| A MICROSTRUCTURAL EVOLUTION OF Ag-Cu NANOCRYSTALLINE ALLOYS |
| PING Dehai;QIN Hiaoying;LI Douxing;ZHANG Lide;YE Hengqiang(Laboratory of Atomic Imaging of Solids;Institute of Metal Research;Chinese Academy of Sciences;Shenyang 110015)(Institute of Solid State Physics;Chinese Academy of Sciences;Hefei 230031)(Institute of Metal Research;Chinese Academy of Sciences;Shenyang 110015)(Manuscript received 1995-12-25) |
|
Cite this article:
PING Dehai;QIN Hiaoying;LI Douxing;ZHANG Lide;YE Hengqiang(Laboratory of Atomic Imaging of Solids;Institute of Metal Research;Chinese Academy of Sciences;Shenyang 110015)(Institute of Solid State Physics;Chinese Academy of Sciences;Hefei 230031)(Institute of Metal Research;Chinese Academy of Sciences;Shenyang 110015)(Manuscript received 1995-12-25). A MICROSTRUCTURAL EVOLUTION OF Ag-Cu NANOCRYSTALLINE ALLOYS. Acta Metall Sin, 1996, 32(10): 1087-1092.
|
|
|
Abstract A detailed microstructure analysis of Ag1-xCux(0.05≤x≤0.40) nanocrystalline alloys synthesized by an inert gas condensation method was reported.Results show that homogeneous Ag-Cu nanocrystalline alloys can be prepared, and the grains of the two components are about equal in size,no preferred orientation is detectable.However,for larger Cu pontents up to 40%(atomic fraction),the segregation of Cu particles was observed in some of the samples.No appreciable Ag-Cu metastable phase was detected by electron diffraction technique and HREM observation,only a two-phase equilibrium structure was observed.
|
|
Received: 18 October 1996
|
| 1WunderlichW,IshidaY,MaurerR.ScrMetallMater,1990;24:4032SiegelRW,ThomasGJ.Ultramicroscopy,1992;40:3763LiDX,PingDH,YeHQ,QinXY,WuXJ.MaterLett,1993;18:294BirringerR,GleiterH,KleinHP,MarquardtP.physLett,1984;102A:3655GanapathiSK,RigneyDA.ScrMetallMater.1990;24:16756KizukaT,NakagamiY,OhataT,KanazawaI,IchinoseH,MurakamiH,IshidaY.philosMag,1994;69A:5517SiegelRW,RamasamyS,HahuH,LiZQ,LuT,GronskyR.JMaterRes,1988;3:13678HerrU,JingJ,GonserH,GleiterH.SolidStateCommun,1990;76:1979GleiterH.ProgMaterSci,1989;33:22310DuwezP,WillensRH,KlementWJr.,ApplPhys,1960;31:113611UenishiK,KobayashiKF,IshiharaKN,ShinguPH.MaterSciEng,1991,134A:134212PingDH,LiDX,YeHQ.JMaterSciLett,1995;14:153613BirringerR,HerrU,GleiterH.TransJpnInstMet,1986;27:43p |
| No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|