Effect ofIn Situ 2%TiB2 Particles on Microstructure and Mechanical Properties of 2024Al Additive Manufacturing Alloy |
SUN Tengteng1, WANG Hongze1,2( ), WU Yi1,2( ), WANG Mingliang1,2, WANG Haowei1,2 |
1.State Key Laboratory of Metal Matrix Composites, School of Materials Science and Engineering, Shanghai Jiao Tong University, Shanghai 200240, China 2.Institute of Alumics Materials, Shanghai Jiao Tong University (Anhui), Huaibei 235000, China |
|
Cite this article:
SUN Tengteng, WANG Hongze, WU Yi, WANG Mingliang, WANG Haowei. Effect ofIn Situ 2%TiB2 Particles on Microstructure and Mechanical Properties of 2024Al Additive Manufacturing Alloy. Acta Metall Sin, 2023, 59(1): 169-179.
|
Abstract Laser powder bed fusion (L-PBF) is an innovative additive manufacturing method with great potential for fabricating complex geometrical components with integrated functionalities. In the aerospace industry, the Al-Cu-Mg (2024Al) alloy is widely used because of its excellent mechanical properties and low density; however, its disadvantages include low printability and high crack susceptibility. This work investigates the effects of in situ TiB2 particles on the microstructure and tensile properties of the solution-treated (510oC treat 1 h and then cooling by water) and T6-treated (i.e., solution and aging treatments) L-PBF fabricated 2024Al alloy at room temperature. Equiaxed grains with an average size of approximately 5.8 μm dominate in the printed 2024Al-2%TiB2 alloy because of the high cooling rate during the L-PBF process and the heterogeneous nucleation effect of the TiB2 particles. After the T6 heat treatment, many uniformly distributed, fine, and long precipitation strips formed in both the 2024Al and 2024Al-2%TiB2 alloys. The 2024Al-2%TiB2 alloy has ultimate tensile and yield strengths of (458.2 ± 6.5) and (398.4 ± 2.7) MPa, respectively; further, it has a maximum elongation of (3.4 ± 0.4)%. These parameters indicate a substantial improvement in the strength and elongation of the 2024Al-2%TiB2 alloy compared to those of the 2024Al alloy. Furthermore, the mechanical properties of the T6-treated 2024Al-2%TiB2 alloy are comparable to those of the wrought T6-treated 2024Al-T6 alloy. The main strengthening mechanisms of the 2024Al-2%TiB2 alloy include solid solution strengthening, dislocation strengthening, grain boundary strengthening, precipitation strengthening, Orowan strengthening, and load-bearing strengthening induced by TiB2 particles. In conclusion, 2024Al-2%TiB2 alloy manufactured using the L-PBF method provides excellent printability and room-temperature tensile properties.
|
Received: 25 August 2022
|
|
Fund: National Natural Science Foundation of China(52075327);National Natural Science Foundation of China(52004160);Shanghai Sailing Program(20YF1419200);Natural Science Foundation of Shanghai(20ZR1427500);Major Science and Technology Project of Huaibei(Z2020001);Shanghai Synchrotron Radiation Facility (SSRF) Beamline BL13W1(2020-SSRF-PT-012107) |
1 |
Wang A, Wang H Z, Wu Y, et al. 3D printing of aluminum alloys using laser powder deposition: A review [J]. Int. J. Adv. Manuf. Technol., 2021, 116: 1
doi: 10.1007/s00170-021-07440-5
|
2 |
Shi Y S, Zhang J L, Wen S F, et al. Additive manufacturing and foundry innovation [J]. China Foundry, 2021, 18: 286
doi: 10.1007/s41230-021-1008-8
|
3 |
Molitch-Hou M. Overview of additive manufacturing process [A]. Additive Manufacturing [M]. Oxford: Elsevier, 2018: 1
|
4 |
Sun X F, Song W, Liang J J, et al. Research and development in materials and processes of superalloy fabricated by laser additive manufacturing [J]. Acta Metall. Sin., 2021, 57: 1471
doi: 10.11900/0412.1961.2021.00371
|
|
孙晓峰, 宋 巍, 梁静静 等. 激光增材制造高温合金材料与工艺研究进展 [J]. 金属学报, 2021, 57: 1471
doi: 10.11900/0412.1961.2021.00371
|
5 |
