| PREPARATION OF NANOCRYSTALLINE Ti BY BALL MILLING |
| WANG Kaiyang;SHEN Tongde;WANG Jingtang;QUAN Mingxiu State Key Laboratory of RSA; Institute of Metal Research; Academia Sinica; ShenyangUniversity of Science and Technology Beijing; Beijing 100083 |
|
Cite this article:
WANG Kaiyang;SHEN Tongde;WANG Jingtang;QUAN Mingxiu State Key Laboratory of RSA; Institute of Metal Research; Academia Sinica; ShenyangUniversity of Science and Technology Beijing; Beijing 100083. PREPARATION OF NANOCRYSTALLINE Ti BY BALL MILLING. Acta Metall Sin, 1993, 29(7): 89-91.
|
|
|
Abstract Average grain size of crystalline Ti powder may be yielded down to 12-13 nmafter 24 h milling. Its oxygen and nitrogen contents are very low. Relationship betweenhardness and grain size seems to be followed the usual Hall-Petch relationship.
|
|
Received: 18 July 1993
|
1 Gleiter H, Marquardt P, Z Metallk, 1984; 75: 263 2 Cokshi A H, Rosen A, Karch J, Gleiter H, Script Metall, 1989; 23: 1679 3 Nieman, G W, Weertman J R, Siegel R W, Script Metall, 1989; 23: 1679 4 Fecht H J, Heestern E, Fu Z, Johnson W L, Metall Trans, 1990; 21A: 2333 5 Jang J S C, Koch C C, Script Metall Mater. 1990; 24: 1599 6 Hellstern E, Fecht H J, Fu Z, Johnson W L, J Appl Phys, 1989; 45: 305 7 Jang J S C, Koch C C, J Mater Res 1990; 5: 498 8 Williamson G K, Hall W H, Acta Metall, 1953; 1: 22 9 Enzo S, Sampoli M, Cocco G, Schiffini L, Battezzati L, Phil Mag B. 1989; 59: 169 |
| No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|