| Effects of Particle Size on Processability of AlSi10Mg Alloy Manufactured by Selective Laser Melting |
WANG Meng, YANG Yongqiang, Trofimov Vyacheslav, SONG Changhui, ZHOU Hanxiang, WANG Di( ) |
| School of Mechanical and Automotive Engineering, South China University of Technology, Guangzhou 510640, China |
|
Cite this article:
WANG Meng, YANG Yongqiang, Trofimov Vyacheslav, SONG Changhui, ZHOU Hanxiang, WANG Di. Effects of Particle Size on Processability of AlSi10Mg Alloy Manufactured by Selective Laser Melting. Acta Metall Sin, 2023, 59(1): 147-156.
|
|
|
Abstract Selective laser melting (SLM) is a widely used high-precision additive manufacturing technology that can achieve arbitrarily complex structures. The powder size used by SLM is generally 15-53 μm, which is suitable for manufacturing parts with a forming accuracy within tens of microns. However, the reason why smaller or larger particle size powders are not suitable is not yet clear. The effect of particle size on SLM processability was studied by simulation and experimentation. Three powder particle sizes of AlSi10Mg were used to study the behavior of powder spreading and melting/solidification during SLM by discrete element and computational fluid dynamics methods, respectively. The macroscopic forming quality of the formed samples was tested. The results show that the powders with a particle size below 20 μm agglomerate vigorously to form many cavities, and the powders with a particle size above 53 μm tend to form few large cavities. The relative density of the powder bed with the medium particle size is 7.69% and 3.17% higher than those of the fine and large particle sizes, respectively. The melt channels of the fine and coarse particle sizes are irregular due to the uneven quality of powder laying when the powder bed is melted. However, after multilayer melting, defects in the melt channel of the fine particle size are partially alleviated. With the increase in particle size, the melt channel surface flatness decreases, the fine particle size powder samples have more porosity, and the coarse particle size powder has a few unfused defects. The processability of the medium particle size for SLM is the best among them. The relative density of the sample with the medium particle size reach 99.8%, which is 1.4% and 0.4% higher than those of samples with fine and coarse particle sizes, respectively.
|
|
Received: 06 September 2022
|
|
|
| Fund: National Natural Science Foundation of China(U2001218);Guangdong Basic and Applied Basic Research Foundation(2022B1515020064) |
About author: WANG Di, professor, Tel: 15913117137, E-mail: mewdlaser@scut.edu.cn
|
| 1 |
Geng Y X, Fan S M, Jian J L, et al. Mechanical properties of AlSiMg alloy specifically designed for selective laser melting [J]. Acta Metall. Sin., 2020, 56: 821
doi: 10.11900/0412.1961.2019.00306
|
|
耿遥祥, 樊世敏, 简江林 等. 选区激光熔化专用AlSiMg合金成分设计及力学性能 [J]. 金属学报, 2020, 56: 821
doi: 10.11900/0412.1961.2019.00306
|
| 2 |
Si L, Zhang T F, Zhou M Y, et al. Numerical simulation of the flow behavior and powder spreading mechanism in powder bed-based additive manufacturing [J]. Powder Technol., 2021, 394: 1004
doi: 10.1016/j.powtec.2021.09.010
|
| 3 |
Chen H, Chen Y X, Liu Y, et al. Packing quality of powder layer during counter-rolling-type powder spreading process in additive manufacturing [J]. Int. J. Mach. Tools Manuf., 2020, 153: 103553
doi: 10.1016/j.ijmachtools.2020.103553
|
| 4 |
Tsuji Y, Tanaka T, Ishida T. Lagrangian numerical simulation of plug flow of cohesionless particles in a horizontal pipe [J]. Powder Technol., 1992, 71: 239
doi: 10.1016/0032-5910(92)88030-L
|
| 5 |
Ma Y F, Evans T M, Philips N, et al. Numerical simulation of the effect of fine fraction on the flowability of powders in additive manufacturing [J]. Powder Technol., 2020, 360: 608
doi: 10.1016/j.powtec.2019.10.041
|
| 6 |
Han Q Q, Gu H, Setchi R. Discrete element simulation of powder layer thickness in laser additive manufacturing [J]. Powder Technol., 2019, 352: 91
doi: 10.1016/j.powtec.2019.04.057
|
| 7 |
Chen H, Wei Q S, Zhang Y J, et al. Powder-spreading mechanisms in powder-bed-based additive manufacturing: Experiments and computational modeling [J]. Acta Mater., 2019, 179: 158
doi: 10.1016/j.actamat.2019.08.030
|
| 8 |
Yao D Z, An X Z, Fu H T, et al. Dynamic investigation on the powder spreading during selective laser melting additive manufacturing [J]. Addit. Manuf., 2021, 37: 101707
|
| 9 |
He Y, Hassanpour A, Bayly A E. Combined effect of particle size and surface cohesiveness on powder spreadability for additive manufacturing [J]. Powder Technol., 2021, 392: 191
