Abstract The addition of Nb was used to improve ductility during rolling process. The (Fe81Ga19)+1at.%Nb sheet with thickness of 0.6 mm was prepared by conventional rolling, including hot rolling and cold rolling. Results that demonstrate the rolled texture, recrystallization texture and magnetostriction of (Fe81Ga19)+1at.%Nb sheets are presented in this work. The as-rolled sheet had {111} and near {001}<110> rolling-texture grains, and had magnetostriction only as 26×10-6. A near {011}<100> texture and a {001}<100> texture were formed in recrystallized sheets which were water quenched after two hours annealed at 1250 °C and1300 °C, and their magnetostriction (3/2)s were 106×10-6and136×10-6 respectively.
[1]Guruswamy S,Srisukhumbowornchai N,Clark A E, Restorff J B,Wun-Fogle M.Scr Mater,2000;43:239 [2]Lograsso T A,Ross A R,Schlagel D L,Clark A E,Wun- Fogle M.J Alloys Compd,2003;350:95 [3]Cheng S F,Das B N,Wun-Fogle M,Lubitz P,Clark A E. IEEE Trans Magn,2002;38:2838 [4]Wun-Fogle M,Clark A E,Restorff J B.J Intell Mater Syst Struct,2006;17:117 [5]Kumagai A,Fujita A,Fukamichi K,Oikawa K,Kainuma R,Ishida K.J Magn Mater,2004;272-276:2060 [6]Clark A E,Wun-Fogle M,Restorff J B,Thomas A,Lo- grasso T A.Mater Trans,2002;43:881 [7]Han Z Y,Zhou S Z,Zhang M C,Gao X X.J Magn Mater Dev,2004;35(1):15 (韩志勇,周寿增,张茂才,高学绪.磁性材料及器件,2004;35(1):15) [8]Srisukhumbowornchai N,Guruswamy S.Metall Mater Trans,2004;35A:2963 [9]Na S M,Flatau A B.Proc SPIE,2005;5761:192 [10]Na S M,Flatau A B.Mater Res Soc Symp Proc,2006; 888:V06-07 [11]Yang W Y,Mao W M,Sun Z Q.Chin J Nonferrous Met, 1998;8:390 (杨王玥,毛卫民,孙祖庆.中国有色金属学报,1998;8:390) [12]Yu Y N.Principles of Physical Metallurgy.Beijing:Met- allurgical Industry Press,2000:463 (余永宁.金属学原理.北京:冶金工业出版社,2000:463)