Enhancement of Microstructure and Mechanical Property of AlSi10Mg-Er-Zr Alloys Fabricated by Selective Laser Melting |
YANG Tianye, CUI Li( ), HE Dingyong, HUANG Hui |
Faculty of Materials and Manufacturing, Beijing University of Technology, Beijing 100124, China |
|
Cite this article:
YANG Tianye, CUI Li, HE Dingyong, HUANG Hui. Enhancement of Microstructure and Mechanical Property of AlSi10Mg-Er-Zr Alloys Fabricated by Selective Laser Melting. Acta Metall Sin, 2022, 58(9): 1108-1117.
|
Abstract The AlSi10Mg alloy fabricated using selective laser melting (SLM) has attracted attention because of its excellent quality and properties. However, the mechanical properties of SLM AlSi10Mg alloy cannot meet the requirements of the high strength of aluminum alloys in the aerospace industry. To improve the mechanical properties of SLM AlSi10Mg alloy, AlSi10Mg-Er-Zr powders were prepared using in situ alloying mechanism and gas atomization. The relative density, microstructure, and mechanical properties of SLM AlSi10Mg-Er-Zr alloys have been investigated. The results show that the relative density of AlSi10Mg-Er-Zr alloys fabricated using SLM reaches 99.20%. The SLM AlSi10Mg-Er-Zr alloy has a microhardness value of 156.5 HV. The ultimate tensile strength (UTS) and yield strength (YS) of the SLM AlSi10Mg-Er-Zr alloy can reach 461 and 304 MPa, respectively. Compared with the conventional AlSi10Mg alloy, the microhardness has been increased by 25.8%; the UTS and YS are increased by 22.6% and 26.7%, respectively. The fine-grain and solid solution strengthening associated with SLM processing with the addition of Er and Zr elements, as a result of increased grain size refinement and solid solubility of Si element in the α-Al matrix, are responsible for the improvement in the mechanical properties.
|
Received: 26 February 2021
|
|
Fund: National Natural Science Foundation of China(51621003) |
About author: CUI Li, professor, Tel: 13311267636, E-mail: cuili@bjut.edu.cn
|
1 |
Zhang X J, Tang S Y, Zhao H Y, et al. Research status and key technologies of 3D printing [J]. J. Mater. Eng., 2016, 44(2): 122
|
|
张学军, 唐思熠, 肇恒跃 等. 3D打印技术研究现状和关键技术 [J]. 材料工程, 2016, 44(2): 122
|
2 |
Gong S L, Suo H B, Li H X. Development and application of metal additive manufacturing technology [J]. Aeronaut. Manuf. Technol., 2013, (13): 66
|
|
巩水利, 锁红波, 李怀学. 金属增材制造技术在航空领域的发展与应用 [J]. 航空制造技术, 2013, (13): 66
|
3 |
Zhang S. Research on the forming processes and propertiesin selective laser melting of medical alloy powders [D]. Wuhan: Huazhong University of Science and Technology, 2014
|
|
张 升. 医用合金粉末激光选区熔化成形工艺与性能研究 [D]. 武汉: 华中科技大学, 2014
|
4 |
Chen J T, Guo Z Y, Wang C Y, et al. Research status of Ti-6Al-4V manufactured by selective laser melting for medical device applications [J]. Laser Technol., 2020, 44: 288
|
|
陈锦堂, 郭紫莹, 王成勇 等. 激光选区熔化Ti-6Al-4V在医疗器械领域的研究现状 [J]. 激光技术, 2020, 44: 288
|
5 |
Li X D, Zhao F. 3D printing technology impact on development of industrial design [J]. Key Eng. Mater., 2016, 693: 1901
