[J]. Intermetallics, 2021, 129: 107053
doi: 10.1016/j.intermet.2020.107053
|
| [34] |
Wang Q, Wang X W, Chen R R, et al. Microstructure evolution and fracture toughness of Nb-Si-Ti based alloy with Cr, Mo and W elements addition[J]. Intermetallics, 2022, 140: 107408
doi: 10.1016/j.intermet.2021.107408
|
| [35] |
Su L F, Jia L N, Jiang K Y, et al. The oxidation behavior of high Cr and Al containing Nb-Si-Ti-Hf-Al-Cr alloys at 1200 and 1250 oC[J]. Int. J. Refract. Met. Hard Mater., 2017, 69: 131
doi: 10.1016/j.ijrmhm.2017.08.006
|
| [36] |
Portillio B I, Varma S K. Oxidation behavior of Nb-20Mo-15Si-25Cr and Nb-20Mo-15Si-25Cr-5B alloys[J]. Metall. Mater. Trans., 2012, 43A: 147
|
| [37] |
Sha J, Yang C, Liu J. Toughening and strengthening behavior of an Nb-8Si-20Ti-6Hf alloy with addition of Cr[J]. Scr. Mater., 2010, 62: 859
doi: 10.1016/j.scriptamat.2010.02.023
|
| [38] |
Sun Z P, Guo J M, Zhang C, et al. Effect of Ti and Al interaction on microstructures and mechanical properties of the Nb-Ti-Si-Al alloys[J]. Rare Met. Mater. Eng., 2016, 45: 1678
doi: 10.1016/S1875-5372(16)30139-4
|
| [39] |
Yu J Y, Chen D Z, Xu F D, et al. Simultaneous improving high temperature oxidation resistance and room temperature toughness of Nb-Si based alloy via appropriate Ta content addition strategy[J]. Int. J. Refract. Met. Hard Mater., 2024, 124: 106800
doi: 10.1016/j.ijrmhm.2024.106800
|
| [40] |
Wang Q, Zhao T Y, Chen R R, et al. Collaborative optimization of microstructure, phase composition and room-temperature fracture toughness of Nb-Si based alloys using Ti, Zr and Hf elements[J]. Trans. Nonferrous Met. Soc. China, 2024, 34: 194
doi: 10.1016/S1003-6326(23)66391-5
|
| [41] |
Li Z F, Tsakiropoulos P. On the microstructures and hardness of the Nb-24Ti-18Si-5Al-5Cr-5Ge and Nb-24Ti-18Si-5Al-5Cr-5Ge-5Hf (at.%) silicide based alloys[J]. Materials, 2019, 12: 2655
doi: 10.3390/ma12172655
|
| [42] |
Vazquez A, Varma S K. High-temperature oxidation behavior of Nb-Si-Cr alloys with Hf additions[J]. J. Alloys Compd., 2011, 509: 7027
doi: 10.1016/j.jallcom.2011.02.174
|
| [43] |
Wang X W, Wang Q, Chen R R, et al. Improved microstructure and mechanical properties of Nb-Si in situ composites: Focus on interstitial element B doping, atomic diffusion and dislocation behaviors[J]. Mater. Sci. Eng., 2025, A946: 149097
|
| [44] |
Zhang S, Guo X P. Effects of B addition on the microstructure and properties of Nb silicide based ultrahigh temperature alloys[J]. Intermetallics, 2015, 57: 83
doi: 10.1016/j.intermet.2014.10.007
|
| [45] |
Guo J T, Zhou L Z, Tian Y X, et al. Effect of Hf, Sn, Ta, Zr, Dy and Ho on microstructure and mechanical properties of Nb-Nb5Si3 alloy[J]. Acta Metall. Sin., 2015, 51: 815
|
|
郭建亭, 周兰章, 田玉新 等. 合金元素Hf, Sn, Ta, Zr, Dy和Ho对Nb-Nb5Si3合金组织和力学性能的影响[J]. 金属学报, 2015, 51: 815
|
| [46] |
Tian Y X, Guo J T, Zhou L Z, et al. Effect of Dy addition on microstructure and mechanical properties of Nb-Nb5Si3 eutectic alloy[J]. Acta Metall. Sin., 2008, 44: 589
|
|
田玉新, 郭建亭, 周兰章 等. Dy对Nb-Nb5Si3共晶合金显微组织和力学性能的影响[J]. 金属学报, 2008, 44: 589
|
| [47] |
Chen D Z, Wang Q, Chen R R, et al. An as-cast Nb-Si-based alloy with fine-grains and remarkable fracture toughness by minor Sc addition[J]. J. Alloys Compd., 2022, 895: 162707
doi: 10.1016/j.jallcom.2021.162707
|
| [48] |
Chen D Z, Wang Y X, Yu J Y, et al. Er-induced microstructural refinement and internal oxidation enhancing fracture toughness in Nb-Si alloys[J]. J. Alloys Compd., 2025, 1045: 184777
doi: 10.1016/j.jallcom.2025.184777
|
| [49] |
Cui X Y, Chen D Z, Xu F D, et al. Investigating scandium-alloyed Nb-Si systems: Microstructure, oxidation behavior, and fracture toughness[J]. Mater. Charact., 2024, 217: 114409
