Acta Metall Sin  1992, Vol. 28 Issue (1): 21-26    DOI:
Current Issue | Archive | Adv Search |
EFFECT OF MICROSTRUCTURE ON MECHANICAL PROPERTIES OF INCOLOY 907
XIE Yun;YANG Ke;ZHAO Xu;FAN Cungan;LI Yiyi Institute of Metal Research; Academia Sinica; Shenyang
Cite this article: 

XIE Yun;YANG Ke;ZHAO Xu;FAN Cungan;LI Yiyi Institute of Metal Research; Academia Sinica; Shenyang. EFFECT OF MICROSTRUCTURE ON MECHANICAL PROPERTIES OF INCOLOY 907. Acta Metall Sin, 1992, 28(1): 21-26.

Download:  PDF(2233KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  Effect of microstructure on the mechanical properties of a precipitation strengthening Fe--Ni--Co based low expansion alloy, Incoloy 907, has been investigated under different heat treatments. the dispersed γ phase is found to be the principal strengthening phase in the alloy. The microstructure of the alloy with even dispersed fine γ' phase seems to have the best match of its mechanical properties. However, it will be worsened if the alloy aged at some higher temperature or overaged to precipitate needle--like ε phase.
Key words:  precipitation strengthening      Incoloy      microstructure      mechanical property     
Received:  18 January 1992     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1992/V28/I1/21

1 Alloy Digest, Feb., 1988
2 Carpenter H W. Met Prog, 1976; 110(3) : 25
3 陈淦生,赵兴隆,郑汉平,江贵藻.见:冶金工业部钢铁研究总院汇编,第6届全国高温合金年会论文集,1987:227
4 郑汉平,刘凤英,刘群,章锦芝,陈淦生,赵兴隆.见:冶金工业部钢铁研究总院汇编,第6届金国高温合金年会论文集,1987:289
5 尚世显,江贵藻.航空材料,1989;9(2) :17
6 Ernst S C, Baeslack W A Ⅲ, Lippold J C. Weld J, 1989; 68(10) : 418-s
7 章守华主编.合金纲,北京:冶金工业出版社,1981:230
8 Summers L T, Dal der E N C. Adv Cryog Eng, 1986; 32: 73
[1] GONG Shengkai, LIU Yuan, GENG Lilun, RU Yi, ZHAO Wenyue, PEI Yanling, LI Shusuo. Advances in the Regulation and Interfacial Behavior of Coatings/Superalloys[J]. 金属学报, 2023, 59(9): 1097-1108.
[2] ZHANG Jian, WANG Li, XIE Guang, WANG Dong, SHEN Jian, LU Yuzhang, HUANG Yaqi, LI Yawei. Recent Progress in Research and Development of Nickel-Based Single Crystal Superalloys[J]. 金属学报, 2023, 59(9): 1109-1124.
[3] ZHENG Liang, ZHANG Qiang, LI Zhou, ZHANG Guoqing. Effects of Oxygen Increasing/Decreasing Processes on Surface Characteristics of Superalloy Powders and Properties of Their Bulk Alloy Counterparts: Powders Storage and Degassing[J]. 金属学报, 2023, 59(9): 1265-1278.
[4] WANG Lei, LIU Mengya, LIU Yang, SONG Xiu, MENG Fanqiang. Research Progress on Surface Impact Strengthening Mechanisms and Application of Nickel-Based Superalloys[J]. 金属学报, 2023, 59(9): 1173-1189.
[5] ZHANG Leilei, CHEN Jingyang, TANG Xin, XIAO Chengbo, ZHANG Mingjun, YANG Qing. Evolution of Microstructures and Mechanical Properties of K439B Superalloy During Long-Term Aging at 800oC[J]. 金属学报, 2023, 59(9): 1253-1264.
[6] LU Nannan, GUO Yimo, YANG Shulin, LIANG Jingjing, ZHOU Yizhou, SUN Xiaofeng, LI Jinguo. Formation Mechanisms of Hot Cracks in Laser Additive Repairing Single Crystal Superalloys[J]. 金属学报, 2023, 59(9): 1243-1252.
[7] CHEN Liqing, LI Xing, ZHAO Yang, WANG Shuai, FENG Yang. Overview of Research and Development of High-Manganese Damping Steel with Integrated Structure and Function[J]. 金属学报, 2023, 59(8): 1015-1026.
[8] LIU Xingjun, WEI Zhenbang, LU Yong, HAN Jiajia, SHI Rongpei, WANG Cuiping. Progress on the Diffusion Kinetics of Novel Co-based and Nb-Si-based Superalloys[J]. 金属学报, 2023, 59(8): 969-985.
[9] LI Jingren, XIE Dongsheng, ZHANG Dongdong, XIE Hongbo, PAN Hucheng, REN Yuping, QIN Gaowu. Microstructure Evolution Mechanism of New Low-Alloyed High-Strength Mg-0.2Ce-0.2Ca Alloy During Extrusion[J]. 金属学报, 2023, 59(8): 1087-1096.
[10] DING Hua, ZHANG Yu, CAI Minghui, TANG Zhengyou. Research Progress and Prospects of Austenite-Based Fe-Mn-Al-C Lightweight Steels[J]. 金属学报, 2023, 59(8): 1027-1041.
[11] YUAN Jianghuai, WANG Zhenyu, MA Guanshui, ZHOU Guangxue, CHENG Xiaoying, WANG Aiying. Effect of Phase-Structure Evolution on Mechanical Properties of Cr2AlC Coating[J]. 金属学报, 2023, 59(7): 961-968.
[12] SUN Rongrong, YAO Meiyi, WANG Haoyu, ZHANG Wenhuai, HU Lijuan, QIU Yunlong, LIN Xiaodong, XIE Yaoping, YANG Jian, DONG Jianxin, CHENG Guoguang. High-Temperature Steam Oxidation Behavior of Fe22Cr5Al3Mo-xY Alloy Under Simulated LOCA Condition[J]. 金属学报, 2023, 59(7): 915-925.
[13] ZHANG Deyin, HAO Xu, JIA Baorui, WU Haoyang, QIN Mingli, QU Xuanhui. Effects of Y2O3 Content on Properties of Fe-Y2O3 Nanocomposite Powders Synthesized by a Combustion-Based Route[J]. 金属学报, 2023, 59(6): 757-766.
[14] WANG Fa, JIANG He, DONG Jianxin. Evolution Behavior of Complex Precipitation Phases in Highly Alloyed GH4151 Superalloy[J]. 金属学报, 2023, 59(6): 787-796.
[15] GUO Fu, DU Yihui, JI Xiaoliang, WANG Yishu. Recent Progress on Thermo-Mechanical Reliability of Sn-Based Alloys and Composite Solder for Microelectronic Interconnection[J]. 金属学报, 2023, 59(6): 744-756.
No Suggested Reading articles found!