Research Progress on Alloying Regulation of Strengthening, Toughening, and Oxidation Resistance in Nb-Si-Based Ultrahigh-Temperature Alloys
LI Yunlong1(), ZHANG Zirun1, YU Jun2, ZHAO Zhanyong1, LIN Xin2(), BAI Peikang1
1 Provincial Key Laboratory of Metal Solidification Control and Additive Manufacturing, North University of China, Taiyuan 030051, China
2 State Key Laboratory of Solidification Processing, Northwestern Polytechnical University, Xi'an 710072, China
Cite this article: 

LI Yunlong, ZHANG Zirun, YU Jun, ZHAO Zhanyong, LIN Xin, BAI Peikang. Research Progress on Alloying Regulation of Strengthening, Toughening, and Oxidation Resistance in Nb-Si-Based Ultrahigh-Temperature Alloys. Acta Metall Sin, 2026, 62(10): 1635-1654.

Download:  HTML  PDF(2260KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  

Nb-Si-based ultrahigh-temperature alloys are considered promising candidates to replace conventional Ni-based superalloys in hot-end aerospace components operating at 1200-1400 oC owing to their high melting point, low density, high-temperature strength, and creep resistance. Their microstructures generally comprise a niobium solid solution (Nbss) and silicide phases, with the Nbss providing room-temperature toughness and the silicides imparting high-temperature strength and thermal stability. However, the inherent brittleness of the silicides, insufficient continuity of the Nbss phase, and the difficulty of forming a stable protective oxide scale at elevated temperatures create a long-standing trade-off between room-temperature fracture toughness and high-temperature oxidation resistance, thereby severely limiting the engineering applications of these alloys. This review focuses on the relationships among processing technology, microstructure, and properties in Nb-Si-based alloys. The effects of directional solidification, arc melting, powder metallurgy, and additive manufacturing on phase constitution, microstructural characteristics, and properties are systematically summarized. Particular attention is given to the roles of Ti, Zr, Mo, Cr, Al, B, Ta, Hf, and rare-earth elements in phase stabilization, microstructure optimization, strengthening, toughening, and oxidation resistance. In addition, the synergistic and antagonistic effects of multi-element alloying are discussed in terms of suppressing Nb3Si formation, stabilizing beneficial silicides, maintaining Nbss continuity, and promoting the formation of protective oxide scales. Finally, current challenges, including the lack of unified performance evaluation criteria, insufficient understanding of composition-process coupling, and limited design strategies for simultaneously enhancing toughness and oxidation resistance, are highlighted. Future directions for the design and development of high-performance Nb-Si-based ultrahigh-temperature alloys for extreme service environments are also proposed.

Key words:  Nb-Si-based ultrahigh-temperature alloy      alloying regulation      phase stability      microstructural optimization      fracture toughness      high-temperature oxidation resistance     
Received:  16 April 2026     
ZTFLH:  TG146.4  
Fund: National Natural Science Foundation of China(52405433);Fundamental Research Program of Shanxi Province(202403021212119)
Corresponding Authors:  LI Yunlong, associate professor, Tel: 15702962668, E-mail: lyunlong@nuc.edu.cn;
LIN Xin, professor, Tel: (029)88494001, E-mail: xlin@nwpu.edu.cn

URL: 

https://www.ams.org.cn/EN/10.11900/0412.1961.2026.00109     OR     https://www.ams.org.cn/EN/Y2026/V62/I10/1635

Fig.1  Binary phase diagram of the Nb-Si system (Blue area indicates the major phase fields/composition ranges that this review focuses on)[9]
Fig.2  Schematics of phase constitution, microstructural roles, and core bottlenecks of Nb-Si-based ultrahigh-temperature alloys (Nbss—niobium solid solution)
Fig.3  Preparation processes of different Nb-Si-based ultrahigh-temperature alloys and their typical microstructures
(a) directional solidification (DS) [10] and the aligned microstructures[11](b) vacuum induction melting (VIM) [12] and as-cast coarse microstructures[13](c) spark plasma sintering (SPS) [14] and refined grains[15](d) laser directed energy deposition (LDED) and the continuous Nbss morphologies[16] (e) laser powder bed fusion (LPBF) [17] and the ultrafine microstructures[18] (BD—building direction, h—hatching distance)
ProcessMicrostructure characteristic

Main advantage

Main limitationRepresentative application

Arc melting[24-26]

Coarse as-cast structure;microsegregation;shrinkage cavities;limited Nbss continuity controlMature process;flexible alloy design;convenient for composition explorationInhomogeneous solidification;casting defects;limited ingot sizeAlloy preparation; composition optimization; phase analysis

Powder metallurgy[5,15,21]

Refined grains;high densification;uniform phase distributionGrain refinement; defect reduction; improved microstructure homogeneityHigh powder cost; bulk size limit; complex processingDense bulk alloy fabrication; fine-grained design

Directional solidification[5,19,20]

Refined silicides; ordered phase alignment; directional Nbss/silicides distributionExcellent high-temperature strength, creep resistance; directional load-bearingNarrow processing window; strict equipment control; poor room-temperature toughnessHigh-temperature alloy development; creep-resistant design

