| Anisotropy in Microstructures and Mechanical Properties of 2Cr13 Alloy Produced by Wire Arc Additive Manufacturing |
GE Jinguo1,2, LU Zhao3, HE Siliang1, SUN Yan4, YIN Shuo2,5( ) |
1.School of Mechanical and Electrical Engineering, Guilin University of Electronic Technology, Guilin 541010, China 2.Trinity College Dublin, The University of Dublin, Dublin D02PN40, Ireland 3.School of Materials Science and Engineering, Guilin University of Electronic Technology, Guilin 541010, China 4.Design & Research Institute, Dalian Shipbuilding Industry Co., Ltd., Dalian 116005, China 5.School of Mechanical Engineering, Yangzhou University, Yangzhou 225127, China |
|
Cite this article:
GE Jinguo, LU Zhao, HE Siliang, SUN Yan, YIN Shuo. Anisotropy in Microstructures and Mechanical Properties of 2Cr13 Alloy Produced by Wire Arc Additive Manufacturing. Acta Metall Sin, 2023, 59(1): 157-168.
|
|
|
Abstract 2Cr13 martensite stainless steel has been widely used for the manufacturing of surgical tools and turbine blades. Contrary to the conventional fabrication technologies, there are several remarkable advantages in the fabrication of 2Cr13 parts by adopting wire arc additive manufacturing (WAAM) technologies, such as excellent metallurgical bonding, high production efficiency, near-net-shape production, and limited environmental contamination. In this work, the effect of interlayer dwelling temperature (110-550oC) on microstructural and mechanical properties has been revealed, providing a new approach for the active control of the performances of 2Cr13 buildups produced by wire-arc additive manufacturing. The part with a dwelling temperature of 550oC was featured by elongated acicular martensite features, with a slightly enhanced fiber-like texture, along with minor fine irregular-reverse austenite structures, dispersed among martensite gaps. This special martensitic distribution was mainly caused by the grain-broken effect under the intensive thermal shock from liquid melting pool. Consequently, the enhanced tensile strength and microhardness were obtained due to grain refinement, although exhibiting an obvious anisotropy in tensile properties. The parts with dwelling temperatures of 110-180oC were characterized by relatively coarsened martensite laths, with a random texture type, within block-shaped ferrite matrix. The average martensite size was gradually refined due to the increased cooling rate by lowering interlayer temperature. The isotropic mechanical properties of all three parts (110-180oC) were similar because of the similar martensite laths.
|
|
Received: 25 August 2022
|
|
|
| Fund: China Postdoctoral Science Foundation(2021M693230);Natural Science Foundation of Guangxi Province(2021JJB160022) |
About author: YIN Shuo, professor, Tel: (00353)18968583, E-mail: yins@tcd.ie
|
| 1 |
Ge J G, Lin J, Fu H G, et al. A spatial periodicity of microstructural evolution and anti-indentation properties of wire-arc additive manufacturing 2Cr13 thin-wall part [J]. Mater. Des., 2018, 160: 218
doi: 10.1016/j.matdes.2018.09.021
|
| 2 |
Zhao M P, You P P, Liu M H. Pockmarks on ground surface of nitrided 2Cr13 steel [J]. Heat Treat. Met., 2020, 45(5): 176
|
|
赵明鹏, 游平平, 刘明虎. 2Cr13钢渗氮后磨削面的“麻点”问题 [J]. 金属热处理, 2020, 45(5): 176
|
| 3 |
Liu X, Yang J C, Yang L, et al. Effect of Ce on inclusions and impact property of 2Cr13 stainless steel [J]. J. Iron Steel Res. Int., 2010, 17: 59
|
| 4 |
Shao Y K. Effects of laser shock peening on cavitation erosion and cavitation-silt erosion resistance of 2Cr13 stainless steel [D]. Zhenjiang: Jiangsu University, 2020
|
|
邵亦锴. 激光冲击强化2Cr13不锈钢抗气蚀和空化—颗粒侵蚀行为研究 [D]. 镇江: 江苏大学, 2020
|
| 5 |
Ge J G, Lin J, Long Y H, et al. Microstructural evolution and mechanical characterization of wire arc additively manufactured 2Cr13 thin-wall part [J]. J. Mater. Res. Technol., 2021, 13: 1767
doi: 10.1016/j.jmrt.2021.05.110
|
| 6 |
Javurek M, Brummayer M, Wincor R. Turbulent flow measurements in continuous steel casting mold water model [J]. Mater. Today, 2022, 62: 2581
|
| 7 |
Wang H W, Zhang X Y, Tian Z P, et al. Effects of heat treatment process on microstructure, strength and toughness of 2Cr13 stainless steel [J]. Hot Work. Technol., 2020, 49(20): 124
|
|
王浩伟, 张戌有, 田志平 等. 热处理工艺对2Cr13不锈钢组织和强韧性的影响 [J]. 热加工工艺, 2020, 49(20): 124
|
| 8 |
Cao J C. Research on CAD&FEM of turbine blade die forging [D]. Qinhuangdao: Yanshan University, 2006
|
|
曹竟成. 汽轮机叶片模锻工艺CAD与模锻过程有限元分析 [D]. 秦皇岛: 燕山大学, 2006
|
| 9 |
Kumar N, Bhavsar H, Mahesh P V S, et al. Wire arc additive manufacturing—A revolutionary method in additive manufacturing [J]. Mater. Chem. Phys., 2022, 285: 126144
