Please wait a minute...
Acta Metall Sin  1992, Vol. 28 Issue (4): 5-9    DOI:
Current Issue | Archive | Adv Search |
ISOTROPIC YIELD BEHAVIOURS OF FCC AND BCC METALS
CHEN Jiwei;LIAN Jianshe Jilin University of Technology; Changchun
Cite this article: 

CHEN Jiwei;LIAN Jianshe Jilin University of Technology; Changchun. ISOTROPIC YIELD BEHAVIOURS OF FCC AND BCC METALS. Acta Metall Sin, 1992, 28(4): 5-9.

Download:  PDF(365KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  Isotropic yield surfaces of both fcc and bcc metals have been simulated with theTBH model. Using the five--dimensional stress space proposed recently by Lequeu et al., theyield subsurface on any two of the three shear stresses can be considered approximately as in-scribed circles of their corresponding subsurface on π plane. Based on this concept, the HHHyield function has been transformed into the form where the parameters are uniquely deter-mined by two crystallographic factors: the mean Taylor factor in plane strain (M_p) and thecritical shear stress (τ_c) on slip systems.
Key words:  polycrystalline plasticity      yield function      cubic metals     
Received:  18 April 1992     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1992/V28/I4/5

1 Taylor G I. J Inst Met, 1938; 62: 307
2 Bishop J W F. Hill R. Philos Mag, 1951; 42: 414, 1298
3 Lequeu P. Gilormini P, Montheillet F. Bacroix B, Jonas J J. Acta Metall, 1987; 35: 439, 1159
4 Kocks U F, Canova G R. Jonas J J. Acta Metall, 1983; 31: 1243
5 Van Houtte P. Aernoudt E. Z Metallk, 1975; 66: 202
6 Lequeu P, Jonas J J. Metall Trans, 1988; 19A: 105
7 Hill R. Proc R Soc London, 1948; 193A: 281
8 Chin G Y. Mammel W L. Trans Metall Soc AIME, 1969; 245: 1211
9 Bacroix B. Jonas J J, Montheillet F, Skalli A. Acta Metall, 1986; 34: 937
10 Hershey A V. Trans ASME, Ser. E: J Appl Mech, 1954; 76: 241
11 Hosford W F. Trans ASME, Ser. E: J Appl Mech, 1972; 39: 607
12 Hill R. Math Prog Cambridge Philos Soc, 1979; 85: 179
13 Barlat F, Lian J. Int J Plasticity, 1989; 5: 51
14 Lian J, Barlat F, Baudelet B. Int J Plasticity, 1989; 5: 131@
No related articles found!