| EFFECT OF COOLING RATE AND Ce CONTENT ON STRUCTURE OF RAPIDLY SOLIDIFIED Al-Ce BINARY ALLOYS |
| QIU Qingrong;LI Qingchun;JIANG Zuling Harbin Institute of Technology |
|
Cite this article:
QIU Qingrong;LI Qingchun;JIANG Zuling Harbin Institute of Technology. EFFECT OF COOLING RATE AND Ce CONTENT ON STRUCTURE OF RAPIDLY SOLIDIFIED Al-Ce BINARY ALLOYS. Acta Metall Sin, 1993, 29(2): 20-23.
|
|
|
Abstract Less Ce content in rapidly solidified Al-Ce alloys at a certain cooling rate wasfound to facilitate the formation of granular disperse phase. While the alloys with definitecomposition may easily precipitate globular grains of higher dispersity if the cooling rate wasaccelerated.
|
|
Received: 18 February 1993
|
1 Ruder A, Eliezer D. J Mater Sci, 1990; 25: 3541 2 神尾彰彦,手塚裕康,里达雄,Long T T,高桥恒夫.轻金属,1985;35:439 3 Ayer R, Angers L M, Mueller R R, Scanlon J C, Klein C F. Metall Trans. 1988; 19A: 1645 4 Burden M H, Jones H. J Inst Met, 1970; 98: 249 5 Sato T, Ohira G. Trans Jpn Inst Met, 197l; 12: 285 6 Ungar L H, Brown R A. Phys Rev, 1985; 31: 5931C |
| No Suggested Reading articles found! |
|
|