| BEHAVIOUR OF Mg AND ITS EFFECT ON MECHANICAL PROPERTIES OF CAST Fe_3Al ALLOY |
| YIN Weimin;HU Zhuangqi;Institute of Metal Research; Academia Sinica; ShenyangGUO Jianting.Professor;Institute of Metal Research;Acsdemia Sinieca;Shenyang110015 |
|
Cite this article:
YIN Weimin;HU Zhuangqi;Institute of Metal Research; Academia Sinica; ShenyangGUO Jianting.Professor;Institute of Metal Research;Acsdemia Sinieca;Shenyang110015. BEHAVIOUR OF Mg AND ITS EFFECT ON MECHANICAL PROPERTIES OF CAST Fe_3Al ALLOY. Acta Metall Sin, 1993, 29(5): 1-6.
|
|
|
Abstract Proper addition of 0.002wt-% Mg to cast Fe_3Al alloy may obviously improvethe room and high temperature tensile properties. Auger spectra show that Mg segregatesnear grain boundaries as very thin layer. Observation under TEM reveals that a suitableamount of Mg enhances the ability of cooperative internal deformation so that the disloca-tions will ease the continuous slip deformation through grain boundaries. The fracture featureof Fe_3Al alloy is of transgranular cleavage at room temperature and cracks initiate at grainboundaries.
|
|
Received: 18 May 1993
|
1 McKamey C G, Horton J A, Liu C T. Scr Metall, 1988; 22: 1679 2 Culbertson G C, Kortovich C S. TRW AD-A168578/3/WMS, 1986 3 北京钢铁学院,冶金工业部钢铁研究总院,抚顺钢厂.见:徐志超,马培立主编,高温合金中微量元素的作用与控制,北京:冶金工业出版社,1987:3 4 Stoloff N S, Fuchs G E, Kurrvilla A K, Choe S J. In: Stoloff N S, Koch C C, Liu C T, Izumi O eds., High-Temperature Ordered Intermetallic Alloys, Vol. 81, Pittsburgh P A: MRS, 1987: 251 5 马培立,庄景云,朱静,杨锦炎,仲增墉,高良,朱金元,浦惠康.见:徐志超,马培立主编,高温合金中微量元素的作用与控制.北京:冶金工业出版社,1987:72q |