| INFLUENCE OF Nb ON STRUCTURE AND PROPERTIES OF MELT-QUENCHED Fe_(70)Cr18Mo_2B_9Si_1 ALLOY |
| HU Jian;LIN Yijian;XU Jialong;ZHANG Shixun Shanghai Iron and Steel Research Institute Guangzhou UniversityDepartment of Applted Basic Research; Shanghai Iron and Steel Research Institute; Shanghai 200940 |
|
Cite this article:
HU Jian;LIN Yijian;XU Jialong;ZHANG Shixun Shanghai Iron and Steel Research Institute Guangzhou UniversityDepartment of Applted Basic Research; Shanghai Iron and Steel Research Institute; Shanghai 200940. INFLUENCE OF Nb ON STRUCTURE AND PROPERTIES OF MELT-QUENCHED Fe_(70)Cr18Mo_2B_9Si_1 ALLOY. Acta Metall Sin, 1993, 29(7): 85-88.
|
|
|
Abstract An investigation was made of the structure and microhardness variation formelt-quenched Fe_(70)Cr_(18)Mo_2B_9Si_1 alloy, in comparison with Fe_(68.5)Cr_(18)Mo_2B_9Si_1Nb_(1.5), afterannealing under various temperatures. The effect of Nb on grain size of α-Fe matrix and thechemical composition, lattice parameters, nucleation and growth rate of M_2B andM_3B_2 borides phases have been analysed. It was observed that Nb may promote thenucleation of M_3B_2 and reduce the growth rate of M_2B and M_3B_2.
|
|
Received: 18 July 1993
|
1 Ray R, Panchanathan V, Isserow S, J Met, 1983; (3516) : 30. 2 林一坚,尤云龙,张小岷,井春永,严守平,章靖国,金属学报1987;23:A346. 3 胡坚,上海钢铁研究所硕士论文,1987. 4 Lin Yijian, Hu Jian, J Mater Sci, 1991; 26: 2833 5 林一坚,尤云龙,井春永,郁泉琴,金属学报,1991;27:B96. |
| No Suggested Reading articles found! |
|
|