| FORMATION MECHANISM FOR NANOCRYSTALLINE FROM AMORPHOUS Fe_(85)Zr_9B_6 AND Fe_(84)Zr_9B_6Cu_1 ALLOYS |
| LING Gang; JI Yu; HU Xiao jun; WU Qiulin; CHU Wei; YANG Guobin; WANG Run (University of Science & Technology Beijing; Beijing 100083) (Shougang Metallurgical Research Institute; Beijing 100085) (Manuscript received 1994-11-25; in revised form 1995-04-03) |
|
Cite this article:
LING Gang; JI Yu; HU Xiao jun; WU Qiulin; CHU Wei; YANG Guobin; WANG Run (University of Science & Technology Beijing; Beijing 100083) (Shougang Metallurgical Research Institute; Beijing 100085) (Manuscript received 1994-11-25; in revised form 1995-04-03). FORMATION MECHANISM FOR NANOCRYSTALLINE FROM AMORPHOUS Fe_(85)Zr_9B_6 AND Fe_(84)Zr_9B_6Cu_1 ALLOYS. Acta Metall Sin, 1995, 31(20): 353-359.
|
|
|
Abstract The microstructure changes in the nanocrystalline soft magnetic material of FeZrB(Cu) alloys with different temperatures of heat treatment and dynamic heating-up processes have been investigated by using TEM and EDAX. It has been found that there appears appreciable phase separation before crystallization. In amorphous phase there are Zr-rich and Fe-rich regions. The Zr-rich phase has a very important effect on precipitation and stability of bcc Fe phase, and the obvious precipitation of α-Zr phase indictates the beginning of instable growth for bcc Fe phase. It has been confirmed that the phase separation of FeZrB(Cu) alloys is a spinodal decomposition process. Correspondent. LING Gang, postdoctor, Box 61, Beijing Agricultural Engineering University, Beijing 100083
|
|
|
| 1SuzukiK,MakinoA,KataokaN,InoueA,MasumotaT.MaterTransJIM.1991:32:932YoshizawaY,Ogumas,YamauchiK.JApplPhys,1988;64:60443涂国超,张家骥,季雨,史长利.金属学报,1991;27:B2144BudurovS,SpassovT,StephaniG,RothS,ReiboldM.MaterSciEng,1988;97:3615KataokaN,InoueA,MasumotiT,YashizawaY,YamauchiK.JpnJApplPhys,1989;28:L18206吉克仁,山内清隆.日本金属学会志,1989;53:2417SuzukiK,KikuchiM,MakinoA,InoueA,MasumotoT.MaterTrunsJIM,1991:32:961 8胡小军,凌刚等.物理学报,待发表工作,1995 9冯端.金属物理(第一卷).北京:科学出版社,1987:2210凌刚.北京科技大学博士学位论文.1994:5511肖纪美.合金相与相变.北京:冶金工业出版社,1987:52 |
| No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|