doi: 10.1016/j.matchar.2024.114409
|
| [50] |
Guo Y L, Jia L N, Zhang H R, et al. Enhancing the oxidation resistance of Nb-Si based alloys by yttrium addition[J]. Intermetallics, 2018, 101: 165
doi: 10.1016/j.intermet.2018.08.004
|
| [51] |
Wang X W, Wang Q, Chen R R, et al. Gadolinium doping induced the microstructure evolution and mechanical properties improvement of Nb-Si based in-situ superalloy[J]. J. Alloys Compd., 2024, 1004: 175942
doi: 10.1016/j.jallcom.2024.175942
|
| [52] |
Wang Y, Jia L N, Sun G X, et al. Synchronous improvement in room-temperature fracture toughness and high-temperature oxidation resistance of Nb-Si based alloys with erbium addition[J]. Int. J. Refract. Met. Hard Mater., 2021, 94: 105359
doi: 10.1016/j.ijrmhm.2020.105359
|
| [53] |
Wei W, Wang Q, Chen R R, et al. Improved toughness and oxidation resistance of Nb-Si based ultra-high temperature alloys by in-situ generated La2O3 phase[J]. Mater. Charact., 2024, 208: 113686
doi: 10.1016/j.matchar.2024.113686
|
| [54] |
Yin X Y, Li X X, Sun H, et al. Fine microstructure, better compactness, and significant fracture toughness of multi-component Nb-Si based alloy by an appropriate amount of yttrium addition during the laser melting deposition[J]. Int. J. Refract. Met. Hard Mater., 2026, 137: 107655
doi: 10.1016/j.ijrmhm.2026.107655
|
| [55] |
Launey M E, Ritchie R O. On the fracture toughness of advanced materials[J]. Adv. Mater., 2009, 21: 2103
doi: 10.1002/adma.v21:20
|
| [56] |
Chan K S, Davidson D L. Effects of Ti addition on cleavage fracture in Nb-Cr-Ti solid-solution alloys[J]. Metall. Mater. Trans., 1999, 30A: 925
|
| [57] |
Li Y L, Lin X, Hu Y L, et al. Microstructure and fracture toughness of a Nb-Ti-Si-based in-situ composite fabricated by laser-based directed energy deposition[J]. Composites, 2024, 278B: 111427
|
| [58] |
Qiao Y Q, Guo X P, Zeng Y X. Study of the effects of Zr addition on the microstructure and properties of Nb-Ti-Si based ultrahigh temperature alloys[J]. Intermetallics, 2017, 88: 19
doi: 10.1016/j.intermet.2017.04.008
|
| [59] |
Li Z B, Luo L S, Wang B B, et al. The microstructural characteristics and mechanical properties of Nb-16Si-22Ti-2Al-2Cr alloys with Zr addition[J]. Mater. Sci. Eng., 2023, A880: 145305
|
| [60] |
Li Y L, Lin X, Hu Y L, et al. The effect of Mo on microstructure and mechanical properties of Nb-22Ti-16Si alloy additively manufactured via laser directed energy deposition[J]. J. Alloys Compd., 2021, 858: 158143
doi: 10.1016/j.jallcom.2020.158143
|
| [61] |
Zhang S, Guo X P. Effects of Cr and Hf additions on the microstructure and properties of Nb silicide based ultrahigh temperature alloys[J]. Mater. Sci. Eng., 2015, A638: 121
|
| [62] |
Guo Y L, Jia L N, Kong B, et al. Microstructure and fracture toughness of Nb-Si based alloys with Ta and W additions[J]. Intermetallics, 2018, 92: 1
doi: 10.1016/j.intermet.2017.09.005
|
| [63] |
Tian Y X, Guo J T, Zhou L Z, et al. Microstructure and room temperature fracture toughness of cast Nbss/silicides composites alloyed with Hf[J]. Mater. Lett., 2008, 62: 2657
doi: 10.1016/j.matlet.2008.01.007
|
| [64] |
Kim J H, Tabaru T, Sakamoto M, et al. Mechanical properties and fracture behavior of an Nbss/Nb5Si3 in-situ composite modified by Mo and Hf alloying[J]. Mater. Sci. Eng., 2004, A372: 137
|
| [65] |
Sala K, Kashyap S K, Mitra R. Effect of Ti addition on the kinetics and mechanism of non-isothermal and isothermal oxidation of Nb-Si-Mo alloys at 900 oC-1200 oC[J]. Intermetallics, 2021, 138: 107338
doi: 10.1016/j.intermet.2021.107338
|
| [66] |
Yao D Z, Zhou C G, Yang J Y, et al. Experimental studies and modeling of the oxidation of multiphase niobium-base alloys[J]. Corros. Sci., 2009, 51: 2619
