| STRUCTURE OF HYDRIDES IN HIGHLY HYDROGENATED Ti-6Al-4V ALLOYS |
| ZHANG Caibei;BIAN Weimin;LAI Zuhan;GONG Bo Northeast University of Technology; Shenyang |
|
Cite this article:
ZHANG Caibei;BIAN Weimin;LAI Zuhan;GONG Bo Northeast University of Technology; Shenyang. STRUCTURE OF HYDRIDES IN HIGHLY HYDROGENATED Ti-6Al-4V ALLOYS. Acta Metall Sin, 1992, 28(4): 10-16.
|
|
|
Abstract The microstructure and various hydrides precipitated in Ti--6Al--4V alloys con-taining hydrogen 0.16, 0.58, 0.87, 1.49 wt--%, respectively, have been studied by means of TEMand X--ray diffraction. The Ti_3Al phase may precipitate when [H] over 0.58 wt--%. In thesame time, the morphology of hydrides gradually changed from rugged sheets to narrow laths as[H] contents increased. The microstructure of highly H--doped alloys is obviously fine. A mas-sive hydride and the hydride with tetragonal lattice were observed in the specimen containing1.49 wt--% H. The twin hydrides were found in the alloys with different H contents and theelectron diffraction patterns of the twin hydrides can be served as a simple criterion for distin-guishing the cubic and tetragonal structures.
|
|
Received: 18 April 1992
|
1 徐振声,宫波,张彩碚,赖祖涵.金属学报,1991;27:A270 2 Karpenko G V, Kuzin O A, Tkachev V I, Rudenko V P. Dokl Akad Nauk SSSR, 1976; 85: 227 3 Hall I W. Scand J Metall, 1978; 7: 277 4 Gong B, Lai Z H, Zhang C B, Chin J Met Sci Technol, 1991; 6: 425 5 Woo O T, Weatherly G C, Coleman C E, Gilbert R W. Acta Metall, 1985; 33: 1897 6 Hall I W. Metall Trans, 1978; 9A: 815^ |
| No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|