| MICROSTRUCTURE REFINEMENT OF EUTECTOID STEEL BASED ON DIVORCED EUTECTOID TRANSFORMATION |
| LI Longfei1; LI Wei1; SUN Zuqing1; YANG Wangyue2 |
1.State Key Laboratory for Advanced Metals and Materials; University of Science \& Technology Beijing; Beijing 100083
2.Materials Science and Engineering School; University of Science \& Technology Beijing; Beijing 100083 |
|
Cite this article:
LI Longfei LI Wei SUN Zuqing YANG Wangyue. MICROSTRUCTURE REFINEMENT OF EUTECTOID STEEL BASED ON DIVORCED EUTECTOID TRANSFORMATION. Acta Metall Sin, 2009, 45(6): 704-710.
|
|
|
Abstract For high carbon steels, the (α+θ) microduplex structure consisting of ultrafine ferrite matrix and dispersed cementite particles demonstrates a good balance between strength and ductility as compared with a normal microstructure, i.e., lamellar pearlite in eutectoid steel or lamellar pearlite plus pro--eutectoid cementite in hypereutectoid steel. The divorced eutectoid transformation (DET) has been confirmed to be very effective in ultrahigh carbon steels for the production of the (α+θ) microduplex structure. In ultrahigh carbon steels, DET takes place during slow cooling of a mixing microstructure of austenite plus dispersed undissolved cementite particles formed by the intercritical annealing within the (γ+θ) two phase range. Due to the absence of the (γ+θ) two phase range, DET is difficult to take place in eutectoid steel. In the present work, DET was realized in eutectoid steel by a special thermal--mechanical treatment, which involved two--stage hot deformation in the temperature ranges of A1 to Ar1 and A1 to Ac1 and subsequent slow cooling. The microstructure evolution during such treatment was studied by hot uniaxial compression tests using a
Gleeble 1500 hot simulation test machine in combination with SEM and EBSD. The results indicate that during hot deformation in the
temperature range of A1 to Ac1 after hot deformation of undercooled austenite in the temperature range of A1 to Ar1 , the re--austenization could be controlled by the applied strain, leading to the formation of the mixing microstructure of austenite plus undissolved cementite particles at certain conditions. During subsequent slow cooling, DET took place, resulting in the formation of an ultrafine (α+θ) microduplex structure with α--Fe
grains less than 3 μm and θ--Fe3C particles less than 0.5 μm.
|
|
Received: 05 December 2008
|
|
|
| [1] Oyama T, Sherby O D, Wadsworth J, Walser B. Scr Metall , 1984; 18: 799
[2] Sherby O D. ISIJ Int, 1999; 39: 637
[3] Sherby O D,Walser B, Young C M, Cady E M. Scr Metall, 1975; 9: 569
[4] Walser B, Sherby O D. Metall Trans, 1979; 10A: 1461
[5] Wadsworth J, Lin J H, Sherby O D. Met Technol, 1981; 8: 190
[6] Sherby O D, Oyama T, Kum D W, Walser B, Wadsworth J. J Met, 1985; 37(6): 50
[7] Syn C K, Lesuer D R, Sherby O D. Metall Mater Trans, 1994; 25A: 1481
[8] Langford G. Metall Trans, 1977; 8A: 861
[9] Fu W, Furuhara T, Maki T. ISIJ Int, 2004; 44: 171
[10] Furuhara T, Mizoguchi T, Maki T. ISIJ Int, 2005; 45: 392
[11] Lupton D F, Warrington D H. Met Sci J, 1972; 6: 200
[12] Kaspar R, Kapellner W, Lang C. Steel Res, 1988; 59: 492
[13] Huang Q S, Li L F, Yang W Y, Sun Z Q. Acta Metall Sin, 2007; 43: 724
(黄青松, 李龙飞, 杨王玥, 孙祖庆. 金属学报, 2007; 43: 724)
[14] Li L F, Yang W Y, Sun Z Q. Metall Mater Trans, 2007; 39A: 624
[15] Chen W, Li L F, Yang W Y, Sun Z Q. Acta Metall Sin, 2009; 45: 151
(陈 \ \ 伟, 李龙飞, 杨王玥, 孙祖庆. 金属学报, 2009; 45: 151)
[16] Xu P G, Tomota Y. Acta Metall Sin, 2006; 42: 681
(徐平光, 友田阳. 金属学报, 2006; 42: 681)
[17] Honda K, Saito S. J Iron Steel Inst, 1920; 102: 261
[18] Whiteley J H. J Iron Steel Inst, 1922; 105: 339
[19] Payson P, Hodapp W L, Leeder J. Trans ASM, 1940; 28:306
[20] Grossmann M A, Bain E C. Principles of Heat Treatment. 5th ed., Ohio: American Society for Metals, 1964: 201
[21] Cullen O E. Met Prog, 1953; 64: 79
[22] Parusov V V, Dolzhenkov I I, Sukhomlin V I. Met Sci Heat Treatment, 1985; 27: 402
[23] Verhoeven J D, Gibson E D. Metall Mater Trans, 1998; 29A: 1181
[24] Sun Z Q, Yang W Y, Qi J J, Hu A M. Mater Sci Eng, 2002; A334: 201
[25] Yang W Y, Qi J J, Sun Z Q, Yang P. Acta Metall Sin, 2004; 40: 135
(杨王玥, 齐俊杰, 孙祖庆, 杨平. 金属学报, 2004; 40: 135)
[26] Tsuzaki K, Sato E, Furimoto S, Furuhara T, Maki T. ScrMater, 1999; 40: 675 |