Please wait a minute...
Acta Metall Sin  1991, Vol. 27 Issue (5): 8-13    DOI:
Current Issue | Archive | Adv Search |
SYMMETRICAL SUPERLATTICE INTRINSJC STACKING FAULTS IN DEFORMEDPOLYCRYSTALLINE Ni_3 Al AND THEIR FORMATION MECHANISM
YAN Wen Xi'an Institute of Technology Correspondent associate professor;xi'an Institute of Technology
Cite this article: 

YAN Wen Xi'an Institute of Technology Correspondent associate professor;xi'an Institute of Technology. SYMMETRICAL SUPERLATTICE INTRINSJC STACKING FAULTS IN DEFORMEDPOLYCRYSTALLINE Ni_3 Al AND THEIR FORMATION MECHANISM. Acta Metall Sin, 1991, 27(5): 8-13.

Download:  PDF(1942KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  TEM analysis and computer simulation of the symmetrical superlattice intrinsic stacking faults (SISFs) in slightly deformed polycrystalline Ni_3Al at room temperature are presented. The symmetrical SISFs are important components of the crystal defects in deformed Ni_3Al alloys; the formation mechanism of the symmetrical SISF can be resulted from the reorientation, dissociation and annihilation of a dipole on {111} plane under applied shear stress.
Key words:  polycrystalline Ni_3Al      symmetrical SISF      computer simulation     
Received:  18 May 1991     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1991/V27/I5/8