Additive manufacturing[5,18,23]

Ultrafine structure;reduced dendrite spacing; enhanced Nbss continuityNear-net shaping of complex parts; strong grain refinement; rapid composition iterationHigh residual stress; pronounced anisotropy; unstable process parametersComplex component fabrication; rapid alloy development
Table 1  Comparisons of major preparation processes for Nb-Si-based ultrahigh-temperature alloys[5,15,18-21,23-26]
Fig.4  BSE images of Nb-16Si-xZr alloy[30]
(a) x = 0 (b) x = 2 (c) x = 4 (d) x = 6
Fig.5  Low (a, c, e, g) and high (b, d, f, h) magnified BSE images of arc-melted Nb-22Ti-16Si-5Cr-4Hf-3Al-xB alloys[44](The rectangle areas in Figs.5b, d, f, and h indicate the regions containing Nbss/(Nb, X)5Si3/Cr2(Nb, X) three-phase eutectics)
(a, b) x = 0 (c, d) x = 2 (e, f) x = 5 (g, h) x = 10
Fig.6  Toughening mechanism of Nb-Si-based ultrahigh-temperature alloys[55]
Fig.7  Mechanical properties of Nb-16Si-22Ti-2Al-2Cr alloy with different Zr contents obtained by arc melting[59]
(a) loading-displacement curves(b) room-temperature fracture toughness (KQ)(c) volume fractions of constituent phases(d) true stress-strain curves(e) high-temperature compression strengths and variable quantities
Fig.8  Schematics of antioxidation mechanism of Nb-Si-based ultrahigh-temperature alloys
(a) Nb2O5-dominated failure mechanism (b) composite oxide protective layer (RE—rare earth)
Fig.9  Effects of Zr addition on high-temperature oxidation resistance of Nb-Si-based ultrahigh-temperature alloys[31]
(a1, a2) weight gain versus time (a1) and the square root of time (a2)(b) macroscopic morphologies before and after oxidation at 1300 oC for 100 h(c1-c5) cross-sectional SEM images of the oxide layer in 0Zr (c1), 1Zr (c2), 3Zr (c3), 5Zr (c4), and 7Zr (c5) alloys(d) BSE image and corresponding EDS elemental mappings of the oxide layer

Alloying

element

Main oxide-scale featureProtective effectMain trade-off

Ti[65]

TiO2-containing composite scale, Ti-rich outer layer; can form denser layer at high temperature

Improves compactness at > 1100 oC

Poor efficacy at lower temperatures; clear temperature window

Zr[31,58]

ZrO2 particles/regions; improved continuity of inner SiO2 layerZrO2 fills defects, reduces porosity, stabilizes protective sublayerExcess Zr increases brittle silicide fraction and degrades mechanical balance

Mo[33]

Less porous at suitable content; excessive Mo introduces pores and fast-diffusion pathsOptimizes phase constitution and indirectly retards oxidation at appropriate levelsNarrow beneficial window; overaddition aggravates oxidation via pore formation

Cr[35,66-68,70]

Forms Cr2O3, CrNbO4, or Cr-enriched outer scale; promotes dense external protective layerEnhances compactness and slows inward oxygen diffusionOften sacrifices room temperature toughness

Al[35,68]

Forms relatively dense Al2O3-containing scale; suppresses loose Nb2O5 growthImproves scale continuity, compactness, and oxygen-barrier capabilityReduces Nbss continuity and lowers room-temperature toughness

Ta[39]

Slightly denser scale; in some systems, helps reduce severe scale disruptionIndirectly optimizes phase constitution and oxidation responseVery narrow optimum (~1%, atomic fraction); over-addition reverses the benefit

Hf[42,69]

HfO2-containing scale or dispersed Hf-rich oxides; denser and more adherent multilayer architecture containing scale or dispersed Hf

Markedly improves scale adhesion, suppresses spallation, stabilizes protective layers

Increases density and cost; excessive Hf complicates phase constitution

B[36,44]

Alters oxidation response mainly through microstructure/eutectic modification, not by forming a dominant oxideRefines microstructure and helps construct a more uniform oxidation pathwayVery narrow window; excess B increases silicide fraction, impairing toughness and oxidation balance

Rare-earth element[45-54]

Forms stable rare-earth oxides or complex oxides (e.g., ErNbO4); denser and more adherent scaleReactive element effect: improves adhesion, suppresses cracking/spallation, reduces oxygen diffusion, purifies interfacesEffective only at trace/low levels; over-addition forms coarse oxides/inclusions that degrade integrity
Table 2  Comparisons of oxidation behavior of Nb-Si-based ultrahigh-temperature alloys modified by various alloying elements[31,33,35,36,39,42,44-54,58,65-70]
Fig.10  Design window of synergistic and negative synergistic effects in multicomponent alloying[40,61,71-74]
Fig.11  Synergistic effects of Mo and Zr on mechanical properties and high-temperature oxidation resistance of Nb-Si-based ultrahigh-temperature alloys[71]
(a1-a5) KQ (a1) and fracture surface morphologies of 0Mo-0Zr (a2), 5Mo-0Zr (a3), 0Mo-4Zr (a4), and 5Mo-4Zr (a5) alloys
(b1-b5) high-temperature compression stress-strain curves (b1) and deformation microstructures of 0Mo-0Zr (b2), 5Mo-0Zr (b3), 0Mo-4Zr (b4), and 5Mo-4Zr (b5) alloys
(c1-c5) oxidation mass gain (c1) and microstructures of oxide layers of 0Mo-0Zr (c2), 5Mo-0Zr (c3), 0Mo-4Zr (c4), and 5Mo-4Zr (c5) alloys

