| RELATIONSHIPS BETWEEN SMELTING REDUCTION RATE AND SLAG STRUCTURE FOR VANADIUM-TITANIUM-CONTAINING MAG NETITE |
| LIU Qingcai(Chongqing University;Chongqing 630044)(Department of Metallurgy and Materials Engineering;Chongqing University;Chongqing 630044)(Manuscript received 1995-12-11;in revised form 1996-06-14) |
|
Cite this article:
LIU Qingcai(Chongqing University;Chongqing 630044)(Department of Metallurgy and Materials Engineering;Chongqing University;Chongqing 630044)(Manuscript received 1995-12-11;in revised form 1996-06-14). RELATIONSHIPS BETWEEN SMELTING REDUCTION RATE AND SLAG STRUCTURE FOR VANADIUM-TITANIUM-CONTAINING MAG NETITE. Acta Metall Sin, 1996, 32(10): 1081-1086.
|
|
|
Abstract The slag structure and mechanism of multipeaks in reduction rate during smelting reduction of V-Ti containing magnetite were systematically analysed.There are three peaks of reduction rate without iron bath and two peaks with iron bath.The first peak is formed by reduction of magnetite,the second peak by reduction of ferric oxides to iron and the third mainly by reduction of titanium oxide to metallic titanium or TiC and TiN.
|
|
Received: 18 October 1996
|
| 1刘清才、裴鹤年.重庆大学学报,1994;17(5):942王宏民、盛世雄.钢铁钒钛,1980;1(4):43张丙怀,刘清才.重庆大学学报,1988;11(13):134ZhangB,LiuQ,LiC,ZouD,SunJ.ActaMetallSin(EnglLett),1993;6B:3995刘清才、张丙怀,邹德余,涂敏.钢铁钒钛.1990;11(3):24Z |
| No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|