Interfacial Fatigue Spalling Behavior of TiN Films on High Speed Steel |
QIU Longshi1,2, ZHAO Jing1, PAN Xiaolong1( ), TIAN Feng1 |
1.Xi'an Rare Metal Materials Institute Co. , Ltd. , Xi'an 710016, China 2.State-Key Laboratory for Mechanical Behavior of Materials, Xi'an Jiaotong University, Xi'an 710049, China |
|
Cite this article:
QIU Longshi, ZHAO Jing, PAN Xiaolong, TIAN Feng. Interfacial Fatigue Spalling Behavior of TiN Films on High Speed Steel. Acta Metall Sin, 2021, 57(8): 1039-1047.
|
Abstract Performance and fatigue life of coating parts are seriously restricted by their interfacial fatigue property. Herein, TiN films were deposited on W6Mo5Cr4V2 steel substrates by multiarc ion plating. The interfacial fatigue failure mechanisms were studied by the rolling contact fatigue method. The results show that the interfacial fatigue failure mode is mainly film spalling. The fatigue cracks generated initially at the film/substrate interface proceed to the surface, resulting in film spalling. The interfacial maximum shear stress amplitude (Δτinter) is a key factor for controlling interfacial crack initiation and propagation. The evolution model built using Δτinter and critical cycles (N) can be used to determine interfacial fatigue performance and for life forecast. The interfacial fatigue property is determined using a film/substrate interface, and glow discharge cleaning and prefabricated metal layer before coating deposition can improve interface fatigue performance. The evaluation model based on Δτinter-N curves can effectively used to identify the differences in interface states. Selection of the film-spalling area ratios of 5% and 50% and failure probabilities of 30%, 60%, and 90% have little effect on the determination of film/substrate interfacial fatigue performance. The results provide important theoretical references for fatigue performance determination and lifespan prediction of coated bearings and other parts.
|
Received: 19 August 2020
|
|
Fund: Natural Science Basic Research Program of Shaanxi Province(2020JQ-924);Xi'an Postdoctoral Innovation Base Research Project |
About author: PAN Xiaolong, senior engineer, Tel: (029)86258754, E-mail: 919516928@qq.com
|
1 |
Stewart S, Ahmed R. Rolling contact fatigue of surface coatings—A review [J]. Wear, 2002, 253: 1132
|
2 |
Piao Z Y, Xu B S, Wang H D, et al. Investigation of fatigue failure prediction of Fe-Cr alloy coatings under rolling contact based on acoustic emission technique [J]. Appl. Surf. Sci., 2011, 257: 2581
|
3 |
Colombo D A, Echeverría M D, Laino S, et al. Rolling contact fatigue resistance of PVD CrN and TiN coated austempered ductile iron [J]. Wear, 2013, 308: 35
|
4 |
Mayrhofer P H, Mitterer C, Hultman L, et al. Microstructural design of hard coatings [J]. Prog. Mater. Sci., 2006, 51: 1032
|
5 |
Musil J. Hard nanocomposite coatings: Thermal stability, oxidation resistance and toughness [J]. Surf. Coat. Technol., 2012, 207: 50
|
6 |
Santecchia E, Hamouda A M S, Musharavati F, et al. Wear resistance investigation of titanium nitride-based coatings [J]. Ceram. Int., 2015, 41: 10349
|
7 |
Kuhn M, Gold P W, Loos J. Wear and friction characteristics of PVD-coated roller bearings [J]. Surf. Coat. Technol., 2004, 177-178: 469
|
8 |
Mutyala K C, Singh H, Evans R D, et al. Effect of deposition method on the RCF performance of CrxN thin film ball coatings [J]. Surf. Coat. Technol., 2016, 305: 176
|
9 |
Liu H X, Jiang Y H, Zhou R, et al. Rolling contact fatigue life and mechanical property of TiN film fabricated by plasma immersion ion implantation and deposition [J]. Acta Metall. Sin., 2008, 44: 325
|
|
刘洪喜, 蒋业华, 周 荣等. 等离子体浸没离子注入与沉积合成TiN薄膜的滚动接触疲劳寿命和机械性能 [J]. 金属学报, 2008, 44: 325