doi: 10.1016/j.corsci.2009.06.053
|
| [67] |
Li Y L, Lin X, Zhao Z Y, et al. Investigation on the composite effect of Zr and Cr on oxidation behavior and fracture toughness of Nb-Ti-Si-based alloys manufactured by directed energy deposition[J]. Mater. Charact., 2024, 214: 114078
doi: 10.1016/j.matchar.2024.114078
|
| [68] |
Shen F Q, Yu L H, Fu T, et al. Effect of the Al, Cr and B elements on the mechanical properties and oxidation resistance of Nb-Si based alloys: A review[J]. Appl. Phys., 2021, 127A: 852
|
| [69] |
Li N, Zhang B D, Huang H, et al. Discussion of effects of Hf on the high temperature oxidation of Nb-based alloy[J]. New Technol. New Process, 2015, (4): 103
|
|
李 宁, 张宝东, 黄 辉 等. 铪提高铌硅基合金高温抗氧化性能的机理探讨[J]. 新技术新工艺, 2015, (4): 103
|
| [70] |
Li Y L, Lin X, Hu Y L, et al. Alloying on the high-temperature oxidation behavior of Nb-Ti-Si-based alloy additively manufactured by laser directed energy deposition[J]. Int. J. Refract. Met. Hard Mater., 2024, 121: 106682
doi: 10.1016/j.ijrmhm.2024.106682
|
| [71] |
Ma R, Guo X P. Effects of Mo and Zr composite additions on the microstructure, mechanical properties and oxidation resistance of multi-elemental Nb-Si based ultrahigh temperature alloys[J]. J. Alloys Compd., 2021, 870: 159437
doi: 10.1016/j.jallcom.2021.159437
|
| [72] |
Sun A K, Dong Z Q, Yang S, et al. Effect of Zr and Ti on isothermal oxidation behavior of Nb-Si based alloys[J]. Prog. Nat. Sci. Mater. Int., 2022, 32: 226
doi: 10.1016/j.pnsc.2022.02.004
|
| [73] |
Li Z B, Luo L S, Wang B B, et al. Cooperative effects of Mo and B additions on the microstructure and mechanical properties of multi-elemental Nb-Si-Ti based alloys[J]. Mater. Charact., 2023, 206: 113421
doi: 10.1016/j.matchar.2023.113421
|
| [74] |
Ma R, Guo X P. Cooperative effects of Mo, V and Zr additions on the microstructure and properties of multi-elemental Nb-Si based alloys[J]. J. Mater. Sci. Technol., 2023, 132: 27
doi: 10.1016/j.jmst.2022.06.006
|
| [75] |
Li Y L, Lin X, Hu Y L, et al. Seynergistic effect of Mo and Zr additions on microstructure and mechanical properties of Nb-Ti-Si-based alloys additively manufactured by laser directed energy deposition[J]. J. Mater. Sci. Technol., 2022, 103: 84
doi: 10.1016/j.jmst.2021.06.027
|
| [76] |
Prasad S, Paul A. Growth mechanism of the Nb(X)Si2 and [Nb(X)]5Si3 phases by reactive diffusion in Nb (X = Ti, Mo, or Zr)-Si systems[J]. Intermetallics, 2012, 22: 210
doi: 10.1016/j.intermet.2011.11.012
|
| [77] |
Sun G X, Jia L N, Ye C T, et al. Balancing the fracture toughness and tensile strength by multiple additions of Zr and Y in Nb-Si based alloys[J]. Intermetallics, 2021, 133: 107172
doi: 10.1016/j.intermet.2021.107172
|
| [78] |
Liu G X, Jia L N, Kong B, et al. Artificial neural network application to study quantitative relationship between silicide and fracture toughness of Nb-Si alloys[J]. Mater. Des., 2017, 129: 210
doi: 10.1016/j.matdes.2017.05.027
|
| [79] |
Ma E, Shin S H, Choi W, et al. Machine learning approach for predicting the fracture toughness of Nb-Si based alloys[J]. Int. J. Refract. Met. Hard Mater., 2023, 117: 106420
doi: 10.1016/j.ijrmhm.2023.106420
|
| [80] |
Yin X Y, Liang J, Liu C, et al. Accelerating the design of multivariate Nb-Si based alloys with excellent strength and toughness matching through machine learning[J]. Next Mater., 2025, 6: 100294
|
| [81] |
Liu G X, Jia L N, Kong B, et al. Artificial neural network application to microstructure design of Nb-Si alloy to improve ultimate tensile strength[J]. Mater. Sci. Eng., 2017, A707: 452
|
| No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|