| INFLUENCES OF ULTRASONIC PULSE SQUARE-WAVE CURRENT PARAMETERS ON MICROSTRUCTURES AND MECHANICAL PROPERTIES OF 2219 ALUMINUM ALLOY WELD JOINTS |
| CONG Baoqiang; QI Bojin; ZHOU Xingguo; LUO Jun |
| School of Mechanical Engineering and Automation; Beihang University; Beijing 100191 |
|
Cite this article:
CONG Baoqiang QI Bojin ZHOU Xingguo LUO Jun. INFLUENCES OF ULTRASONIC PULSE SQUARE-WAVE CURRENT PARAMETERS ON MICROSTRUCTURES AND MECHANICAL PROPERTIES OF 2219 ALUMINUM ALLOY WELD JOINTS. Acta Metall Sin, 2009, 45(9): 1057-1062.
|
|
|
Abstract In order to overcome some problems in variable polarity gas tungsten arc welding (VP-GTAW) employed for welding aluminum alloy components, poor strength and ductility of weld metal, solidification cracking and weld porosity, a novel ultrafast-convert high frequency pulsed current VP-GTAW technique is developed. The current converting speed in the novel technique is enhanced from less than 10 A/μs to more than 50-100 A/μs and high frequency pulsed current which has a frequency of more than 20 kHz is exactly integrated in the positive polarity current duration. It is expected that the novel pulsed VP-GTAW technique can improve the weld quality of aluminum alloy significantly. Thus, it is imperative to understand the effect of pulsed current parameters on the weld characteristics in the pulsed VP-GTAW process. The measured results of 2219-T87 high strength aluminum alloy weld joints show that the application of ultrasonic pulse current makes the coarse grains in weld zone change to the fine equiaxed grains, and a band-like zone with finer equiaxed non-dentrites appears. The width of weld fusion zone is obviously decreased and the mechanical properties of weld joints are predominantly improved. The improvements of the structure and weld properties can be significantly enhanced with the increases of the ultrasonic pulse current amplitude and pulse frequency, and decrease of the pulse duty cycle in certain ranges. Compared with the conventional VP-GTAW, tensile strength and elongation of weld joints are increased by about 22% and 111%, respectively, under the conditions of pulse current amplitude of 100 A, pulse frequency of 40 kHz and pulse duty cycle of 20%.
|
|
Received: 26 February 2009
|
|
|
| [1] Albertini G, Bruno G, Dunn B D, Fiori F, Reimers W, Wright J S. Mater Sci Eng, 1997; A224: 157
[2] Liu C F. Aeronaut Manufact Technol, 2003; (2): 22
(刘春飞. 航空制造技术, 2003; (2): 22)
[3] Yang C G, Guo X M, Hong Z F, Qian B N. Acta Metall Sin, 2005; 41: 1077
(杨成刚, 国旭明, 洪张飞, 钱百年. 金属学报, 2005; 41: 1077)
[4] Qi B J, Cong B Q. Trans Chin Weld Inst, 2008; 29: 57
(齐铂金, 从保强. 焊接学报, 2008; 29: 57)
[5] Cong B Q, Qi B J, Zhou X G, Luo J. Trans Chin Weld Inst, 2009; 30: 25
(从保强, 齐铂金, 周兴国, 罗 军. 焊接学报, 2009; 30: 25)
[6] Cong B Q, Qi B J, Zhou X G, Luo J. Aerospace Mater Technol, 2009; 39: 71
(从保强, 齐铂金, 周兴国, 罗 军. 宇航材料工艺, 2009; 39: 71)
[7] Cook G E, Eassa E H. IEEE Trans Indust Applic, 1985; 1A–21: 1294
[8] Cong B Q. PhD Thesis, Beihang University, Beijing, 2009
(从保强. 北京航空航天大学博士学位论文, 北京, 2009)
[9] Guo X M, Yang C G, Qian B N, Xu Q, Zhang H Y. Acta Metall Sin, 2005; 41: 397
(国旭明, 杨成刚, 钱百年, 徐强, 张洪延. 金属学报, 2005; 41: 397)
[10] Hunt J D. Mater Sci Eng, 1984; A65: 75
[11] Sun J S, Wu C S. Acta Phys Sin, 2001; 50: 209
(孙俊生, 武传松. 物理学报, 2001; 50: 209)
[12] Kou S, Le Y. Weld J, 1986; 65: 305
[13] Yunjia H, Frost R H, Olson D L, Edwards G R. Weld J, 1989; 68: 280
[14] Kou S, Le Y. Metall Trans, 1988; 19A: 1075
[15] Dvornak M J, Frost R H, Olson D L. Weld J, 1991; 70: 271
[16] Hao C Y, Yu E J, Ying H J, Shi C G. Acta Metall Sin, 1996; 32: 647
(郝传勇, 于尔靖, 应慧筠, 施成根. 金属学报, 1996; 32: 647)
[17] Wang Q, He J C, Kawai S, Iwai K, Asai S. Acta Metall Sin, 2002; 38: 961
(王强, 赫冀成, 川合悟, 岩井一彦, 浅井滋生. 金属学报, 2002; 38: 961)
[18] Yu E J, Hao C Y, Ying H J, Shi C G, Li G H. Trans Chin Weld Inst, 1996; 17: 1
(于尔靖, 郝传勇, 应慧筠, 施成根, 李敢红. 焊接学报, 1996; 17: 1)
[19] Gutierrez A, Lippold J C. Weld J, 1998; 77: 123
[20] Reddy G M, Gokhale A A. J Mater Sci, 1997; 32: 4117
[21] Huang C, Kou S. Weld J, 2000; 79: 113
[22] Huang C, Kou S. Weld J, 2001; 80: 9 |
| No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|