doi: 10.4028/www.scientific.net/KEM.693.1901
|
6 |
Zhong X H. 3D printing technology applied in the field of racing lightweight [D]. Guangzhou: Guangdong University of Technology, 2019
|
|
钟兴华. 3D打印技术在赛车轻量化领域应用研究 [D]. 广州: 广东工业大学, 2019
|
7 |
Röttger A, Geenen K, Windmann M, et al. Comparison of microstructure and mechanical properties of 316 L austenitic steel processed by selective laser melting with hot-isostatic pressed and cast material [J]. Mater. Sci. Eng., 2016, A678: 365
|
8 |
Zhang W Q, Zhu H H, Hu Z H, et al. Study on the selective laser melting of AlSi10Mg [J]. Acta Metall. Sin., 2017, 53: 918
|
|
张文奇, 朱海红, 胡志恒 等. AlSi10Mg的激光选区熔化成形研究 [J]. 金属学报, 2017, 53: 918
doi: 10.11900/0412.1961.2016.00472
|
9 |
Aboulkhair N T, Simonelli M, Parry L, et al. 3D printing of aluminium alloys: Additive manufacturing of aluminium alloys using selective laser melting [J]. Prog. Mater. Sci., 2019, 106: 100578
doi: 10.1016/j.pmatsci.2019.100578
|
10 |
Kempen K, Thijs L, Van Humbeeck J, et al. Mechanical properties of AlSi10Mg produced by selective laser melting [J]. Phys. Proc., 2012, 39: 439
doi: 10.1016/j.phpro.2012.10.059
|
11 |
Brandl E, Heckenberger U, Holzinger V, et al. Additive manufactured AlSi10Mg samples using selective laser melting (SLM): Microstructure, high cycle fatigue, and fracture behavior [J]. Mater. Des., 2012, 34: 159
doi: 10.1016/j.matdes.2011.07.067
|
12 |
Read N, Wang W, Essa K, et al. Selective laser melting of AlSi10Mg alloy: Process optimisation and mechanical properties development [J]. Mater. Des., 2015, 65: 417
doi: 10.1016/j.matdes.2014.09.044
|
13 |
Jiang L Y, Liu T T, Zhang C D, et al. Preparation and mechanical properties of CNTs-AlSi10Mg composite fabricated via selective laser melting [J]. Mater. Sci. Eng., 2018, A734: 171
|
14 |
Zhao Z Y, Bai P K, Misra R D K, et al. AlSi10Mg alloy nanocomposites reinforced with aluminum-coated graphene: Selective laser melting, interfacial microstructure and property analysis [J]. J. Alloys Compd., 2019, 792: 203
doi: 10.1016/j.jallcom.2019.04.007
|
15 |
Xi L X, Gu D D, Guo S, et al. Grain refinement in laser manufactured Al-based composites with TiB2 ceramic [J]. J. Mater. Res. Technol., 2020, 9: 2611
doi: 10.1016/j.jmrt.2020.04.059
|
16 |
Xiao Y K, Bian Z Y, Wu Y, et al. Effect of nano-TiB2 particles on the anisotropy in an AlSi10Mg alloy processed by selective laser melting [J]. J. Alloys Compd., 2019, 798: 644
doi: 10.1016/j.jallcom.2019.05.279
|
17 |
Li X P, Ji G, Chen Z, et al. Selective laser melting of nano-TiB2 decorated AlSi10Mg alloy with high fracture strength and ductility [J]. Acta Mater., 2017, 129: 183
doi: 10.1016/j.actamat.2017.02.062
|
18 |
Wang H Q, Gu D D. Nanometric TiC reinforced AlSi10Mg nanocomposites: Powder preparation by high-energy ball milling and consolidation by selective laser melting [J]. J. Compos. Mater., 2015, 49: 1639
doi: 10.1177/0021998314538870
|
19 |