DebRoy T, Wei H L, Zuback J S, et al. Additive manufacturing of metallic components—Process, structure and properties [J]. Prog. Mater. Sci., 2018, 92: 112
doi: 10.1016/j.pmatsci.2017.10.001
|
6 |
Geng Y X, Tang H, Xu J H, et al. Formability and mechanical properties of high-strength Al-(Mn, Mg)-(Sc, Zr) alloy produced by selective laser melting [J]. Acta Metall. Sin., 2022, 58: 1044
|
|
耿遥祥, 唐 浩, 许俊华 等. 选区激光熔化高强Al-(Mn, Mg)-(Sc, Zr)合金成形性及力学性能 [J]. 金属学报, 2022, 58: 1044
doi: 10.11900/0412.1961.2021.00023
|
7 |
Wen X L, Wang Q Z, Mu Q, et al. Laser solid forming additive manufacturing TiB2 reinforced 2024Al composite: Microstructure and mechanical properties [J]. Mater. Sci. Eng., 2019, A745: 319
|
8 |
Yang H H, W J Y, Wei Q L, et al. Stable cladding of high reflectivity pure copper on the aluminum alloy substrate by an infrared-blue hybrid laser [J]. Addit. Manufact. Lett., 2022, 3: 100040
|
9 |
Lopez-Botello O, Martinez-Hernandez U, Ramírez J, et al. Two-dimensional simulation of grain structure growth within selective laser melted AA-2024 [J]. Mater. Des., 2017, 113: 369
doi: 10.1016/j.matdes.2016.10.031
|
10 |
Zhang C, Zhang H, Wang L, et al. Microcracking and mechanical properties in laser-arc hybrid welding of wrought Al-6Cu aluminum alloy [J]. Metall. Mater. Trans., 2018, 49A: 4441
|
11 |
Martin J H, Yahata B D, Hundley J M, et al. 3D printing of high-strength aluminium alloys [J]. Nature, 2017, 549: 365
doi: 10.1038/nature23894
|
12 |
Tan Q Y, Zhang J Q, Sun Q, et al. Inoculation treatment of an additively manufactured 2024 aluminium alloy with titanium nanoparticles [J]. Acta Mater., 2020, 196: 1
doi: 10.1016/j.actamat.2020.06.026
|
13 |
Li X P, Kong C, Becker T, et al. Investigation of interfacial reaction products and stress distribution in selective laser melted Al12Si/SiC composite using confocal Raman microscopy [J]. Adv. Eng. Mater., 2016, 18: 1337
doi: 10.1002/adem.201600150
|
14 |
Sun T T, Xiao Y K, Luo G D, et al. Roadmap to improve the printability of a non-castable alloy for additive manufacturing [J]. Metall. Mater. Trans., 2022, 53A: 2780
|
15 |
Sun T T, Wang H Z, Gao Z Y, et al. The role of in-situ nano-TiB2 particles in improving the printability of noncastable 2024Al alloy [J]. Mater. Res. Lett., 2022, 10: 656
doi: 10.1080/21663831.2022.2080514
|
16 |
Fiocchi J, Tuissi A, Biffi C A. Heat treatment of aluminium alloys produced by laser powder bed fusion: A review [J]. Mater. Des., 2021, 204: 109651
doi: 10.1016/j.matdes.2021.109651
|
17 |
Xiao Y K, Bian Z Y, Wu Y, et al. Simultaneously minimizing residual stress and enhancing strength of selective laser melted nano-TiB2 decorated Al alloy via post-uphill quenching and ageing [J]. Mater. Charact., 2021, 178: 111242
doi: 10.1016/j.matchar.2021.111242
|
18 |
Li W, Li S, Liu J, et al. Effect of heat treatment on AlSi10Mg alloy fabricated by selective laser melting: Microstructure evolution, mechanical properties and fracture mechanism [J]. Mater. Sci. Eng., 2016, A663: 116
|
19 |
Malikov A, Orishich A, Vitoshkin I, et al. Effect of post-heat treatment on microstructure and mechanical properties of laser welded Al-Cu-Mg alloy [J]. J. Manuf. Process., 2021, 64: 620
doi: 10.1016/j.jmapro.2021.02.008
|
20 |
Tao Y, Zhang Z, Xue P, et al. Effect of post weld artificial aging and water cooling on microstructure and mechanical properties of friction stir welded 2198-T8 Al-Li joints [J]. J. Mater. Sci. Technol., 2022, 123: 92
doi: 10.1016/j.jmst.2022.01.020
|
21 |
Sun T T, Chen J, Wu Y, et al. Achieving excellent strength of the LPBF additively manufactured Al-Cu-Mg composite via in-situ mixing TiB2 and solution treatment [J]. Mater. Sci. Eng., 2022, A850: 143531
|
22 |
Thapliyal S, Shukla S, Zhou L, et al. Design of heterogeneous structured Al alloys with wide processing window for laser-powder bed fusion additive manufacturing [J]. Addit. Manuf., 2021, 42: 102002
|
23 |
