| THERMODYNAMICS AND PHASE EQUILIBRIUM OF Cu-Ce-O, Cu-Ce-S, Cu-Ce-O-S LIQUID SOLUTIONS |
| DU Ting;LI Guodong Central Iron and Steel Research Institute; Ministry of Metallurgical Industry; BeijingCentral Iron and Steel Research Institute; Ministry of Metallurgical Industry; Beijing 100081 |
|
Cite this article:
DU Ting;LI Guodong Central Iron and Steel Research Institute; Ministry of Metallurgical Industry; BeijingCentral Iron and Steel Research Institute; Ministry of Metallurgical Industry; Beijing 100081. THERMODYNAMICS AND PHASE EQUILIBRIUM OF Cu-Ce-O, Cu-Ce-S, Cu-Ce-O-S LIQUID SOLUTIONS. Acta Metall Sin, 1993, 29(7): 78-84.
|
|
|
Abstract Thermodynamics of Cu-Ce-O, Cu-Ce-S and Cu-Ce-O-S solutions at1200℃ were studied by using solid electrolyte cell and chemical equilibrium method.The equilibrium constants of deoxidation, desulfurization and deoxysulfurization by Ce,the Gibbs standard free energies of the formation of Ce_2O_3, CeS, Ce_2O_2S in Cu-basesolution, activity interaction coefficients of S and Ce, temperature dependence of stand-ard free energy of solution of Ce in Cu and the self-interaction coefficients of Ce in liq-uid Cu have been obtained. The phase precipitation diagram for Cu-Ce-S-O systemhas been plotted. The steady thermodynamic condition of the existence of Ce_2O_3, CeSand Ce_2O_2S in liquid Cu has been determined.
|
|
Received: 18 July 1993
|
1 杜挺,科学通报,1963;7:13 2 陈新民主编,火法冶金物理化学.北京:冶金工业出版社,1984 3 王龙妹,杜挺,钢铁,1985;20:9 4 王龙妹,杜挺,金属学报 1985;21:A249 5 王龙妹,杜挺,金属学报,1987;23:B283 6 李国栋,杜挺,金属学报,1991;27:B286 7 Niemelae J, Taskinen P. Scan J Metall, 1984; 25: 291 8 Sigworth G K, Elliott J F. Can Metall Q, 1974; 13: 455 9 Turkdogan E T. Physical Chemistry of High Temperature Technology, New York: Academic Press, 1980: 24 |
| No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|