| STUDY ON MULTIPLE-LAYER STRUCTURE OF PASSIVE FILM ON STAINLESS STEEL BY POTENTIOSTATIC-GALVANOSTATIC TRANSIENT TECHNIQUE III. Stability of Passive Film on 2205 and 316L Stainless Steels in NaCl Media |
| TANG Zilong; SONG Shizhe(Tian jin University; Tian jin 300072).KANG Cuirong(Analysis Center; Tianjin Universitry; Tianjin 300072)(Manuscript received 1994-09-19; in revised form 1995-02-23) |
|
Cite this article:
TANG Zilong; SONG Shizhe(Tian jin University; Tian jin 300072).KANG Cuirong(Analysis Center; Tianjin Universitry; Tianjin 300072)(Manuscript received 1994-09-19; in revised form 1995-02-23). STUDY ON MULTIPLE-LAYER STRUCTURE OF PASSIVE FILM ON STAINLESS STEEL BY POTENTIOSTATIC-GALVANOSTATIC TRANSIENT TECHNIQUE III. Stability of Passive Film on 2205 and 316L Stainless Steels in NaCl Media. Acta Metall Sin, 1995, 31(20): 360-367.
|
|
|
Abstract Structure and stability of the passive films on 2205 and 316L stainless steels in the NaCl solution media, 0.5 and 1.0 mol/L, were studied by using the potentiostatic-galvanostatic (P-G) transient technique. A multiple layer structure of the passive films is revealed on both steels. The action model and breakdown mechanism were suggested on the discussion of the Cl- behaviour against growth and breakdown of the passive films on the steels.The polarized potential dependence on the electrochemical parameters may be determined by P-G response curves. The corrosion resistance to NaCl media of 2205 diphase steel is much superior to that of 316L steel. Furthermore. A preliminary discussion of effect of metallographical structure of 2205 diphase steel on the stability and pitting resistance of passive film was made.Correspondent: SONG Shizhe, professor, Department of Materials Science and Engineering, Tianjin University, Tianjin, 300072
|
|
|
| 1SedriksAJ.Corrosion,1989:45:5102SriramR.TromansD.Corrosion,1989:45:8043SugimotoK,MatsudaS.JElectrochemSoc,1983:130:23234唐子龙,宋诗哲.中国腐蚀与防护学报,1993;341:135MatsudaS,SugimotoS,SawadaS.In:FrankenthalR,KrugerJeds.PassivityofMetals.Princeton:ElectrochemicalSocietyINC,1978:6996OkamotoG.CorrosSci,1973:13:4717宋诗哲,唐子龙.金属学报,1995;31:B678SongZilong,SongShizhe.CorrosSci,1993;1607:349SongShizhe,CaoChunan.CorrosSci,1990;31:64910冈毅民.中国不锈钢腐蚀手册.北京:冶金工业出版社,1992:655 |
| No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|