STRUCTURE OF HYDRIDES IN HIGHLY HYDROGENATED Ti-6Al-4V ALLOYS
ZHANG Caibei;BIAN Weimin;LAI Zuhan;GONG Bo Northeast University of Technology; Shenyang
Cite this article: 

ZHANG Caibei;BIAN Weimin;LAI Zuhan;GONG Bo Northeast University of Technology; Shenyang. STRUCTURE OF HYDRIDES IN HIGHLY HYDROGENATED Ti-6Al-4V ALLOYS. Acta Metall Sin, 1992, 28(4): 10-16.

Download:  PDF(2600KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  The microstructure and various hydrides precipitated in Ti--6Al--4V alloys con-taining hydrogen 0.16, 0.58, 0.87, 1.49 wt--%, respectively, have been studied by means of TEMand X--ray diffraction. The Ti_3Al phase may precipitate when [H] over 0.58 wt--%. In thesame time, the morphology of hydrides gradually changed from rugged sheets to narrow laths as[H] contents increased. The microstructure of highly H--doped alloys is obviously fine. A mas-sive hydride and the hydride with tetragonal lattice were observed in the specimen containing1.49 wt--% H. The twin hydrides were found in the alloys with different H contents and theelectron diffraction patterns of the twin hydrides can be served as a simple criterion for distin-guishing the cubic and tetragonal structures.
Key words:  titanium hydride      microstructure      twin hydride     
Received:  18 April 1992     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1992/V28/I4/10

1 徐振声,宫波,张彩碚,赖祖涵.金属学报,1991;27:A270
2 Karpenko G V, Kuzin O A, Tkachev V I, Rudenko V P. Dokl Akad Nauk SSSR, 1976; 85: 227
3 Hall I W. Scand J Metall, 1978; 7: 277
4 Gong B, Lai Z H, Zhang C B, Chin J Met Sci Technol, 1991; 6: 425
5 Woo O T, Weatherly G C, Coleman C E, Gilbert R W. Acta Metall, 1985; 33: 1897
6 Hall I W. Metall Trans, 1978; 9A: 815^
[1] WANG Lei, LIU Mengya, LIU Yang, SONG Xiu, MENG Fanqiang. Research Progress on Surface Impact Strengthening Mechanisms and Application of Nickel-Based Superalloys[J]. 金属学报, 2023, 59(9): 1173-1189.
[2] GONG Shengkai, LIU Yuan, GENG Lilun, RU Yi, ZHAO Wenyue, PEI Yanling, LI Shusuo. Advances in the Regulation and Interfacial Behavior of Coatings/Superalloys[J]. 金属学报, 2023, 59(9): 1097-1108.
[3] ZHANG Leilei, CHEN Jingyang, TANG Xin, XIAO Chengbo, ZHANG Mingjun, YANG Qing. Evolution of Microstructures and Mechanical Properties of K439B Superalloy During Long-Term Aging at 800oC[J]. 金属学报, 2023, 59(9): 1253-1264.
[4] LU Nannan, GUO Yimo, YANG Shulin, LIANG Jingjing, ZHOU Yizhou, SUN Xiaofeng, LI Jinguo. Formation Mechanisms of Hot Cracks in Laser Additive Repairing Single Crystal Superalloys[J]. 金属学报, 2023, 59(9): 1243-1252.
[5] LI Jingren, XIE Dongsheng, ZHANG Dongdong, XIE Hongbo, PAN Hucheng, REN Yuping, QIN Gaowu. Microstructure Evolution Mechanism of New Low-Alloyed High-Strength Mg-0.2Ce-0.2Ca Alloy During Extrusion[J]. 金属学报, 2023, 59(8): 1087-1096.
[6] LIU Xingjun, WEI Zhenbang, LU Yong, HAN Jiajia, SHI Rongpei, WANG Cuiping. Progress on the Diffusion Kinetics of Novel Co-based and Nb-Si-based Superalloys[J]. 金属学报, 2023, 59(8): 969-985.
[7] CHEN Liqing, LI Xing, ZHAO Yang, WANG Shuai, FENG Yang. Overview of Research and Development of High-Manganese Damping Steel with Integrated Structure and Function[J]. 金属学报, 2023, 59(8): 1015-1026.
[8] SUN Rongrong, YAO Meiyi, WANG Haoyu, ZHANG Wenhuai, HU Lijuan, QIU Yunlong, LIN Xiaodong, XIE Yaoping, YANG Jian, DONG Jianxin, CHENG Guoguang. High-Temperature Steam Oxidation Behavior of Fe22Cr5Al3Mo-xY Alloy Under Simulated LOCA Condition[J]. 金属学报, 2023, 59(7): 915-925.
[9] ZHANG Deyin, HAO Xu, JIA Baorui, WU Haoyang, QIN Mingli, QU Xuanhui. Effects of Y2O3 Content on Properties of Fe-Y2O3 Nanocomposite Powders Synthesized by a Combustion-Based Route[J]. 金属学报, 2023, 59(6): 757-766.
[10] WU Dongjiang, LIU Dehua, ZHANG Ziao, ZHANG Yilun, NIU Fangyong, MA Guangyi. Microstructure and Mechanical Properties of 2024 Aluminum Alloy Prepared by Wire Arc Additive Manufacturing[J]. 金属学报, 2023, 59(6): 767-776.
[11] GUO Fu, DU Yihui, JI Xiaoliang, WANG Yishu. Recent Progress on Thermo-Mechanical Reliability of Sn-Based Alloys and Composite Solder for Microelectronic Interconnection[J]. 金属学报, 2023, 59(6): 744-756.
[12] WANG Fa, JIANG He, DONG Jianxin. Evolution Behavior of Complex Precipitation Phases in Highly Alloyed GH4151 Superalloy[J]. 金属学报, 2023, 59(6): 787-796.
[13] FENG Aihan, CHEN Qiang, WANG Jian, WANG Hao, QU Shoujiang, CHEN Daolun. Thermal Stability of Microstructures in Low-Density Ti2AlNb-Based Alloy Hot Rolled Plate[J]. 金属学报, 2023, 59(6): 777-786.
[14] WANG Changsheng, FU Huadong, ZHANG Hongtao, XIE Jianxin. Effect of Cold-Rolling Deformation on Microstructure, Properties, and Precipitation Behavior of High-Performance Cu-Ni-Si Alloys[J]. 金属学报, 2023, 59(5): 585-598.
[15] LIU Manping, XUE Zhoulei, PENG Zhen, CHEN Yulin, DING Lipeng, JIA Zhihong. Effect of Post-Aging on Microstructure and Mechanical Properties of an Ultrafine-Grained 6061 Aluminum Alloy[J]. 金属学报, 2023, 59(5): 657-667.
No Suggested Reading articles found!