Alloy

combination

Main benefitMain riskBest application target

Zr-Mo[71,75]

Improves phase stability, suppresses Nb3Si, refines microstructure, enhances both toughness and oxidation resistanceNarrow content windows; excess Mo embrittles Nbss and worsens oxidation, excess Zr increases brittle silicideBalanced design for toughness + high- temperature strength + oxidation resistance

Ti-Zr-Hf[40]

Stabilizes favorable silicide constitution, improves phase distribution, retains better strength-toughness balance than single additionsExcess total addition reduces Nbss continuity, raises silicide fraction, increases density/costIntegrated microstructure optimization focusing on phase stability and toughness retention

Cr-Hf[61]

Oxidation-oriented synergy: Cr builds protective external oxides, Hf improves scale adhesion and long-term stabilityStill increases brittle intermetallic fractions; room temperature toughness remains a concern if Cr is too highHigh-temperature oxidation resistance with improved scale stability
Cr-Al[35]Strong oxidation synergy via dense Cr/Al-containing protective scalesweakened Nbss continuity and increased brittle phasesOxidation-prioritized alloy design

Mo-B[73]

Strong high-temperature strengthening synergy via phase regulation + eutectic-path control; overall performance improves with careful B controlB has very narrow safe range; excess B sharply increases brittle silicide, excess Mo narrows toughness marginHigh-temperature strength and microstructure-regulated eutectic design

Zr-Ti[72]

In selected systems, improves room temperature toughness and compressive strength through combined refinement and phase-distribution optimizationBenefits not universal; oxidation benefit is limited and strongly system dependentToughness-oriented or mechanically balanced composition design

Mo-V[74]

May provide selective strengthening in some compositions

Often limited or antagonistic overall benefit; can increase phase complexity and reduce toughness if poorly controlledExploratory strengthening-oriented design, not mainstream balanced route

Ti-Zr-Mo[76]

Combines Ti-assisted phase adjustment, Zr refinement, and Mo-driven Nb3Si suppression; potentially beneficial for overall structural optimizationStrong system dependence; optimum balance shifts with base Si/Ti/Nb ratio and processing routeComprehensive phase-constitution and morphology control

RE-containing multicomponent[77]

