| THERMO-MECHANICAL TREATMENT OF 2O91 Al-Li ALLOY |
| YIN Zhimin;CHEN Xiaoqun;ZHANG Siqi;ZHANG Weibin Central South University of Technology; Changsha |
|
Cite this article:
YIN Zhimin;CHEN Xiaoqun;ZHANG Siqi;ZHANG Weibin Central South University of Technology; Changsha. THERMO-MECHANICAL TREATMENT OF 2O91 Al-Li ALLOY. Acta Metall Sin, 1991, 27(2): 52-58.
|
|
|
Abstract The effect of cold rolling prior to aging and two-step aging treatmenton the microstructure and mechanical properties of 2091 Al-Li alloy has been inves-tigated. The superior strength-ductility of the alloy may be matched by the treat-ment of 8% prior cold rolling and subsequently 170℃, 6h+190℃, 4 h double agingafter solid solutioning. The principal reasons for improving the strength-ducti-lity of the alloy are the suitable particle size of σ′ (Al_3Li), the dispersal precipita-tion of second strengthening phase S′ (Al_2CuMg) along dislocation substructures in-troduced by cold rolling, the decrease of equilibrium phase precipitated and thenarrowing σ′ precipitate free zone at grain boundary.
|
|
Received: 18 February 1991
|
1 Kim N J, Skinner D J, Okazaki K, Adam C M. In: Baker C, Gregson P J, Harris S J, Peel C J eds., Aluminum-Lithium Alloys, Proc 3th Int Aluminum-Lithium Conf, 8-11 July, 1985, University of Oxford, London: The Institute of Metals, 1986: 78 2 Sinko R J, Ahrens T, Shifiet G J, Starke E A Jr. In: Sanders T H Jr., Starke E A Jr. eds., Aluminum-Lithium Alloys, Proc 5th Int Aluminum-Lithium Conf, Williamsburg, Virginia, March 27-31, 1989, Birmingham, UK: Materials and Component Engineering Publications Ltd., 1989: 375 3 White J, Miller W S. In: Champier G, Dubost B, Miannay D, Sabetay L eds., 4th International Aluminium Lithium Conference, 10-12, June, 1987, Paris, J Phys (Paris), 1987; 48(C3) : 425 4 尹志民,Aust K T, Weatherly G C.金属学报,1988;24: A347 5 刘学志,中南工业大学硕士学位论文,1988 6 Xia Xiaoxin, Martin J W. In: Champier G, Dubost B, Miannay D, Sabetay L eds., 4 th International Aluminium Lithium Conference, 10-12, June, 1987, Paris, J Phys(Paris), 1987; 48(C3) : 433a |
| No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|