Hooper P A. Melt pool temperature and cooling rates in laser powder bed fusion [J]. Addit. Manuf., 2018, 22: 548
|
24 |
Zhang H Y, Li J M, Sun J L, et al. Theoretical analysis for condensation heat transfer of binary refrigerant mixtures with annular flow in horizontal mini-tubes [J]. Heat Mass Transfer, 2016, 52: 47
doi: 10.1007/s00231-015-1596-1
|
25 |
Olakanmi E O, Cochrane R F, Dalgarno K W. A review on selective laser sintering/melting (SLS/SLM) of aluminium alloy powders: Processing, microstructure, and properties [J]. Prog. Mater. Sci., 2015, 74: 401
doi: 10.1016/j.pmatsci.2015.03.002
|
26 |
Wang W Q, Wang S Y, Chen F, et al. Microstructure and mechanical properties of TiN/Inconel 718 composites fabricated by selective laser melting [J]. Acta Metall. Sin., 2021, 57: 1017
doi: 10.11900/0412.1961.2020.00485
|
|
王文权, 王苏煜, 陈 飞 等. 选区激光熔化成形TiN/Inconel 718复合材料的组织和力学性能 [J]. 金属学报, 2021, 57: 1017
doi: 10.11900/0412.1961.2020.00485
|
27 |
Li X P, Ji G, Chen Z, et al. Selective laser melting of nano-TiB2 decorated AlSi10Mg alloy with high fracture strength and ductility [J]. Acta Mater., 2017, 129: 183
doi: 10.1016/j.actamat.2017.02.062
|
28 |
Liu Y X, Wang R C, Peng C Q, et al. Microstructural evolution and mechanical performance of in-situ TiB2/AlSi10Mg composite manufactured by selective laser melting [J]. J. Alloys Compd., 2021, 853: 157287
doi: 10.1016/j.jallcom.2020.157287
|
29 |
Wang P, Gammer C, Brenne F, et al. A heat treatable TiB2/Al-3.5Cu-1.5Mg-1Si composite fabricated by selective laser melting: Microstructure, heat treatment and mechanical properties [J]. Composites, 2018, 147B: 162
|
30 |
McPeak K M, Jayanti S V, Kress S J P, et al. Plasmonic films can easily be better: Rules and recipes [J]. ACS Photonics, 2015, 2: 326
pmid: 25950012
|
31 |
Cui H C, Lu F G, Peng K, et al. Comparison of laser welding between TiB2/ZL101 composites and ZL101 [J]. Weld. Joining, 2010, (3): 48
|
|
崔海超, 芦凤桂, 彭 坤 等. TiB2/ZL101复合材料与ZL101合金激光焊对比研究 [J]. 焊接, 2010, (3): 48
|
32 |
Ma Y, Addad A, Ji G, et al. Atomic-scale investigation of the interface precipitation in a TiB2 nanoparticles reinforced Al-Zn-Mg-Cu matrix composite [J]. Acta Mater., 2020, 185: 287
doi: 10.1016/j.actamat.2019.11.068
|
33 |
Mohamed I F, Masuda T, Lee S, et al. Strengthening of A2024 alloy by high-pressure torsion and subsequent aging [J]. Mater. Sci. Eng., 2017, A704: 112
|
34 |
Jia Q B, Rometsch P, Kürnsteiner P, et al. Selective laser melting of a high strength Al-Mn-Sc alloy: Alloy design and strengthening mechanisms [J]. Acta Mater., 2019, 171: 108
doi: 10.1016/j.actamat.2019.04.014
|
35 |
Ma K K, Wen H M, Hu T, et al. Mechanical behavior and strengthening mechanisms in ultrafine grain precipitation-strengthened aluminum alloy [J]. Acta Mater., 2014, 62: 141
doi: 10.1016/j.actamat.2013.09.042
|
36 |
Zhang J L, Song B, Yang L, et al. Microstructure evolution and mechanical properties of TiB/Ti6Al4V gradient-material lattice structure fabricated by laser powder bed fusion [J]. Composites, 2020, 202B: 108417
|
37 |
Hadadzadeh A, Baxter C, Amirkhiz B S, et al. Strengthening mechanisms in direct metal laser sintered AlSi10Mg: Comparison between virgin and recycled powders [J]. Addit. Manuf., 2018, 23: 108
|
38 |
Considére A. Mémoire sur l'emploi du fer et de l'acier dans les constructions [J]. Ann. Ponts Chaussées, 1885, 9: 574
|
39 |
Xiao Y K, Chen H, Bian Z Y, et al. Enhancing strength and ductility of AlSi10Mg fabricated by selective laser melting by TiB2 nanoparticles [J]. J. Mater. Sci. Technol., 2022, 109: 254
doi: 10.1016/j.jmst.2021.08.030
|
40 |
Chen B, Moon S K, Yao X, et al. Strength and strain hardening of a selective laser melted AlSi10Mg alloy [J]. Scr. Mater., 2017, 141: 45
doi: 10.1016/j.scriptamat.2017.07.025
|
No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
|
Shared |
|
|
|
|
|
Discussed |
|
|
|
|