Trace RE addition amplifies benefits of other elements via melt purification, interface improvement, oxide-scale stabilization, and microstructural refinementOver-addition introduces oxide inclusions, segregation, or coarse particles, offsetting synergyControlling inclusions, segregation, or coarse particles to preserve synergy
Table 3  Synergistic benefits, risks, and application targets of multicomponent alloying systems in Nb-Si-based ultrahigh-temperature alloys[35,40,61,71-77]
[1] Bewlay B P, Lewandowksi J J, Jackson M R. Refractory metal-intermetallic in-situ composites for aircraft engines[J]. JOM, 1997, 49(8): 44
[2] Busby J T, Leonard K J. Space fission reactor structural materials: Choices past, present, and future[J]. JOM, 2007, 59(4): 20
[3] Bewlay B P, Jackson M R, Zhao J C, et al. A review of very-high-temperature Nb-silicide-based composites[J]. Metall. Mater. Trans., 2003, 34A: 2043
[4] Bewlay B P, Jackson M R, Zhao J C, et al. Ultrahigh-temperature Nb-silicide-based composites[J]. MRS Bull., 2003, 28: 646
doi: 10.1557/mrs2003.192
[5] Liu W, Huang S, Ye C T, et al. Progress in Nb-Si ultra-high temperature structural materials: A review[J]. J. Mater. Sci. Technol., 2023, 149:127
doi: 10.1016/j.jmst.2022.11.022
[6] Qi C K, Li S R, Liu Y C, et al. Overview of powder forming research on Nb-Si-based ultra-high temperature alloys[J]. Mater. Today Adv., 2024, 24: 100537
[7] Subramanian P R, Mendiratta M G, Dimiduk D M, et al. Advanced intermetallic alloys—Beyond gamma titanium aluminides[J]. Mater. Sci. Eng., 1997, A239-240: 1
[8] Zhu F, Hu P, Ge S W, et al. Research progress of high temperature oxidation behavior of Nb-Si based alloys and their coatings[J]. Rare Met. Mater. Eng., 2023, 52: 4340
朱 飞, 胡 平, 葛松伟 等. Nb-Si基合金及其涂层的高温氧化行为研究进展[J]. 稀有金属材料与工程, 2023, 52: 4340
[9] Li Z, Peng L M. Microstructural and mechanical characterization of Nb-based in situ composites from Nb-Si-Ti ternary system[J]. Acta Mater., 2007, 55: 6573
doi: 10.1016/j.actamat.2007.08.012
[10] Ding H S, Nie G, Chen R R, et al. Directional solidification of TiAl-W-Si alloy by electromagnetic confinement of melt in cold crucible[J]. Intermetallics, 2012, 31: 264
doi: 10.1016/j.intermet.2012.07.018
[11] Ma X, Guo X P, Fu M S, et al. Crystallographic characteristics of an integrally directionally solidified Nb-Ti-Si based in-situ composite[J]. Scr. Mater., 2017, 139: 108
doi: 10.1016/j.scriptamat.2017.06.035
[12] He D D, Feng Q S, Fu Y X, et al. Erosion behaviors of BaZrO3 and BaZrO3/Y2O3 dual-phase refractories within Nb-Si melts during vacuum induction melting[J]. J. Mater. Res. Technol., 2024, 33: 9726
doi: 10.1016/j.jmrt.2024.12.005
[13] Guo Y L, He J Y, Li Z M, et al. Tuning microstructures and improving oxidation resistance of Nb-Si based alloys via electron beam surface melting[J]. Corros. Sci., 2020, 163: 108281
doi: 10.1016/j.corsci.2019.108281
[14] Orrù R, Licheri R, Locci A M, et al. Consolidation/synthesis of materials by electric current activated/assisted sintering[J]. Mater. Sci. Eng., 2009, R63: 127
[15] Liu W, Sha J B. Failure mode transition of Nb phase from cleavage to dimple/tear in Nb-16Si-based alloys prepared via spark plasma sintering[J]. Mater. Des., 2016, 111: 301
doi: 10.1016/j.matdes.2016.08.087
[16] Li Y L, Lin X, Hu Y L, et al. Microstructure and isothermal oxidation behavior of Nb-Ti-Si-based alloy additively manufactured by powder-feeding laser directed energy deposition[J]. Corros Sci., 2020, 173: 108757
doi: 10.1016/j.corsci.2020.108757
[17] Guo Y L, Jia L N, Sun S B, et al. Rapid fabrication of Nb-Si based alloy by selective laser melting: Microstructure, hardness and initial oxidation behavior[J]. Mater. Des., 2016, 109: 37
doi: 10.1016/j.matdes.2016.07.048
[18] Guo Y L, Jia L N, Kong B, et al. Improvement in the oxidation resistance of Nb-Si based alloy by selective laser melting[J]. Corros Sci., 2017, 127: 260
doi: 10.1016/j.corsci.2017.08.022
[19] Guo H S, Guo X P. Microstructure and microhardness of directionally solidified and heat-treated Nb-Ti-Si based ultrahigh temperature alloy[J]. Trans. Nonferrous Met. Soc. China, 2011, 21: 1283
doi: 10.1016/S1003-6326(11)60854-6