Gao C, Wang Z, Xiao Z, et al. Selective laser melting of TiN nanoparticle-reinforced AlSi10Mg composite: Microstructural, interfacial, and mechanical properties [J]. J. Mater. Process. Technol., 2020, 281: 116618
doi: 10.1016/j.jmatprotec.2020.116618
|
20 |
Gao C, Wu W, Shi J, et al. Simultaneous enhancement of strength, ductility, and hardness of TiN/AlSi10Mg nanocomposites via selective laser melting [J]. Addit. Manuf., 2020, 34: 101378
|
21 |
Ye H, Huang J Q, Zhang J Q, et al. Microstructure and mechanical properties of nano-WC reinforced AlSi10Mg fabricated by selective laser melting [J]. J. Mater. Eng., 2020, 48(3): 75
|
|
叶 寒, 黄俊强, 张坚强 等. 纳米WC增强选区激光熔化AlSi10Mg显微组织与力学性能 [J]. 材料工程, 2020, 48(3): 75
|
22 |
Xue G, Ke L D, Zhu H H, et al. Influence of processing parameters on selective laser melted SiCp/AlSi10Mg composites: Densification, microstructure and mechanical properties [J]. Mater. Sci. Eng., 2019, A764: 138155
|
23 |
Zhao X, Gu D D, Ma C L, et al. Microstructure characteristics and its formation mechanism of selective laser melting SiC reinforced Al-based composites [J]. Vacuum, 2019, 160: 189
doi: 10.1016/j.vacuum.2018.11.022
|
24 |
Spierings A B, Dawson K, Dumitraschkewitz P, et al. Microstructure characterization of SLM-processed Al-Mg-Sc-Zr alloy in the heat treated and HIPed condition [J]. Addit. Manuf., 2018, 20: 173
|
25 |
Nie Z R, Wen S P, Huang H, et al. Research progress of Er-containing aluminum alloy [J]. Chin. J. Nonferrous Met., 2011, 21: 2361
|
|
聂祚仁, 文胜平, 黄 晖 等. 铒微合金化铝合金的研究进展 [J]. 中国有色金属学报, 2011, 21: 2361
|
26 |
Feng Q N. Research on process, microstructures and properties of AlSi10Mg aluminum alloy prepared by laser melting deposition [D]. Nanjing: Nanjing University of Aeronautics and Astronautics, 2017
|
|
冯秋娜. 激光熔化沉积成形AlSi10Mg合金的工艺与组织性能研究 [D]. 南京: 南京航空航天大学, 2017
|
27 |
Aboulkhair N T, Maskery I, Tuck C, et al. The microstructure and mechanical properties of selectively laser melted AlSi10Mg: The effect of a conventional T6-like heat treatment [J]. Mater. Sci. Eng., 2016, A667: 139
|
28 |
Xing Z B, Nie Z R, Zou J X, et al. Existing form and effect of erbium in Al-Er alloy [J]. J. Chin. Rare Earth Soc., 2007, 25: 234
|
|
邢泽炳, 聂祚仁, 邹景霞 等. Al-Er合金铸锭中铒的存在形式及作用研究 [J]. 中国稀土学报, 2007, 25: 234
|
29 |
Loucif A, Figueiredo R B, Baudin T, et al. Ultrafine grains and the Hall-Petch relationship in an Al-Mg-Si alloy processed by high-pressure torsion [J]. Mater. Sci. Eng., 2012, A532: 139
|
30 |
Wu B L, Song L H, Wan G, et al. Distribution of generalized schmid factor in Euler orientation space and rollability of AZ31B alloy with basal texture [J]. J. Mater. Eng. Perform., 2020, 29: 8145
doi: 10.1007/s11665-020-05279-7
|
31 |
Yan H L. Mechanical behavior and texture evolution of low stacking fault energy FCC metals at large deformation [D]. Shenyang: Northeastern University, 2012
|
|
闫海乐. 大形变下低层错能面心立方金属力学行为和织构演化的研究 [D]. 沈阳: 东北大学, 2012
|
No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
|
Shared |
|
|
|
|
|
Discussed |
|
|
|
|