|
10 |
Qiu L S, Qiao G L, Ma F, et al. Study on residual stress modulation and mechanical properties of titanium nitride coatings [J]. J. Mech. Eng., 2017, 53(24): 42
|
|
邱龙时, 乔关林, 马 飞等. TiN薄膜的残余应力调控及力学性能研究 [J]. 机械工程学报, 2017, 53(24): 42
|
11 |
Oettel H, Wiedemann R. Residual stresses in PVD hard coatings [J]. Surf. Coat. Technol., 1995, 76-77: 265
|
12 |
Colombo D A, Echeverría M D, Dommarco R C, et al. Influence of TiN coating thickness on the rolling contact fatigue resistance of austempered ductile iron [J]. Wear, 2016, 350-351: 82
|
13 |
Colombo D A, Massone J M, Echeverría M D, et al. Rolling contact fatigue behavior of Ti/TiN coated ADI by cathodic arc deposition [J]. Ceram. Int., 2017, 43: 4263
|
14 |
Vera E E, Vite M, Gallardo E A, et al. Fatigue life of TiN and CrN coatings in rolling contact [J]. Proc. Inst. Mech. Eng., 2013, 227J: 339
|
15 |
Polonsky I A, Keer L M. Numerical analysis of the effect of coating microstructure on three-dimensional crack propagation in the coating under rolling contact fatigue conditions [J]. J. Tribol., 2002, 124: 14
|
16 |
Polonsky I A, Chang T P, Keer L M, et al. An analysis of the effect of hard coatings on near-surface rolling contact fatigue initiation induced by surface roughness [J]. Wear, 1997, 208: 204
|
17 |
Xu B S, Wang H D, Piao Z Y, et al. Investigation of structural integrity and life time prediction of the thermal sprayed alloy coating for remanufacturing [J]. Acta Metall. Sin., 2011, 47: 1355
|
|
徐滨士, 王海斗, 朴钟宇等. 再制造的热喷涂合金涂层的结构完整性与服役寿命预测研究 [J]. 金属学报, 2011, 47: 1355
|
18 |
Qiu L S, Zhu X D, Lu S, et al. Evaluation of hard-coating/substrate interfacial adhesion in rolling contact fatigue method under elastic-plastic deformation [J]. Chin. J. Vacuum Sci. Technol., 2015, 35: 1380
|
|
邱龙时, 朱晓东, 鲁 莎等. 基于弹塑性滚动接触疲劳法评价硬质薄膜结合强度 [J]. 真空科学与技术学报, 2015, 35: 1380
|
19 |
Qiu L S, Ma S L, Xu K W. Dynamicfailure mechanism and evaluation method of TiN hard coatings deposited by multi-arc ion plating (MAIP) [J]. Mater. Prot., 2014, 47(suppl.2): 109
|
|
邱龙时, 马胜利, 徐可为. 多弧离子镀制备TiN镀层的动态失效机制及评价方式 [J]. 材料保护, 2014, 47(): 109
|
20 |
Qiu L S, Zhu X D, Lu S, et al. Quantitative evaluation of bonding strength for hard coatings by interfacial fatigue strength under cyclic indentation [J]. Surf. Coat. Technol., 2017, 315: 303
|
21 |
Thornton J A. High rate thick film growth [J]. Ann. Rev. Mater. Sci., 1977, 7: 239
|
22 |
Xie Z H, Hoffman M, Munroe P, et al. Microstructural response of TiN monolithic and multilayer coatings during microscratch testing [J]. J. Mater. Res., 2007, 22: 2312
|
23 |
Piao Z Y, Xu B S, Wang H D, et al. A separation of experimental study on coatings failure signal responses under rolling contact [J]. Tribol. Int., 2011, 44: 1304
|
24 |
Hogmark S, Hedenqvist P. Tribological characterization of thin, hard coatings [J]. Wear, 1994, 179: 147
|
25 |
Way S. Pitting due to rolling contact [J]. J. Appl. Mech., 1935, 2: A49
|
26 |
Qiu L, Zhu X, He G, et al. The repeated spherical indentation test: An efficient way to evaluate the adhesion of hard coatings [J]. Surf. Eng., 2016, 32: 578
|
27 |
Qiu L S, Zhu X D, Xu K W. Internal stress on adhesion of hard coatings synthesized by multi-arc ion plating [J]. Surf. Coat. Technol., 2017, 332: 267
|
28 |
Zhang X C, Xu B S, Wang H D, et al. Hertzian contact response of single-layer, functionally graded and sandwich coatings [J]. Mater. Des., 2007, 28: 47
|
29 |
Gerth J, Wiklund U. The influence of metallic interlayers on the adhesion of PVD TiN coatings on high-speed steel [J]. Wear, 2008, 264: 885
|
No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
|
Shared |
|
|
|
|
|
Discussed |
|
|
|
|