[20] Wang J Y, Jia L N, Ma L M, et al. Microstructure optimization of directionally solidified hypereutectic Nb-Si alloy[J]. Trans. Nonferrous Met. Soc. China, 2013, 23: 2874
doi: 10.1016/S1003-6326(13)62809-5
[21] Liu T, Li T J, Cao Y K, et al. Improvement in the oxidation resistance of Nb-16Si-24Ti-2Al-2Cr alloy by hot pressing[J]. Int. J. Refract. Met. Hard Mater., 2024, 120: 106605
doi: 10.1016/j.ijrmhm.2024.106605
[22] Kumar M D B, Madesh R, Adarsh S J, et al. Recent developments and future perspectives in metal additive manufacturing: Techniques, challenges, and functional performance[J]. J Alloys Compd., 2026, 1064: 187718
doi: 10.1016/j.jallcom.2026.187718
[23] Liu W, Ren X Y, Li N, et al. Rapid directionally solidified microstructure characteristic and fracture behaviour of laser melting deposited Nb-Si-Ti alloy[J]. Prog. Nat. Sci. Mater. Int., 2021, 31: 113
doi: 10.1016/j.pnsc.2020.12.003
[24] Li M, Kang Y W, Guo F W. Research progress in manufacturing technology of Nb-Si based ultra-high temperature structural materials[J]. J. Mater. Eng., 2020, 48: 58
doi: 10.11868/j.issn.1001-4381.2020.000284
[25] Sha J B, Hirai H, Tabaru T, et al. High-temperature strength and room-temperature toughness of Nb-W-Si-B alloys prepared by arc-melting[J]. Mater. Sci. Eng., 2004, A364: 151
[26] Sun Z P, Guo X P, He Y S, et al. Investigation on the as-cast microstructure of Nb-Nb silicide based multicomponent alloys[J]. Intermetallics, 2010, 18: 992
doi: 10.1016/j.intermet.2010.01.024
[27] Sala K, Mitra R. Effect of Ti addition and microstructural evolution on toughening and strengthening behavior of as cast or annealed Nb-Si-Mo based hypoeutectic and hypereutectic alloys[J]. Metall. Mater. Trans., 2021, 52A: 3436
[28] Li Y L, Lin X, Hu Y L, et al. Precipitation behavior of Nb-Si-based in-situ composite manufactured by laser directed energy deposition[J]. Scr. Mater., 2022, 207: 114288
doi: 10.1016/j.scriptamat.2021.114288
[29] Li Y L, Lin X, Hu Y L, et al. Zirconium modified Nb-22Ti-16Si alloys fabricated by laser additive manufacturing: Microstructure and fracture toughness[J]. J. Alloys Compd., 2019, 783: 66
doi: 10.1016/j.jallcom.2018.12.280
[30] Sankar M, Phanikumar G, Satya Prasad V V. Effect of Zr addition on the mechanical properties of Nb-Si based alloys[J]. Mater. Sci. Eng., 2019, A754: 224
[31] Zhang S N, Jia L N, Guo Y L, et al. Improvement in the oxidation resistance of Nb-Si-Ti based alloys containing zirconium[J]. Corros. Sci., 2020, 163: 108294
doi: 10.1016/j.corsci.2019.108294
[32] Xu Q, Ma X H, Wang Q, et al. Formation of (Nb, X)ss/β-(Nb, X)5Si3 eutectic and its effect on mechanical properties of Nb-Si-Ti alloys by addition of Mo[J]. Mater. Today Commun., 2025, 42: 111556
[33] Ma R, Guo X P. Influence of molybdenum contents on the microstructure, mechanical properties and oxidation behavior of multi-elemental Nb-Si based ultrahigh temperature alloys[J]. Intermetallics, 2021, 129: 107053
doi: 10.1016/j.intermet.2020.107053
[34] Wang Q, Wang X W, Chen R R, et al. Microstructure evolution and fracture toughness of Nb-Si-Ti based alloy with Cr, Mo and W elements addition[J]. Intermetallics, 2022, 140: 107408
doi: 10.1016/j.intermet.2021.107408
[35] Su L F, Jia L N, Jiang K Y, et al. The oxidation behavior of high Cr and Al containing Nb-Si-Ti-Hf-Al-Cr alloys at 1200 and 1250 oC[J]. Int. J. Refract. Met. Hard Mater., 2017, 69: 131
doi: 10.1016/j.ijrmhm.2017.08.006
[36] Portillio B I, Varma S K. Oxidation behavior of Nb-20Mo-15Si-25Cr and Nb-20Mo-15Si-25Cr-5B alloys[J]. Metall. Mater. Trans., 2012, 43A: 147
[37] Sha J, Yang C, Liu J. Toughening and strengthening behavior of an Nb-8Si-20Ti-6Hf alloy with addition of Cr[J]. Scr. Mater., 2010, 62: 859
doi: 10.1016/j.scriptamat.2010.02.023
[38] Sun Z P, Guo J M, Zhang C, et al. Effect of Ti and Al interaction on microstructures and mechanical properties of the Nb-Ti-Si-Al alloys[J]. Rare Met. Mater. Eng., 2016, 45: 1678
doi: 10.1016/S1875-5372(16)30139-4
[39] Yu J Y, Chen D Z, Xu F D, et al. Simultaneous improving high temperature oxidation resistance and room temperature toughness of Nb-Si based alloy via appropriate Ta content addition strategy[J]. Int. J. Refract. Met. Hard Mater., 2024, 124: 106800
