Abstract The nano scratch process of a rigid diamond tip into Ni substrate has been studied by using molecular dynamcs simulation with EAM potential. Simulations are carried out to investigate the scratch depth effect on the friction force in the scrath process. Furthermore, microstructures around the tip are strongly depended on the scratch depth and dislocation loops can be formed with enough penetration depth. Also, present study reveals that stick-slip phenomenon results from dislocation emission and phonon dissipation. The sawtooth phenomena can be explained from the point that elastic energy stored in the stick process transforms to the dislocations beneath the tip, and then dissipates in the form of phonons, and finally forms the surface defects. Finally, effect of the sliding velocity is studied, which can be deduced from the simulation. The scratch velocity is the critical factor on the dislocation loop nucleation and evolution process. At the higher velocity, dislocation loop glide along slip lane downward to the bulk material. While at the lower velocity, dislocation loops beneath the tip will reaction with each other, and finnaly a large loop will be formed under the subsurface of the material. Plastic deformation will focus on the subsurface of the bulk material under low scratch velocity.
[1]Johnson K L.Contact Mechanics.New York:Cambridge University Press,1985:5 [2]Ernest R.Friction and Wear of Materials.New York: John Wiley and Sons Inc,1995:65 [3]Guo Y,Zhuang Z,Chen Z,Li X Y.Int J Solids Struct, 2007;44:1180 [4]Binquan L,Robbins M O.Nature,2005;435:929 [5]Hirano M,Shinjo K,Kaneko R,Murata Y.Phys Rev Lett, 1997;78:1448 [6]Martin D,Gertjan S,Namboodiri P,Joost W M,Jennifer A,Henny W.Phys Rev Lett,2004;92:126101 [7]Socoliuc A,Gnecco E,Maier S,Pfeiffer O,Baratoff A, Bennewitz R,Meyer E.Science,2006;313:207 [8]Cannara R J,Brukman M J,Cimatu K,Sumant A U, Baldelli S,Carpick R W.Science,2007;318:780 [9]Persson N J.Sliding Friction.Berlin:Springer,2000:165 [10]Sang Y,Dube M,Grant M.Phys Rev Lett,2001;87: 174301 [11]Ohno K,Nitta T,Nakamura J,Natori A.J Vac Sci Tech- nol,2004;22B:2026 [12]Fusco C,Fasolino A.Phys Rev,2005;71B:045413 [13]Nakamura J,Wakunami S,Naori A.Phys Rev,2005;72B: 235415 [14]Tomlinson G A.Philos Mag,1929;7:905 [15]Komanduri R,Chandrasekaran N,Raft L M.Wear,2000; 242:60 [16]Li J,Van Vliet K J,Zhu T,Yip S,Suresh S.Nature,2002; 418:307 [17]Li Q K,Zhang Y,Chu W Y.Acta Metall Sin,2004;40: 1238 (李启楷,张跃,褚武扬.金属学报,2004;40:1238) [18]Mulliah D,Kenny S D,Smith R.Phys Rev,2004;69B: 205407 [19]Lee Y,Park J Y,Kim S Y,Jun S,Im S.Mech Mater, 2005;37:1035 [20]Smith R,Mulliah D,Kenn S D,McGee E,Richter A, Gruner M.Wear,2005;259:459 [21]Cho M H,Kim S J,Lim D S,Jang H.Wear,2005;259: 1392 [22]Cheng D,Yan Z J,Yan L.Thin Solid Films,2007;515: 3698 [23]Wang H L,Wang X X,Wang Y,Liang H Y.Acta Metall Sin,2007;43:259 (王海龙,王秀喜,王宇,梁海弋.金属学报,2007;43:259) [24]Pei Q X,Lu C,Lee H P.Comput Mater Sci,2007;41:177 [25]Li B,Clapp P C,Rifkin J A,Zhang X M.J Appl Phys, 2001;90:3090 [26]Wang H,Hu Y Z,Zou K,Leng Y S.Sci China,2001;31A: 261 (王慧,胡元中,邹鲲,冷永胜.中国科学,2001;31A:261) [27]Cheng D,Yan Z J,Yan L.Acta Metall Sin,2006;42:1149 (程东,严志军,严立.金属学报,2006;42:1149) [28]Xu Z M,Huang P.Acta Phys Sin,2007;55:2427 (许中明,黄平.物理学报,2007;55:2427) [29]Mishin Y,Farkas D,Mehl M J,Papaconstantopoulos D A.Phys Rev,1999;59B:393 [30]Fang T H,Weng C I.Nanotechnology,2000;11:148 [31]Berendsen H J,Postma J P M,van Gunsteren W V,Di Nola A,Haak J R.J Chem Phys,1984;81:3684 [32]Honeycutt J D,Andersen H C.J Phys Chem,1987;91: 4950 [33]Humphrey W,Dalke A,Schulten K.J Mol Graphics,1996; 14:33 [34]Nicola L,Bower A F,Kim K S,Needlemana A,Giessenb E V.J Mech Phys Solids,2007;5:1120 [35]Fivel M C,Robertson C F,Canova G R,Boulanger L. Acta Mater,1998;46:6183 [36]Knap J,Ortiz M.Phys Rev Lett,2003;90:226102 [37]Bulatov V V,Cai W.Computer Simulations of Disloca- tions,London:Oxford University Press,2006:18