Please wait a minute...
Acta Metall Sin  1991, Vol. 27 Issue (5): 1-7    DOI:
Current Issue | Archive | Adv Search |
A MICROSTRUCTURAL ANALYSIS OF 7050 ALUMINUM ALLOY
JIN Yan;LI Chunzhi;ZHAO Yingtao;YAN Minggao Beijing Institute of Aeronautical Materials Corresponden JIN Yan Department No.4; Institute of Aeronautical Materiais;
Cite this article: 

JIN Yan;LI Chunzhi;ZHAO Yingtao;YAN Minggao Beijing Institute of Aeronautical Materials Corresponden JIN Yan Department No.4; Institute of Aeronautical Materiais;. A MICROSTRUCTURAL ANALYSIS OF 7050 ALUMINUM ALLOY. Acta Metall Sin, 1991, 27(5): 1-7.

Download:  PDF(2137KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  The microstructure in 7050 Al alloy under heat treatment regime T74 has been studied by means of TEM and dynamical diffraction simulation. The alloy is found to contain mainly Al_3Zr superlattice phase, η′precipitate phase ard Al_?-Cu_? Fe constituent phase. The η′phase has a C-face centered orthorhombic crystal structure with a=0.492 nm, b=0.852 nm and c=0.701 nm. The orientation relation- ship between η′phase and matrix is determined as (101)_m//(010)_(η′), [111]_m//[001]_(η′).
Key words:  7050 Al alloy      microstructure      dynamical diffraction simulation     
Received:  18 May 1991     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1991/V27/I5/1

1 伊藤吾朗,江藤武比古,宫木美光,营野幹宏,轻金属,1988;38:818
2 Ryum N. Acta Metall, 1970; 17: 269
3 Nes E, Billdal H. Ser Metall, 1971; 5: 987
4 Mondolfo L F, Gjostein N A, Levinson D W Trans AIME, 1956; 206: 1378
5 Auger P, Raynal J M, Bernole M, Graf R. Mem Sci Rev Metall, 1974; 71: 557
6 Auld J H, Cousland S McK. J Aust Inst Met, 1974; 19: 194
7 Graf R. J Inst Met, 1957--58; 86: 535
8 Park J K, Ardell A J. Metall Trans, 1983; 14A: 1957
9 Gjonnes J, Simenson C J. Acta Metall, 1970; 18: 881
10 Ayer R, Koo J Y, Steeds J W, Park B K. Metall Trans, 1985; 16A: 1925
11 王顺才,李春志,边为民,颜鸣皋,金属学报,1989;25:A340
12 Li Chunzhi, Yan Minggao. Chin J Met Sci Technol, 1987; 3: 27
13 Shindo D, Hirabayashi M. Acta Crystallogr, 1988; A44: 954
[1] ZHANG Leilei, CHEN Jingyang, TANG Xin, XIAO Chengbo, ZHANG Mingjun, YANG Qing. Evolution of Microstructures and Mechanical Properties of K439B Superalloy During Long-Term Aging at 800oC[J]. 金属学报, 2023, 59(9): 1253-1264.
[2] LU Nannan, GUO Yimo, YANG Shulin, LIANG Jingjing, ZHOU Yizhou, SUN Xiaofeng, LI Jinguo. Formation Mechanisms of Hot Cracks in Laser Additive Repairing Single Crystal Superalloys[J]. 金属学报, 2023, 59(9): 1243-1252.
[3] WANG Lei, LIU Mengya, LIU Yang, SONG Xiu, MENG Fanqiang. Research Progress on Surface Impact Strengthening Mechanisms and Application of Nickel-Based Superalloys[J]. 金属学报, 2023, 59(9): 1173-1189.
[4] GONG Shengkai, LIU Yuan, GENG Lilun, RU Yi, ZHAO Wenyue, PEI Yanling, LI Shusuo. Advances in the Regulation and Interfacial Behavior of Coatings/Superalloys[J]. 金属学报, 2023, 59(9): 1097-1108.
[5] LI Jingren, XIE Dongsheng, ZHANG Dongdong, XIE Hongbo, PAN Hucheng, REN Yuping, QIN Gaowu. Microstructure Evolution Mechanism of New Low-Alloyed High-Strength Mg-0.2Ce-0.2Ca Alloy During Extrusion[J]. 金属学报, 2023, 59(8): 1087-1096.
[6] LIU Xingjun, WEI Zhenbang, LU Yong, HAN Jiajia, SHI Rongpei, WANG Cuiping. Progress on the Diffusion Kinetics of Novel Co-based and Nb-Si-based Superalloys[J]. 金属学报, 2023, 59(8): 969-985.
[7] CHEN Liqing, LI Xing, ZHAO Yang, WANG Shuai, FENG Yang. Overview of Research and Development of High-Manganese Damping Steel with Integrated Structure and Function[J]. 金属学报, 2023, 59(8): 1015-1026.
[8] SUN Rongrong, YAO Meiyi, WANG Haoyu, ZHANG Wenhuai, HU Lijuan, QIU Yunlong, LIN Xiaodong, XIE Yaoping, YANG Jian, DONG Jianxin, CHENG Guoguang. High-Temperature Steam Oxidation Behavior of Fe22Cr5Al3Mo-xY Alloy Under Simulated LOCA Condition[J]. 金属学报, 2023, 59(7): 915-925.
[9] ZHANG Deyin, HAO Xu, JIA Baorui, WU Haoyang, QIN Mingli, QU Xuanhui. Effects of Y2O3 Content on Properties of Fe-Y2O3 Nanocomposite Powders Synthesized by a Combustion-Based Route[J]. 金属学报, 2023, 59(6): 757-766.
[10] WU Dongjiang, LIU Dehua, ZHANG Ziao, ZHANG Yilun, NIU Fangyong, MA Guangyi. Microstructure and Mechanical Properties of 2024 Aluminum Alloy Prepared by Wire Arc Additive Manufacturing[J]. 金属学报, 2023, 59(6): 767-776.
[11] GUO Fu, DU Yihui, JI Xiaoliang, WANG Yishu. Recent Progress on Thermo-Mechanical Reliability of Sn-Based Alloys and Composite Solder for Microelectronic Interconnection[J]. 金属学报, 2023, 59(6): 744-756.
[12] FENG Aihan, CHEN Qiang, WANG Jian, WANG Hao, QU Shoujiang, CHEN Daolun. Thermal Stability of Microstructures in Low-Density Ti2AlNb-Based Alloy Hot Rolled Plate[J]. 金属学报, 2023, 59(6): 777-786.
[13] WANG Fa, JIANG He, DONG Jianxin. Evolution Behavior of Complex Precipitation Phases in Highly Alloyed GH4151 Superalloy[J]. 金属学报, 2023, 59(6): 787-796.
[14] WANG Changsheng, FU Huadong, ZHANG Hongtao, XIE Jianxin. Effect of Cold-Rolling Deformation on Microstructure, Properties, and Precipitation Behavior of High-Performance Cu-Ni-Si Alloys[J]. 金属学报, 2023, 59(5): 585-598.
[15] ZHANG Dongyang, ZHANG Jun, LI Shujun, REN Dechun, MA Yingjie, YANG Rui. Effect of Heat Treatment on Mechanical Properties of Porous Ti55531 Alloy Prepared by Selective Laser Melting[J]. 金属学报, 2023, 59(5): 647-656.
No Suggested Reading articles found!