| PREPARATION OF ULTRAFINE METALLIC PARTICLES BY γ-RAY RADIATION HYDROTHERMAL CRYSTALLIZATION COMBINED METHOD |
| CHEN Zuyao;CHEN Bo;QIAN Yitai;ZHANG Manwei;YANG Li;FAN Chenggao University of Science and Technology of China; Hefei |
|
Cite this article:
CHEN Zuyao;CHEN Bo;QIAN Yitai;ZHANG Manwei;YANG Li;FAN Chenggao University of Science and Technology of China; Hefei. PREPARATION OF ULTRAFINE METALLIC PARTICLES BY γ-RAY RADIATION HYDROTHERMAL CRYSTALLIZATION COMBINED METHOD. Acta Metall Sin, 1992, 28(4): 73-76.
|
|
|
Abstract The combined method of γ-ray radiation together with hydrothermalcrystallization was firstly adopted to prepare the ultrafine particles of Cu or Au metal as well asCu-Au alloy. Discussions were also made of their nucleation, feature, size and stability.
|
|
Received: 18 April 1992
|
1 Fujita H, Izawa M, Yamaziki H, Nature, 1962; 196: 666 2 Belloni J, Delcourt M O, Leclere C. Nouv J Chim. 1982; 6: 507 3 Delcourt M O, Keghouche N, Belloni J. Nouv J Chim, 1983; 7: 131 4 Delcoure M O, Belloni J, Marignier J L, Mory C, Collex C. Radiat Phys Chem, 1984; 23: 485 5 Marignier J L, Belloni J, Deicourt M O, Chevalier J P. Nature, 1985; 317: 344 6 Bruneaux J, Cachet H, Froment M, Amblard J, Belloni J, Mostafavi M. Electrochim Acta, 1987; 32: 1533 7 Belloni J, Deicourt M O, Marignier J L. Amblard J. In: Hedwig. P, Nyokos L Schiller r eds., Akademial Kiado, Proc 6th Symp. on Radiation Chem., Budapest: 1987; 89 8 Hayashi T, Ohno T, Yatsuya S. Uyeda R, Jpn J Appl Phys, 1977; 16: 705 |