EFFECT OF MICROSTRUCTURE ON MECHANICAL PROPERTIES OF INCOLOY 907
XIE Yun;YANG Ke;ZHAO Xu;FAN Cungan;LI Yiyi Institute of Metal Research; Academia Sinica; Shenyang
Cite this article:
XIE Yun;YANG Ke;ZHAO Xu;FAN Cungan;LI Yiyi Institute of Metal Research; Academia Sinica; Shenyang. EFFECT OF MICROSTRUCTURE ON MECHANICAL PROPERTIES OF INCOLOY 907. Acta Metall Sin, 1992, 28(1): 21-26.
Abstract Effect of microstructure on the mechanical properties of a precipitation strengthening Fe--Ni--Co based low expansion alloy, Incoloy 907, has been investigated under different heat treatments. the dispersed γ phase is found to be the principal strengthening phase in the alloy. The microstructure of the alloy with even dispersed fine γ' phase seems to have the best match of its mechanical properties. However, it will be worsened if the alloy aged at some higher temperature or overaged to precipitate needle--like ε phase.
1 Alloy Digest, Feb., 1988 2 Carpenter H W. Met Prog, 1976; 110(3) : 25 3 陈淦生,赵兴隆,郑汉平,江贵藻.见:冶金工业部钢铁研究总院汇编,第6届全国高温合金年会论文集,1987:227 4 郑汉平,刘凤英,刘群,章锦芝,陈淦生,赵兴隆.见:冶金工业部钢铁研究总院汇编,第6届金国高温合金年会论文集,1987:289 5 尚世显,江贵藻.航空材料,1989;9(2) :17 6 Ernst S C, Baeslack W A Ⅲ, Lippold J C. Weld J, 1989; 68(10) : 418-s 7 章守华主编.合金纲,北京:冶金工业出版社,1981:230 8 Summers L T, Dal der E N C. Adv Cryog Eng, 1986; 32: 73