1 Takeuchi S, Kuramoto E, Yamamoto T, Taoka T. Jpn J Appl phys, 1973; 12: 1486--1592
2 Baker I, Schulson E M. Phys Status Solidi, 1984; A85: 481--490
3 Baker I, Schulson E M. Phys Status Solidi, 1985; A89: 163--172
4 Baker I, Schulson E M, Horton J A. Acta Metall, 1987; 35: 1533--1541
5 Yan W, Jones I P, Smallman R E. Ser Metall, 1987; 21: 1511--1515
6 严文.兵器材料科学与工程,1989;8:103--111
7 Pak H-R, Saburi T, Nenno S. Ser Metall, 1976; 10: 1081--1085
8 Pope D P, Ezz S S. Int Met Rev, 1984; 29: 136--167
9 Yan W PhD Dissertation, University of Birmingham, UK, 1988
10 Head A K, Humble P, Clarebrough L M, Morton A J, Forwood C T. Computed Electron Micrographs and Defect Identification, Amsterdam: North-Holland, 1973
11 Suzuki K, Kuramoto E, Takeuchi S, Ichihara M. Jpn J Appl Phys, 1977; 16: 919--923
12 Suzuki K, Ichihara M, Takeuchi S. Acta Metall, 1979; 27: 193--200
[1] ;. STUDY OF 3D QUASI--STATIONARY GRAIN SIZE DISTRIBUTION DERIVED FROM MACPHERSON—SROLOVITZ TOPOLOGY--RELATED GRAIN GROWTH RATE EQUATION[J]. 金属学报, 2008, 44(7): 769-774 .
[2] zhang lin. Modelling structural changes of a molten Cu55 cluster on cooling by molecular dynamics[J]. 金属学报, 2008, 44(10): 1161-1166 .
[3] HOU Hua; ZHAO Yuhong; CHEN Zheng; XU Hong. Prediction for the Early Precipitation Process of Ni75AlxV25-X System with Lower Al Concentration by the Phase-Field Model[J]. 金属学报, 2005, 41(7): 695-702 .
[4] ZHANG Lin; ZHANG Caibei; WANG Yuanming; WANG Shaoqing. Cellular Automaton Modelling Of The Transformation From Austenite to Ferrite In Low Carbon Steels During Continuous Cooling[J]. 金属学报, 2004, 40(1): 8-13 .
[5] CHU Yelong; XIONG Liangyue; SUN Xiaokai (Institute of Metal Research; The Chinese Academy of Sciences; Shenyang 110015). COMPUTER STUDY OF MAGNETIZATION IN NANOCOMPOSITE MAGNETS[J]. 金属学报, 1998, 34(4): 423-430.
[6] SUI Zhitong;ZHANG Peixin(Northeastern University; Shenyang 110006). SELECTIVE PRECIPITATING BEHAVIOR OF THE BORON COMPONENTS FROM THE BORON SLAGS[J]. 金属学报, 1997, 33(9): 943-951.
[7] YIN Aijun; LI Jing; LI Hinhai; HUANG Kexiong; JIANG Hanying (Central South University of Technology; Changsha 410083) (Manuscript received 1995-06-30; in revised form 1995-12-01). COMPUTER SIMULATION ON MINOR ELEMENT BEHAVIOUR IN COPPER FLASH SMELTING[J]. 金属学报, 1996, 32(4): 387-392.
[8] CAI Xun; ZHOU Pingnan; (Shanghai Jiaotong University ; Shanghai 200030)Bangert H (Technical University of Vienna; Auslria)(Manuscript received 94-07-18). SIMULATION OF INDENTATION MICROHARDNESS TESTING[J]. 金属学报, 1995, 31(13): 44-5.
[9] CAO Zhenning(Shandong Polytechnic Unversity; Jinan);WU Chuansong; WU Lin (Harbin Institute of Technology). COMPUTER SIMULATION OF MIG WELD POOLS WITH DROPLET IMPACT[J]. 金属学报, 1994, 30(24): 537-542.
[10] CHEN Da;LU Min;LIN Dongliang (Lin T L) Shanghai Jiao Tong UniversityDepartment of Materials Science;Shanghai Jiao Tong University; Shanghai 200030. SIMULATIVE STUDY OF INTERACTION BETWEEN GRAIN BOUNDARIES AND DISLOCATIONS IN Ni_3Al[J]. 金属学报, 1993, 29(7): 34-39.
[11] SHAO Jun;XU Hua;CHENG Ailan;KLEIN M. L. University of Pennsylvania; Philadelphia; U. S. A; State University of New York; U. S. A.; University of Pennsylvania; Philadelphia; U. S. A.. CONSTANT PRESSURE MOLECULAR DYNAMICS SIMULATION OF MOLTEN LiF-BeF_2 SYSTEM[J]. 金属学报, 1993, 29(1): 59-64.
[12] WANG Xi;ZHOU Jiankun;CHEN Youshan;LIU Xianghuai;ZOU Shichang Ion Beam Laboratory; Shanghai Institute of Metallurgy; Academia Sinica. COMPUTER SIMULATION OF ION BEAM ENHANCED DEPOSITION OF TiN FILMS[J]. 金属学报, 1991, 27(3): 136-141.
[13] WEI Chao;QIAN Rengen;LIN Shi;XIAO Jimei University of Science and Technology Beijing Department of mathematics and mechanics; University of Science and Technology Beijing; Beijing 100083. COMPUTER SIMULATION OF EFFECT OF ORIENTATION DIFFERENCE ON MECHANICAL PROPERTIES OF BICRYSTALLINE SPECIMENS[J]. 金属学报, 1990, 26(4): 18-21.
[14] LIN Dongliang;CHEN Da T. L. Lin Shanghai Jiaotong University professor;Department of Materials Science;Shanghai Jiaotong University;Shanghai 200030. COMPUTER SIMULATION OF GRAIN BOUNDARY STRUCTURES IN Ni_3 Al[J]. 金属学报, 1990, 26(3): 10-17.
[15] XIA Lifang;YAN Mufu Harbin Institute of TechnologyDivision of Metal Materials and Heat treatment; Harbin Institute of Technology; Harbin. MATHEMATICAL MODELS OF NITROGEN CONCENTRATION PROFILE OF ION NITRIDED LAYERS AND COMPUTER SIMULATION[J]. 金属学报, 1988, 24(4): 314-321.
No Suggested Reading articles found!