doi: 10.1016/j.powtec.2021.06.046
|
| 0 |
Wang L, Li E L, Shen H, et al. Adhesion effects on spreading of metal powders in selective laser melting [J]. Powder Technol., 2020, 363: 602
doi: 10.1016/j.powtec.2019.12.048
|
| 11 |
Muñiz-Lerma J A, Nommeots-Nomm A, Waters K E, et al. A comprehensive approach to powder feedstock characterization for powder bed fusion additive manufacturing: A case study on AlSi7Mg [J]. Materials, 2018, 11: 2386
doi: 10.3390/ma11122386
|
| 12 |
Balbaa M A, Ghasemi A, Fereiduni E, et al. Role of powder particle size on laser powder bed fusion processability of AlSi10Mg alloy [J]. Addit. Manuf., 2021, 37: 101630
|
| 13 |
Gu D D, Xia M J, Dai D H. On the role of powder flow behavior in fluid thermodynamics and laser processability of Ni-based composites by selective laser melting [J]. Int. J. Mach. Tools Manuf., 2019, 137: 67
doi: 10.1016/j.ijmachtools.2018.10.006
|
| 14 |
Gilabert F A, Roux J N, Castellanos A. Computer simulation of model cohesive powders: Influence of assembling procedure and contact laws on low consolidation states [J]. Phys. Rev., 2007, 75E: 011303
|
| 15 |
Lee K F, Dosta M, McGuire A D, et al. Development of a multi-compartment population balance model for high-shear wet granulation with discrete element method [J]. Comput. Chem. Eng., 2017, 99: 171
doi: 10.1016/j.compchemeng.2017.01.022
|
| 16 |
Wang Y, Wang J J, Zhang H, et al. Effects of heat treatments on microstructure and mechanical properties of AlSi10Mg alloy produced by selective laser melting [J]. Acta Metall. Sin., 2021, 57: 613
doi: 10.11900/0412.1961.2020.00253
|
|
王 悦, 王继杰, 张 昊 等. 热处理对激光选区熔化AlSi10Mg合金显微组织及力学性能的影响 [J]. 金属学报, 2021, 57: 613
|
| 17 |
Bidare P, Maier R R J, Beck R J, et al. An open-architecture metal powder bed fusion system for in-situ process measurements [J]. Addit. Manuf., 2017, 16: 177
|
| 18 |
Tang C, Tan J L, Wong C H. A numerical investigation on the physical mechanisms of single track defects in selective laser melting [J]. Int. J. Heat Mass Transfer, 2018, 126: 957
doi: 10.1016/j.ijheatmasstransfer.2018.06.073
|
| 19 |
Zhang Y, Zhang J. Modeling of solidification microstructure evolution in laser powder bed fusion fabricated 316L stainless steel using combined computational fluid dynamics and cellular automata [J]. Addit. Manuf., 2019, 28: 750
doi: 10.1016/j.addma.2019.06.024
|
| 20 |
Chiumenti M, Lin X, Cervera M, et al. Numerical simulation and experimental calibration of additive manufacturing by blown powder technology. Part I: thermal analysis [J]. Rapid Prototyping J., 2017, 23: 448
doi: 10.1108/RPJ-10-2015-0136
|
| 21 |
Zheng M, Wei L, Chen J, et al. A novel method for the molten pool and porosity formation modelling in selective laser melting [J]. Int. J. Heat Mass Transfer, 2019, 140: 1091
doi: 10.1016/j.ijheatmasstransfer.2019.06.038
|
| 22 |
Zheng M, Wei L, Chen J, et al. On the role of energy input in the surface morphology and microstructure during selective laser melting of Inconel 718 alloy [J]. J. Mater. Res. Technol., 2021, 11: 392
doi: 10.1016/j.jmrt.2021.01.024
|
| 23 |
Wei H L, Liu F Q, Wei L, et al. Multiscale and multiphysics explorations of the transient deposition processes and additive characteristics during laser 3D printing [J]. J. Mater. Sci. Technol., 2021, 77: 196
doi: 10.1016/j.jmst.2020.11.032
|
| 24 |
Wang L, Yan W T. Thermoelectric magnetohydrodynamic model for laser-based metal additive manufacturing [J]. Phys. Rev. Appl., 2021, 15: 064051
|
| 25 |
Chen H, Wei Q S, Wen S F, et al. Flow behavior of powder particles in layering process of selective laser melting: Numerical modeling and experimental verification based on discrete element method [J]. Int. J. Mach. Tools Manuf., 2017, 123: 146
doi: 10.1016/j.ijmachtools.2017.08.004
|
| 26 |
Khairallah S A, Anderson A T, Rubenchik A, et al. Laser powder-bed fusion additive manufacturing: Physics of complex melt flow and formation mechanisms of pores, spatter, and denudation zones [J]. Acta Mater., 2016, 108: 36
doi: 10.1016/j.actamat.2016.02.014
|
| 27 |
Zhang J L, Song B, Wei Q S, et al. A review of selective laser melting of aluminum alloys: Processing, microstructure, property and developing trends [J]. J. Mater. Sci. Technol., 2019, 35: 270
doi: 10.1016/j.jmst.2018.09.004
|
| 28 |
Yu G Q, Gu D D, Dai D H, et al. On the role of processing parameters in thermal behavior, surface morphology and accuracy during laser 3D printing of aluminum alloy [J]. J. Phys., 2016, 49D: 135501
|
| No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|