| LASER GLAZING RAPIDLY SOLIDIFIED MICROSTRUCTURE OF DD8 SINGLE CRYSTAL Ni--BASED SUPERALLOY |
| JIN Tao; SUN Xiaofeng; ZHAO Nairen; LIU Jinlai; ZHANG Jinghua; HU Zhuangqi |
| Institute of Metal Research; Chinese Academy of Sciences; Shenyang 110016 |
|
Cite this article:
JIN Tao SUN Xiaofeng ZHAO Nairen LIU Jinlai ZHANG Jinghua HU Zhuangqi. LASER GLAZING RAPIDLY SOLIDIFIED MICROSTRUCTURE OF DD8 SINGLE CRYSTAL Ni--BASED SUPERALLOY. Acta Metall Sin, 2009, 45(6): 711-716.
|
|
|
Abstract The laser glazing rapid solidification can make the dendrite refined and reduce the segregation of alloying elements, so it is very favorable to
mechanical properties of alloys, e.g., the fatigue life of Ni--based superalloy can be prolonged by laser surface melting process due to improved
resistance to stress corrosion cleavage. The laser surface melting process can be used for modification of surface or repair of casting defects (such
as surface porosity, surface stray grains) in single crystal components. Recently, this technique has become an attractive research subject with latent application. A successful laser glazing rapid solidification to single--crystal should ensure the preservation of the single--crystal nature, i.e., the
re--solidified surface layer needs to be epitactic with the substrate. The microstructure after laser re--solidification is closely related to the processing parameters, however, the relationship between microstructure and re--solidification conditions or processing parameters is not well understood
and needs further study. In the present work, the microstructure of laser glazing solidified Ni--based single crystal DD8 was investigated by OM, SEM as well as TEM. The results show that the surface width of the melted pool becomes narrow with an increase of scanning rate, so the melted pool has a relatively high interface/volume ratio which leads to a higher cooling rate. The primary dendrite arm spacing decreases with an increase of cooling rate, and gradually reaches a minimum about only 3 μm, which is two orders of magnitude smaller than that of the untreated part of alloy. EDXA shows that the dendritic segregation is not obvious and the chemical compositions tend to be homogeneous after re--solidification, which is caused by the higher solidification rate and related partition coefficients of alloying elements. The solidified structures are composed of the quasi--plane front, cellular and fine dendrites from substrate to surface of melted pool. The structures in the regions of the quasi--plane front and cellular consist of γ--solid solution and dispersive γ' precipitates with about 20 nm in size. In the regions of the cellular--dendrite and the dendrite, however, there is a eutectic structure with a higher Ti content in the interdendrites. These eutectic structures are small in size and look like leaves. In the transition region, both γ and γ'--phases are not completely melted, and there are some dislocations distributed on the interfaces of the γ'--phase particles induced by thermal stress between γ and γ' phases at higher cooling rate. The unmelted γ' particles can act as nuclei of the second precipitated γ' phases which have a size of about 10 nm and a pile--up--like morphology.
|
|
Received: 09 October 2008
|
|
|
| 1] Marchi C S, Zaleski T, Lee S, Yang N Y C, Stuart B. Scr Mater, 2008; 58: 782
[2] Liu W P, DuPont J N. Acta Mater, 2004; 52: 4833
[3] Liu W P, DuPont J N. Acta Mater, 2005; 53: 1545
[4] Gaumann M, Bezencon C, Canalis P. Acta Mater, 2001;49: 1051
[5] Zhang Y W, Zhang S Q, Wang H M. Rare Met Mater Eng, 2008; 37: 169
(张亚伟, 张述泉, 王华明. 稀有金属材料与工程, 2008; 37: 169)
[6] Wang H M, Tang Y J, Zhang J H. J Aero Mater, 1991;11(1): 12
(王华明, 唐亚俊, 张静华. 航空材料学报, 1991; 11(1): 12)
[7] Wang H M, Zhang J H. Acta Metall Sin, 1991; 27: A403
(王华明, 张静华, 金属学报. 1991; 27: A403)
[8] Zhang J H, Zhang Y S, Zhang Z Y, Xu Y B, Tang Y J, Hu Z Q. Acta Metall Sin, 1983; 19: A309
(张静华, 张玉生, 张志亚, 徐永波, 唐亚俊, 胡壮麒. 金属学报, 1983; 19: A309)
[9] Forget P, Jeandia M, Lyoret A. J Phys IV Fr, 1993; 3: C7–921
[10] Narasimhan S L, Copley S M, van Stryland E W, Basset M. Metall Mater Trans, 1979; 10A: 654
[11] Yang S, Huang W D, Liu W J, Zhong M L, Zhou Y H. Acta Mater, 2002; 50: 315 |
| No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|