| INVESTIGATION OF DYNAMIC MECHANICAL BEHAVIOR OF A NEW Zr-Ti ALLOY |
| WANG Jie, ZHANG Hongwei, WANG Aimin, LI Hong, FU Huameng, ZHU Zhengwang,ZHANG Haifeng |
| Shenyang National Laboratory for Materials Science, Institute of Metal Research,Chinese Academy of Sciences,Shenyang 110016 |
|
Cite this article:
WANG Jie, ZHANG Hongwei, WANG Aimin, LI Hong, FU Huameng, ZHU Zhengwang,ZHANG Haifeng. INVESTIGATION OF DYNAMIC MECHANICAL BEHAVIOR OF A NEW Zr-Ti ALLOY. Acta Metall Sin, 2012, 48(5): 636-640.
|
|
|
Abstract Zirconium based alloy is a new type structural material with high specific strength and good comprehensive properties. In this article, quasi-static compression at room temperature and dynamic compression under various temperatures were performed to a new zirconium-titanium alloy. It was found that this alloy showed good strength and plasticity, and the strength increased and plasticity decreased with increasing strain rate or decreasing temperature. A constitutive model under dynamic compression was established based on Johnson-Cook model, and accorded well with experimental results.
|
|
Received: 28 December 2011
|
| [1] Tribble A. The Space Environment-Implications for Spacecraft Design. Princeton: Princeton University Press, 1995: 1[2] Lowenstein D I, Rusek A. Radiat Environ Biophys, 2007; 46: 91[3] Nikiforov A, Chumakov A. In: Daglis I A ed., Effects of Space Weather on Technology Infrastructure. Dordrecht: Kluwer Academic Publishers, 2004: 165[4] Shilobreeva S N, Kashkarov L L, Barabanenkov M Y, Pustovit A N,Zinenko V I, Agafonov Y A. Doklady Earth Sci, 2006; 411: 9[5] Wicklein M, Ryan S, White D M, Clegg R A. Int J Impact Eng,2008; 35: 1861[6] Sakuraba K, Tsuruda Y, Hanada T, Liou J C, Akahoshi Y. Int J Impact Eng, 2008; 35: 1567[7] Sorensen B R, Kimsey K D, Love B M. Int Impact Eng, 2008; 35: 1808[8] Zhao W J. Rare Met Lett, 2004; 23(5): 15 (赵文金. 稀有金属快报, 2004; 23(5): 15)[9] Liu J Z. Nuclear Structural Materials. Beijing: Chemical Industry Press, 2007: 5 (刘建章. 核结构材料, 北京: 化学工业出版社, 2007: 5)[10] Zhao W J, Zhou B X, Miao Z, Peng Q, Jiang Y R, Jiang H M, Pang H. Atom Energy Sci Technol, 2005; 39(suppl): 2 (赵文金, 周邦新, 苗志, 彭倩, 蒋有荣, 蒋宏曼, 庞华.原子能科学技术, 2005; 39(增刊): 2)[11] Wang R S, Weng L K, Zhang Y W, Geng J Q, Wang J H. Mater Rev,2011; 25(13): 105 (王荣山, 翁立奎, 张晏玮, 耿建桥, 王锦红. 材料导报, 2011; 25(13): 105)[12] Zhang J, Wang G P, Zuo X T. J Netshape Forming Eng, 2011; (5); 35 (张建, 王国平, 左小涛. 精密成形工程, 2011; (5); 35)[13] Liu W Q, Zhu X Y, Wang X J, Li Q, Yao M Y, Zhou B X. Atom Energy Sci Technol, 2010; 44: 1477 (刘文庆, 朱晓勇, 王晓姣, 李强, 姚美意, 周邦新. 原子能科学技术,2010; 44: 1477)[14] Peker A, Johnson W L. Appl Phys Lett, 1993; 63: 2342[15] Inoue A, Zhang T, Saida J, Matsushita M, Chen M W, Sakurai T. Mater Trans JIM, 1999; 40: 1137[16] Bruck H A, Christman T, Rosakis A J, Johnson W L. Scr Metall Mater,1994; 30: 429[17] Inoue A. Acta Mater, 2000; 48: 279[18] Liang S X, Ma M Z, Jing R, Zhang X Y, Liu R P. Mater Sci Eng,2012; A532: 1[19] Cui Z Q, Tan Y C. Metallography and Heat Treatment.Beijing: Mechanical Industry Press, 2007: 186 (崔忠圻, 覃耀春. 金属学与热处理. 北京: 机械工业出版社, 2007: 186)[20] Gao L Q, Zhu J H, Li H, Sun J K. Rare Met Mater Eng, 2008; 37: 1051 (高灵清, 朱金华, 李慧, 孙建科. 稀有金属材料与工程, 2008; 37: 1051)[21] Chang L Z, Pan Y T, Zhang Z M, Xue Y. Ordnance Mater Sci Eng,2010; 33(4): 68 (常列珍, 潘玉田, 张治民, 薛勇. 兵器材料科学与工程, 2010; 33(4): 68)[22] Johnson G R, Cook W H. Proc 7th Int Symp on Ballistics,Hague, Netherlands, 1983: 541[23] Johnson G R, Cook W H. Eng Fract Mech, 1985; 21: 31 |