doi: 10.1016/j.ijrmhm.2024.106800
[40] Wang Q, Zhao T Y, Chen R R, et al. Collaborative optimization of microstructure, phase composition and room-temperature fracture toughness of Nb-Si based alloys using Ti, Zr and Hf elements[J]. Trans. Nonferrous Met. Soc. China, 2024, 34: 194
doi: 10.1016/S1003-6326(23)66391-5
[41] Li Z F, Tsakiropoulos P. On the microstructures and hardness of the Nb-24Ti-18Si-5Al-5Cr-5Ge and Nb-24Ti-18Si-5Al-5Cr-5Ge-5Hf (at.%) silicide based alloys[J]. Materials, 2019, 12: 2655
doi: 10.3390/ma12172655
[42] Vazquez A, Varma S K. High-temperature oxidation behavior of Nb-Si-Cr alloys with Hf additions[J]. J. Alloys Compd., 2011, 509: 7027
doi: 10.1016/j.jallcom.2011.02.174
[43] Wang X W, Wang Q, Chen R R, et al. Improved microstructure and mechanical properties of Nb-Si in situ composites: Focus on interstitial element B doping, atomic diffusion and dislocation behaviors[J]. Mater. Sci. Eng., 2025, A946: 149097
[44] Zhang S, Guo X P. Effects of B addition on the microstructure and properties of Nb silicide based ultrahigh temperature alloys[J]. Intermetallics, 2015, 57: 83
doi: 10.1016/j.intermet.2014.10.007
[45] Guo J T, Zhou L Z, Tian Y X, et al. Effect of Hf, Sn, Ta, Zr, Dy and Ho on microstructure and mechanical properties of Nb-Nb5Si3 alloy[J]. Acta Metall. Sin., 2015, 51: 815
郭建亭, 周兰章, 田玉新 等. 合金元素Hf, Sn, Ta, Zr, Dy和Ho对Nb-Nb5Si3合金组织和力学性能的影响[J]. 金属学报, 2015, 51: 815
[46] Tian Y X, Guo J T, Zhou L Z, et al. Effect of Dy addition on microstructure and mechanical properties of Nb-Nb5Si3 eutectic alloy[J]. Acta Metall. Sin., 2008, 44: 589
田玉新, 郭建亭, 周兰章 等. Dy对Nb-Nb5Si3共晶合金显微组织和力学性能的影响[J]. 金属学报, 2008, 44: 589
[47] Chen D Z, Wang Q, Chen R R, et al. An as-cast Nb-Si-based alloy with fine-grains and remarkable fracture toughness by minor Sc addition[J]. J. Alloys Compd., 2022, 895: 162707
doi: 10.1016/j.jallcom.2021.162707
[48] Chen D Z, Wang Y X, Yu J Y, et al. Er-induced microstructural refinement and internal oxidation enhancing fracture toughness in Nb-Si alloys[J]. J. Alloys Compd., 2025, 1045: 184777
doi: 10.1016/j.jallcom.2025.184777
[49] Cui X Y, Chen D Z, Xu F D, et al. Investigating scandium-alloyed Nb-Si systems: Microstructure, oxidation behavior, and fracture toughness[J]. Mater. Charact., 2024, 217: 114409
doi: 10.1016/j.matchar.2024.114409
[50] Guo Y L, Jia L N, Zhang H R, et al. Enhancing the oxidation resistance of Nb-Si based alloys by yttrium addition[J]. Intermetallics, 2018, 101: 165
doi: 10.1016/j.intermet.2018.08.004
[51] Wang X W, Wang Q, Chen R R, et al. Gadolinium doping induced the microstructure evolution and mechanical properties improvement of Nb-Si based in-situ superalloy[J]. J. Alloys Compd., 2024, 1004: 175942
doi: 10.1016/j.jallcom.2024.175942
[52] Wang Y, Jia L N, Sun G X, et al. Synchronous improvement in room-temperature fracture toughness and high-temperature oxidation resistance of Nb-Si based alloys with erbium addition[J]. Int. J. Refract. Met. Hard Mater., 2021, 94: 105359
doi: 10.1016/j.ijrmhm.2020.105359
[53] Wei W, Wang Q, Chen R R, et al. Improved toughness and oxidation resistance of Nb-Si based ultra-high temperature alloys by in-situ generated La2O3 phase[J]. Mater. Charact., 2024, 208: 113686
doi: 10.1016/j.matchar.2024.113686
[54] Yin X Y, Li X X, Sun H, et al. Fine microstructure, better compactness, and significant fracture toughness of multi-component Nb-Si based alloy by an appropriate amount of yttrium addition during the laser melting deposition[J]. Int. J. Refract. Met. Hard Mater., 2026, 137: 107655
doi: 10.1016/j.ijrmhm.2026.107655
[55] Launey M E, Ritchie R O. On the fracture toughness of advanced materials[J]. Adv. Mater., 2009, 21: 2103
doi: 10.1002/adma.v21:20
[56] Chan K S, Davidson D L. Effects of Ti addition on cleavage fracture in Nb-Cr-Ti solid-solution alloys[J]. Metall. Mater. Trans., 1999, 30A: 925
[57] Li Y L, Lin X, Hu Y L, et al. Microstructure and fracture toughness of a Nb-Ti-Si-based in-situ composite fabricated by laser-based directed energy deposition[J]. Composites, 2024, 278B: 111427