doi: 10.1016/j.matchemphys.2022.126144
|
| 10 |
Ren X L, Jiang X Q, Yuan T, et al. Microstructure and properties research of Al-Zn-Mg-Cu alloy with high strength and high elongation fabricated by wire arc additive manufacturing [J]. J. Mater. Process. Technol., 2022, 307: 117665
doi: 10.1016/j.jmatprotec.2022.117665
|
| 11 |
Tomar B, Shiva S, Nath T. A review on wire arc additive manufacturing: Processing parameters, defects, quality improvement and recent advances [J]. Mater. Today, 2022, 31: 103739
|
| 12 |
Xia C Y, Pan Z X, Polden J, et al. A review on wire arc additive manufacturing: Monitoring, control and a framework of automated system [J]. J. Manuf. Syst., 2020, 57: 31
doi: 10.1016/j.jmsy.2020.08.008
|
| 13 |
Sun J X, Yang K, Wang Q Y, et al. Microstructure and mechanical properties of 5356 aluminum alloy fabricated by TIG arc additive manufacturing [J]. Acta Metall. Sin., 2021, 57: 665
doi: 10.11900/0412.1961.2020.00266
|
|
孙佳孝, 杨 可, 王秋雨 等. 5356铝合金TIG电弧增材制造组织与力学性能 [J]. 金属学报, 2021, 57: 665
doi: 10.11900/0412.1961.2020.00266
|
| 14 |
Du Z J, Li W Y, Liu J R, et al. Study on the uniformity of structure and mechanical properties of TC4-DT alloy deposited by CMT process [J]. Acta Metall. Sin., 2020, 56: 1667
|
|
杜子杰, 李文渊, 刘建荣 等. CMT增材制造TC4-DT合金组织均匀性与力学性能一致性研究 [J]. 金属学报, 2020, 56: 1667
|
| 15 |
Priarone P C, Campatelli G, Catalano A R, et al. Life-cycle energy and carbon saving potential of wire arc additive manufacturing for the repair of mold inserts [J]. CIRP J. Manuf. Sci. Technol., 2021, 35: 943
doi: 10.1016/j.cirpj.2021.10.007
|
| 16 |
Hassen A A, Noakes M, Nandwana P, et al. Scaling Up metal additive manufacturing process to fabricate molds for composite manufacturing [J]. Addit. Manuf., 2020, 32: 101093
|
| 17 |
Jing C C, Chen Z, Liu B, et al. Improving mechanical strength and isotropy for wire-arc additive manufactured 304L stainless steels via controlling arc heat input [J]. Mater. Sci. Eng., 2022, A845: 143223
|
| 18 |
Rodideal N, Machado C M, Infante V, et al. Mechanical characterization and fatigue assessment of wire and arc additively manufactured HSLA steel parts [J]. Int. J. Fatigue, 2022, 164: 107146
doi: 10.1016/j.ijfatigue.2022.107146
|
| 19 |
Ge J G, Xu R W, Wang C L, et al. Deposition structure dependence of microstructural evolution and mechanical anisotropy of H13 buildups using cold metal transfer technology [J]. J. Alloys Compd., 2022, 904: 163283
doi: 10.1016/j.jallcom.2021.163283
|
| 20 |
Klein T, Wojcik T, Arnoldt A. A hypoeutectic Al-Ni-Mg in situ composite processed by wire-arc additive manufacturing: Phase evolution and mechanical behavior [J]. Mater. Des., 2022, 222: 111066
doi: 10.1016/j.matdes.2022.111066
|
| 21 |
Nagasai B P, Malarvizhi S, Balasubramanian V. Mechanical properties and microstructural characteristics of wire arc additive manufactured 308 L stainless steel cylindrical components made by gas metal arc and cold metal transfer arc welding processes [J]. J. Mater. Process. Technol., 2022, 307: 117655
doi: 10.1016/j.jmatprotec.2022.117655
|
| 22 |
Krakhmalev P, Yadroitsava I, Fredriksson G, et al. In situ heat treatment in selective laser melted martensitic AISI 420 stainless steels [J]. Mater. Des., 2015, 87: 380
doi: 10.1016/j.matdes.2015.08.045
|
| 23 |
Zhu X C, Wen S F, Wei Q S. Microstructure and mechanical properties of mould steels AISI 420 and S136 by selective laser melting manufacturing [J]. Spec. Cast. Nonferrous Alloys, 2019, 39: 506
|
|
朱学超, 文世峰, 魏青松. AISI420与S136模具钢SLM成形组织及性能 [J]. 特种铸造及有色合金, 2019, 39: 506
|
| 24 |
Alvarez L F, Garcia C, Lopez V. Continuous cooling transformations in martensitic stainless steels [J]. ISIJ Int., 1994, 34: 516
doi: 10.2355/isijinternational.34.516
|
| 25 |
Fang R R, Deng N N, Zhang H B, et al. Effect of selective laser melting process parameters on the microstructure and properties of a precipitation hardening stainless steel [J]. Mater. Des., 2021, 212: 110265
doi: 10.1016/j.matdes.2021.110265
|
| 26 |
Deng F B, Yang G, Zhou S Y, et al. Effect of heat treatment on microstructural heterogeneity and mechanical properties of maraging steel fabricated by wire arc additive manufacturing using 4% nitrogen shielding gas [J]. Mater. Charact., 2022, 191: 112160
doi: 10.1016/j.matchar.2022.112160
|
| 27 |
Fang Y J, Kim M K, Zhang Y L, et al. Particulate-reinforced iron-based metal matrix composites fabricated by selective laser melting: A systematic review [J]. J. Manuf. Process., 2022, 74: 592
doi: 10.1016/j.jmapro.2021.12.018
|
| No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|