| EFFECT OF Nb ON THE CORROSION RESISTANCE OF Zr-4 ALLOY IN SUPERHEATED STEAM AT 500 ℃ |
| YAO Meiyi, LI Shilu, ZHANG Xin, PENG Jianchao, ZHOU Bangxin, ZHAO Xushan, SHEN Jianyun |
1) Institute of Materials, Shanghai University, Shanghai 200072
2) Laboratory for Microstructures, Shanghai University, Shanghai 200444
3) General Research Institute for Nonferrous Metal, Beijing 100088 |
|
Cite this article:
YAO Meiyi LI Shilu ZHANG Xin PENG Jianchao ZHOU Bangxin ZHAO Xushan SHEN Jianyun. EFFECT OF Nb ON THE CORROSION RESISTANCE OF Zr-4 ALLOY IN SUPERHEATED STEAM AT 500 ℃. Acta Metall Sin, 2011, 47(7): 865-871.
|
|
|
Abstract The corrosion resistance of Zr-4+xNb alloys (x=0.1-0.3, mass fraction, %) was investigated in a superheated steam at 500 ℃ and 10.3 MPa by autoclave tests. The microstructure of the alloys and fracture surface morphology of the oxide film formed on the alloys were observed by TEM and SEM, respectively. Results show that no nodular corrosion appears on Zr-4+xNb alloys in 500 ℃/10.3 MPa superheated steam even for 500 h, which is related to the higher Nb concentration dissolved in α-Zr matrix. The Nb dissolved in α-Zr matrix can restrain the nucleation of nodular corrosion, thus improve the nodular corrosion resistance. The uniform corrosion resistance of Z-4+xNb alloys is lowered with the increase of Nb content, which is related to the decrease of the solid solution concentration of (Fe+Cr) in α-Zr matrix and the precipitation of the second phase particles of Zr(Fe, Cr, Nb)2, and the two aspects will accelerate the microstructural evolution of the oxide film during corrosion process to promote the formation of pores and micro-cracks.
|
|
Received: 03 March 2011
|
| Fund: Supported by National Natural Science Foundation of China (Nos.50871064 and 50971084), High Technology Research and Development Program of China (No.2008AA031701), Natural Science Foundation of Shanghai (No.09ZR1411700) and Shanghai Leading Academic Discipline Project (No.S30107) |
| [1] Liu J Z. Nuclear Structural Materials. Beijing: Chemical Industry Press, 2007: 112(刘建章. 核结构材料. 北京: 化学工业出版社, 2007: 112)[2] Ogata K. In: Van Swam L F P, Eucken C M, eds., Zirconium in the Nuclear Industry: 8th International Symposium, ASTM STP 1023, San Diego, CA: ASTM International, 1988: 346[3] Zhou B X, Li Q, Yao M Y, Xia S, Liu W Q, Chu Y L. Rare Met Mater Eng, 2007; 36: 1129(周邦新, 李强, 姚美意, 夏爽, 刘文庆, 禇于良. 稀有金属材料与工程, 2007; 36: 1129)[4] Zhou B X, Zhao W J, Miao Z, Huang D C, Jiang Y R. In: Zhou B X, Shi Y K, eds., Proc III–2 China Nuclear Materials Academic Conference in 1996, Beijing: Chemical Industry Press, 1997: 183(周邦新, 赵文金, 苗志, 黄德诚, 蒋有荣 著; 周邦新, 石永康主编, 96中国核材料研讨会论文集III-2,北京: 化学工业出版社, 1997: 183)[5] Zhou B X, Yao M Y, Li Q, Xia S, Liu W Q, Chu Y L. Rare Met Mater Eng, 2007; 36: 1317(周邦新, 姚美意, 李 强, 夏 爽, 刘文庆, 禇于良. 稀有金属材料与工程, 2007; 36: 1317)[6] Yao M Y, Zhou B X, Li Q, Xia S, Liu W Q. Shanghai Met, 2008; 30: 1(姚美意, 周邦新, 李强, 夏 爽, 刘文庆. 上海金属, 2008; 30: 1)[7] Zhou B X, Li Q, Yao M Y, Liu W Q. Nucl Power Eng, 2005; 26: 364(周邦新, 李 强, 姚美意, 刘文庆. 核动力工程, 2005; 26: 364)[8] Toffolon–Masclet C, Brachet J C, Jago G. J Nucl Mater, 2002; 305: 224[9] Yang W D. Reactor Materials Science. 2nd Ed., Beijing: Atomic Energy Press, 2006: 260(杨文斗. 反应堆材料学. 第二版. 北京: 原子能出版社, 2006: 260)[10] Zhou B X, Li Q, Yao M Y, Liu W Q, Chu Y L. In: Kammenzind B, Limb¨ack M, eds., Zirconium in the Nuclear Industry: 15th International Symposium, ASTM STP 1505, Sunriver, Oregon, USA: ASTM International, 2009: 360[11] Anada H, Takeda K. In: Bradley E R, Sabol G P, eds., Zirconium in the Nuclear Industry: 11th International Symposium, ASTM STP 1295, Garmisch–Partenkirchen, Germany: ASTM International, 1996: 35[12] Kim H G, Jeong Y H, Kim T H. J Nucl Mater, 2004; 326: 125[13] Jeong Y H, Kim H G, Kim D J, Choi B K, Kim J H. J Nucl Mater, 2003; 323: 72[14] Jeong Y H, Kim H G, Kim T H. J Nucl Mater, 2003; 317: 1[15] Hao S M. Thermodynamics of Materials. Beijing: Chemical Industry Press, 2004: 333(郝士明. 材料热力学. 北京: 化学工业出版社, 2004: 333)[16] Charquet D. J Nucl Mater, 2001; 288: 237[17] Li T F. High Temperature Oxidation and Thermal Corrosion of Metals. Beijing: Chemical Industry Press, 2003: 52(李铁藩. 金属高温氧化和热腐蚀. 北京: 化学工业出版社, 2003: 52)[18] Bangaru N V. J Nucl Mater, 1985; 131: 280[19] Zhou B X, Peng J C, Yao M Y, Li Q, Xia S, Du C X, Xu G. J ASTM Int, 8(1), Paper ID JAI102951, www.astm.org.[20] Zhou B X. In: Van Swam L F P, Eucken C M, eds., Zirconium in the Nuclear Industry: 8th International Symposium, ASTM STP 1023, San Diego, CA: ASTM International, 1988: 360[21] Zhou B X, Yao M Y, Xia S, Liu W Q. J Shanghai Univ (Nat Sci Ed), 2008; 14: 441(周邦新, 姚美意, 李 强, 夏 爽, 刘文庆. 上海大学学报(自然科学版), 2008; 14: 441) |
| No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|