Please wait a minute...
Acta Metall Sin  1991, Vol. 27 Issue (2): 52-58    DOI:
Current Issue | Archive | Adv Search |
THERMO-MECHANICAL TREATMENT OF 2O91 Al-Li ALLOY
YIN Zhimin;CHEN Xiaoqun;ZHANG Siqi;ZHANG Weibin Central South University of Technology; Changsha
Cite this article: 

YIN Zhimin;CHEN Xiaoqun;ZHANG Siqi;ZHANG Weibin Central South University of Technology; Changsha. THERMO-MECHANICAL TREATMENT OF 2O91 Al-Li ALLOY. Acta Metall Sin, 1991, 27(2): 52-58.

Download:  PDF(2107KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  The effect of cold rolling prior to aging and two-step aging treatmenton the microstructure and mechanical properties of 2091 Al-Li alloy has been inves-tigated. The superior strength-ductility of the alloy may be matched by the treat-ment of 8% prior cold rolling and subsequently 170℃, 6h+190℃, 4 h double agingafter solid solutioning. The principal reasons for improving the strength-ducti-lity of the alloy are the suitable particle size of σ′ (Al_3Li), the dispersal precipita-tion of second strengthening phase S′ (Al_2CuMg) along dislocation substructures in-troduced by cold rolling, the decrease of equilibrium phase precipitated and thenarrowing σ′ precipitate free zone at grain boundary.
Key words:  Al-Li alloy      thermo-mechanical treatment      microstructure      mechanical properties     
Received:  18 February 1991     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1991/V27/I2/52

1 Kim N J, Skinner D J, Okazaki K, Adam C M. In: Baker C, Gregson P J, Harris S J, Peel C J eds., Aluminum-Lithium Alloys, Proc 3th Int Aluminum-Lithium Conf, 8-11 July, 1985, University of Oxford, London: The Institute of Metals, 1986: 78
2 Sinko R J, Ahrens T, Shifiet G J, Starke E A Jr. In: Sanders T H Jr., Starke E A Jr. eds., Aluminum-Lithium Alloys, Proc 5th Int Aluminum-Lithium Conf, Williamsburg, Virginia, March 27-31, 1989, Birmingham, UK: Materials and Component Engineering Publications Ltd., 1989: 375
3 White J, Miller W S. In: Champier G, Dubost B, Miannay D, Sabetay L eds., 4th International Aluminium Lithium Conference, 10-12, June, 1987, Paris, J Phys (Paris), 1987; 48(C3) : 425
4 尹志民,Aust K T, Weatherly G C.金属学报,1988;24: A347
5 刘学志,中南工业大学硕士学位论文,1988
6 Xia Xiaoxin, Martin J W. In: Champier G, Dubost B, Miannay D, Sabetay L eds., 4 th International Aluminium Lithium Conference, 10-12, June, 1987, Paris, J Phys(Paris), 1987; 48(C3) : 433a
[1] GONG Shengkai, LIU Yuan, GENG Lilun, RU Yi, ZHAO Wenyue, PEI Yanling, LI Shusuo. Advances in the Regulation and Interfacial Behavior of Coatings/Superalloys[J]. 金属学报, 2023, 59(9): 1097-1108.
[2] ZHANG Leilei, CHEN Jingyang, TANG Xin, XIAO Chengbo, ZHANG Mingjun, YANG Qing. Evolution of Microstructures and Mechanical Properties of K439B Superalloy During Long-Term Aging at 800oC[J]. 金属学报, 2023, 59(9): 1253-1264.
[3] LU Nannan, GUO Yimo, YANG Shulin, LIANG Jingjing, ZHOU Yizhou, SUN Xiaofeng, LI Jinguo. Formation Mechanisms of Hot Cracks in Laser Additive Repairing Single Crystal Superalloys[J]. 金属学报, 2023, 59(9): 1243-1252.
[4] WANG Lei, LIU Mengya, LIU Yang, SONG Xiu, MENG Fanqiang. Research Progress on Surface Impact Strengthening Mechanisms and Application of Nickel-Based Superalloys[J]. 金属学报, 2023, 59(9): 1173-1189.
[5] LIU Xingjun, WEI Zhenbang, LU Yong, HAN Jiajia, SHI Rongpei, WANG Cuiping. Progress on the Diffusion Kinetics of Novel Co-based and Nb-Si-based Superalloys[J]. 金属学报, 2023, 59(8): 969-985.
[6] LI Jingren, XIE Dongsheng, ZHANG Dongdong, XIE Hongbo, PAN Hucheng, REN Yuping, QIN Gaowu. Microstructure Evolution Mechanism of New Low-Alloyed High-Strength Mg-0.2Ce-0.2Ca Alloy During Extrusion[J]. 金属学报, 2023, 59(8): 1087-1096.
[7] CHEN Liqing, LI Xing, ZHAO Yang, WANG Shuai, FENG Yang. Overview of Research and Development of High-Manganese Damping Steel with Integrated Structure and Function[J]. 金属学报, 2023, 59(8): 1015-1026.
[8] SUN Rongrong, YAO Meiyi, WANG Haoyu, ZHANG Wenhuai, HU Lijuan, QIU Yunlong, LIN Xiaodong, XIE Yaoping, YANG Jian, DONG Jianxin, CHENG Guoguang. High-Temperature Steam Oxidation Behavior of Fe22Cr5Al3Mo-xY Alloy Under Simulated LOCA Condition[J]. 金属学报, 2023, 59(7): 915-925.
[9] ZHANG Deyin, HAO Xu, JIA Baorui, WU Haoyang, QIN Mingli, QU Xuanhui. Effects of Y2O3 Content on Properties of Fe-Y2O3 Nanocomposite Powders Synthesized by a Combustion-Based Route[J]. 金属学报, 2023, 59(6): 757-766.
[10] WANG Fa, JIANG He, DONG Jianxin. Evolution Behavior of Complex Precipitation Phases in Highly Alloyed GH4151 Superalloy[J]. 金属学报, 2023, 59(6): 787-796.
[11] WU Dongjiang, LIU Dehua, ZHANG Ziao, ZHANG Yilun, NIU Fangyong, MA Guangyi. Microstructure and Mechanical Properties of 2024 Aluminum Alloy Prepared by Wire Arc Additive Manufacturing[J]. 金属学报, 2023, 59(6): 767-776.
[12] GUO Fu, DU Yihui, JI Xiaoliang, WANG Yishu. Recent Progress on Thermo-Mechanical Reliability of Sn-Based Alloys and Composite Solder for Microelectronic Interconnection[J]. 金属学报, 2023, 59(6): 744-756.
[13] FENG Aihan, CHEN Qiang, WANG Jian, WANG Hao, QU Shoujiang, CHEN Daolun. Thermal Stability of Microstructures in Low-Density Ti2AlNb-Based Alloy Hot Rolled Plate[J]. 金属学报, 2023, 59(6): 777-786.
[14] LIU Manping, XUE Zhoulei, PENG Zhen, CHEN Yulin, DING Lipeng, JIA Zhihong. Effect of Post-Aging on Microstructure and Mechanical Properties of an Ultrafine-Grained 6061 Aluminum Alloy[J]. 金属学报, 2023, 59(5): 657-667.
[15] ZHANG Dongyang, ZHANG Jun, LI Shujun, REN Dechun, MA Yingjie, YANG Rui. Effect of Heat Treatment on Mechanical Properties of Porous Ti55531 Alloy Prepared by Selective Laser Melting[J]. 金属学报, 2023, 59(5): 647-656.
No Suggested Reading articles found!