[58] Qiao Y Q, Guo X P, Zeng Y X. Study of the effects of Zr addition on the microstructure and properties of Nb-Ti-Si based ultrahigh temperature alloys[J]. Intermetallics, 2017, 88: 19
doi: 10.1016/j.intermet.2017.04.008
[59] Li Z B, Luo L S, Wang B B, et al. The microstructural characteristics and mechanical properties of Nb-16Si-22Ti-2Al-2Cr alloys with Zr addition[J]. Mater. Sci. Eng., 2023, A880: 145305
[60] Li Y L, Lin X, Hu Y L, et al. The effect of Mo on microstructure and mechanical properties of Nb-22Ti-16Si alloy additively manufactured via laser directed energy deposition[J]. J. Alloys Compd., 2021, 858: 158143
doi: 10.1016/j.jallcom.2020.158143
[61] Zhang S, Guo X P. Effects of Cr and Hf additions on the microstructure and properties of Nb silicide based ultrahigh temperature alloys[J]. Mater. Sci. Eng., 2015, A638: 121
[62] Guo Y L, Jia L N, Kong B, et al. Microstructure and fracture toughness of Nb-Si based alloys with Ta and W additions[J]. Intermetallics, 2018, 92: 1
doi: 10.1016/j.intermet.2017.09.005
[63] Tian Y X, Guo J T, Zhou L Z, et al. Microstructure and room temperature fracture toughness of cast Nbss/silicides composites alloyed with Hf[J]. Mater. Lett., 2008, 62: 2657
doi: 10.1016/j.matlet.2008.01.007
[64] Kim J H, Tabaru T, Sakamoto M, et al. Mechanical properties and fracture behavior of an Nbss/Nb5Si3 in-situ composite modified by Mo and Hf alloying[J]. Mater. Sci. Eng., 2004, A372: 137
[65] Sala K, Kashyap S K, Mitra R. Effect of Ti addition on the kinetics and mechanism of non-isothermal and isothermal oxidation of Nb-Si-Mo alloys at 900 oC-1200 oC[J]. Intermetallics, 2021, 138: 107338
doi: 10.1016/j.intermet.2021.107338
[66] Yao D Z, Zhou C G, Yang J Y, et al. Experimental studies and modeling of the oxidation of multiphase niobium-base alloys[J]. Corros. Sci., 2009, 51: 2619
doi: 10.1016/j.corsci.2009.06.053
[67] Li Y L, Lin X, Zhao Z Y, et al. Investigation on the composite effect of Zr and Cr on oxidation behavior and fracture toughness of Nb-Ti-Si-based alloys manufactured by directed energy deposition[J]. Mater. Charact., 2024, 214: 114078
doi: 10.1016/j.matchar.2024.114078
[68] Shen F Q, Yu L H, Fu T, et al. Effect of the Al, Cr and B elements on the mechanical properties and oxidation resistance of Nb-Si based alloys: A review[J]. Appl. Phys., 2021, 127A: 852
[69] Li N, Zhang B D, Huang H, et al. Discussion of effects of Hf on the high temperature oxidation of Nb-based alloy[J]. New Technol. New Process, 2015, (4): 103
李 宁, 张宝东, 黄 辉 等. 铪提高铌硅基合金高温抗氧化性能的机理探讨[J]. 新技术新工艺, 2015, (4): 103
[70] Li Y L, Lin X, Hu Y L, et al. Alloying on the high-temperature oxidation behavior of Nb-Ti-Si-based alloy additively manufactured by laser directed energy deposition[J]. Int. J. Refract. Met. Hard Mater., 2024, 121: 106682
doi: 10.1016/j.ijrmhm.2024.106682
[71] Ma R, Guo X P. Effects of Mo and Zr composite additions on the microstructure, mechanical properties and oxidation resistance of multi-elemental Nb-Si based ultrahigh temperature alloys[J]. J. Alloys Compd., 2021, 870: 159437
doi: 10.1016/j.jallcom.2021.159437
[72] Sun A K, Dong Z Q, Yang S, et al. Effect of Zr and Ti on isothermal oxidation behavior of Nb-Si based alloys[J]. Prog. Nat. Sci. Mater. Int., 2022, 32: 226
doi: 10.1016/j.pnsc.2022.02.004
[73] Li Z B, Luo L S, Wang B B, et al. Cooperative effects of Mo and B additions on the microstructure and mechanical properties of multi-elemental Nb-Si-Ti based alloys[J]. Mater. Charact., 2023, 206: 113421
doi: 10.1016/j.matchar.2023.113421
[74] Ma R, Guo X P. Cooperative effects of Mo, V and Zr additions on the microstructure and properties of multi-elemental Nb-Si based alloys[J]. J. Mater. Sci. Technol., 2023, 132: 27
doi: 10.1016/j.jmst.2022.06.006
[75] Li Y L, Lin X, Hu Y L, et al. Seynergistic effect of Mo and Zr additions on microstructure and mechanical properties of Nb-Ti-Si-based alloys additively manufactured by laser directed energy deposition[J]. J. Mater. Sci. Technol., 2022, 103: 84
doi: 10.1016/j.jmst.2021.06.027
[76] Prasad S, Paul A. Growth mechanism of the Nb(X)Si2 and [Nb(X)]5Si3 phases by reactive diffusion in Nb (X = Ti, Mo, or Zr)-Si systems[J]. Intermetallics, 2012, 22: 210
doi: 10.1016/j.intermet.2011.11.012
