Abstract In this paper, the method to determine characteristic atom sequences of binary alloy system was pointed out by taking Pt-Ru alloy system as an example. On the basis of lattice constants and heats of formation of experimental value, the energy and volume interaction optimum functions were chosen. The basic information of characteristic atom sequences was determined. The structures and properties of disordered and ordered alloy can be expounded and designed. The correlation between electronic structure and catalytic performance of Pt-Ru alloy was discussed. As the function of coordination of Ru, the potential energy decreases and stability increases. D-orbital vacancy increases and the lattice constants decrease. This lead to strengthen catalytic activity.
[1]Liu G H,Bao H,Li W C.Mater Rev,2001;15(8):10 (刘国华,包宏,李文超.材料导报,2001;15(8):10) [2]Xie Y Q.Mater Rev,2001;15(4):12 (谢佑卿.材料导报,2001;15(4):12) [3]Xie Y Q,Ma L Y.J Cent South Inst Mining Metall,1985; 8(1):1 (谢佑卿,马柳莺.中南矿冶学院学报,1985;8(1):1) [4]Xie Y Q.Sci China,1993;36A:90 [5]Xie Y Q.Chin Sci Bull,1992;37:1529 [6]Xie Y Q.Acta Metall Mater,1994;42:3705 [7]Xie Y Q.Sci China,1998;41E:146 [8]Xie Y Q,Zhang X D.Sci China,1998;41E:157 [9]Xie Y Q,Zhang X D.Sci China,1998;41E:225 [10]Xie Y Q,Peng K Liu X B.Physica,2004;344B:5 [11]Xie Y Q,Liu X B,Peng K,Peng H J.Physica,2004;353B: 15 [12]Xie Y Q,Peng H J,Liu X B,Peng K.Physica,2005;362B: 1 [13]Xie Y Q,Tao H J,Peng H J,Liu X B,Peng K.Physica, 2005;366B:17 [14]Yang X K,Li X,Heng G H.Acta Phys-Chim Sin,2007; 23:389 (杨喜昆,李昕,衡根华.物理化学学报,2007;23:389) [15]Arico A S,Antonucci P L,Modica E,Monforte G,Baglio V,Antonucci V.Electrochim Acta,2002;47:3723 [16]Gasteiger H,Ross P N,Caims T R.Surf Sci,1994;141: 1795