[77] Sun G X, Jia L N, Ye C T, et al. Balancing the fracture toughness and tensile strength by multiple additions of Zr and Y in Nb-Si based alloys[J]. Intermetallics, 2021, 133: 107172
doi: 10.1016/j.intermet.2021.107172
[78] Liu G X, Jia L N, Kong B, et al. Artificial neural network application to study quantitative relationship between silicide and fracture toughness of Nb-Si alloys[J]. Mater. Des., 2017, 129: 210
doi: 10.1016/j.matdes.2017.05.027
[79] Ma E, Shin S H, Choi W, et al. Machine learning approach for predicting the fracture toughness of Nb-Si based alloys[J]. Int. J. Refract. Met. Hard Mater., 2023, 117: 106420
doi: 10.1016/j.ijrmhm.2023.106420
[80] Yin X Y, Liang J, Liu C, et al. Accelerating the design of multivariate Nb-Si based alloys with excellent strength and toughness matching through machine learning[J]. Next Mater., 2025, 6: 100294
[81] Liu G X, Jia L N, Kong B, et al. Artificial neural network application to microstructure design of Nb-Si alloy to improve ultimate tensile strength[J]. Mater. Sci. Eng., 2017, A707: 452
[1] CHENG Feng, LU Hao, LIU Xuemei, SONG Xiaoyan. Phase Constitution, Microstructure, and Properties of Ti-Doped SmFe12-Based Nanocrystalline Permanent Magnetic Alloys[J]. 金属学报, 2026, 62(10): 1727-1736.
[2] ZHU Man, ZHANG Cheng, XU Junfeng, JIAN Zengyun, XI Zengzhe. Microstructure, Mechanical Properties, and High-Temperature Oxidation Behaviors of the CrNbTiVAl x Refractory High-Entropy Alloys[J]. 金属学报, 2025, 61(1): 88-98.
[3] TANG Jingtao, YAO Yingjie, ZHANG Youyou, WU Wenhua, LI Yubo, CHEN Hao, YANG Zhigang. Research Progress on the Influence of Metastable Austenite on the Fracture Toughness of High-Strength Steels[J]. 金属学报, 2025, 61(1): 77-87.
[4] CAI Jie, GAO Jie, HUA Yinqun, YE Yunxia, GUAN Qingfeng, ZHANG Xiaofeng. Effect of High-Current Pulsed Electron Beam Irradiation on Microstructure and Properties of MCrAlY Coating Prepared by Low-Pressure Plasma Spraying[J]. 金属学报, 2024, 60(4): 495-508.
[5] GU Ruicheng, ZHANG Jian, ZHANG Mingyang, LIU Yanyan, WANG Shaogang, JIAO Da, LIU Zengqian, ZHANG Zhefeng. Fabrication of Mg-Based Composites Reinforced by SiC Whisker Scaffolds with Three-Dimensional Interpenetrating-Phase Architecture and Their Mechanical Properties[J]. 金属学报, 2022, 58(7): 857-867.
[6] HU Chen, PAN Shuai, HUANG Mingxin. Strong and Tough Heterogeneous TWIP Steel Fabricated by Warm Rolling[J]. 金属学报, 2022, 58(11): 1519-1526.
[7] CHEN Ruirun, CHEN Dezhi, WANG Qi, WANG Shu, ZHOU Zhecheng, DING Hongsheng, FU Hengzhi. Research Progress on Nb-Si Base Ultrahigh Temperature Alloys and Directional Solidification Technology[J]. 金属学报, 2021, 57(9): 1141-1154.
[8] Jing BAI, Shaofeng SHI, Jinlong WANG, Shuai WANG, Xiang ZHAO. First-Principles Calculations of Phase Stability and Magnetic Properties of Ni-Mn-Ga-Ti FerromagneticShape Memory Alloys[J]. 金属学报, 2019, 55(3): 369-375.
[9] Yizhe LI, Baoming GONG, Xiuguo LIU, Dongpo WANG, Caiyan DENG. Out-of-Plane Constraint Effect on the Fracture Toughness of Single Edge Notch Tension Specimens[J]. 金属学报, 2018, 54(12): 1785-1791.
[10] Hongxi LIU,Zhengxue LI,Xiaowei ZHANG,Jun TAN,Yehua JIANG. Effect of Heat Treatment on High-Temperature Oxidation Resistance of High Niobium Ti-Al Intermetallic Coating Fabricated by Laser In Situ Synthesis on Titanium Alloy[J]. 金属学报, 2017, 53(2): 201-210.
[11] Jing BAI,Ze LI,Zhen WAN,Xiang ZHAO. A First-Principles Study on Crystal Structure, Phase Stability and Magnetic Properties of Ni-Mn-Ga-Cu Ferromagnetic Shape Memory Alloys[J]. 金属学报, 2017, 53(1): 83-89.
[12] Xiangli FENG,Lei WANG,Yang LIU. STUDY ON MICROSTRUCTURE AND DYNAMIC FRACTURE BEHAVIOR OF Q460 STEEL WELDING JOINTS[J]. 金属学报, 2016, 52(7): 787-796.
[13] Yong SHEN,Jian XU. PREPARATION AND MECHANICAL PROPERTIES OF Zr46.9Cu45.5Al5.6Y2.0 IN SITU BMG COMPOSITES WITH B2-CuZr PHASE[J]. 金属学报, 2015, 51(11): 1407-1415.
[14] ZHU Zhendong, XU Jian. Cu56Hf27Ti17 BULK METALLIC GLASS WITH HIGH FRACTURE TOUGHNESS[J]. 金属学报, 2013, 49(8): 969-975.
[15] BI Zongyue, YANG Jun, NIU Jing, ZHANG Jianxun. FRACTURE TOUGHNESS OF WELDED JOINTS OF X100 HIGH-STRENGTH PIPELINE STEEL[J]. 金属学报, 2013, 49(5): 576-582.
No Suggested Reading articles found!