THE EXPERIMENTAL APPARATUS OF THE COUPLING OF FORCE, TEMPERATURE AND MAGNETIC FIELD
;;
吉林大学超塑性与塑性研究所
Cite this article: 

. THE EXPERIMENTAL APPARATUS OF THE COUPLING OF FORCE, TEMPERATURE AND MAGNETIC FIELD. Acta Metall Sin, 2008, 44(1): 69-73 .

Download:  PDF(211KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  The research on the coupling effect of force, temperature and magnetic field on material is one of front branches of material science. The paper introduces the principle and structure of the experimental apparatus of the coupling of force, temperature and magnetic field. The principle and structure of heating outside the furnace and dynamically sealing are advanced. According to this, the inert gases sealed in the furnace may effectively prevent the oxygenation of the specimen and the friction between the furnace mouse and pull bar. While applying the coupling effect of temperature and magnetic field, it is solved that the heated circular resistance wires interfere in the magnetic field of exciting coil. And so a new experiment means is provided for the research on the plasticity and superplasticity.
Key words:  force      temperature      magnetic field      coupling      
Received:  12 July 2007     
ZTFLH:  TG315  
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y2008/V44/I1/69

[1]Li S C.Chin J Mater Res,1998;12:314 (李世春.材料研究学报,1998;12:314)
[2]Li Y,Dong X H.Chin J Nonferrous Met,1996;6(3):151 (李尧,董晓华.中国有包金属学报,1996;6(3):151)
[3]Conrad H,Cao W D,Lu X P.Scr Metall,1989;23:697
[4]Conrad H,Cao W D,Lu X P.Mater Sci Eng,1991;A138: 247
[5]Cao W D,Lu X P,Sprecher A F.Mater Sci Eng,1990; A129:157
[6]Li S C,Conrad H.Scr Mater,1998;39:847
[7]Li M Q,Wn S D.Acta Metall Sin,1995;31:A272 (李淼泉,吴诗惇.金属学报,1995;31:A272)
[8]Li M Q,Liu Y L,Wu S C,Wu X W.J Mater Process Technol,1994;40:385
[9]Li M Q,Wu S C.J Mater Process Technol,1996;61:298
[10]Li M Q,Chen Y Y,Chen D J.J Mater Process Technol, 1998;73:264
[11]Liu B R,Zhang C B,Lai Z H.Chin J Mater Res,1999; 13:385 (刘渤然,张彩碚,赖祖涵.材料研究学报,1999;13:385)
[12]Liu B R,Zhang C B,Lai Z H.Chin J Mater Res,2000; 14:218 (刘渤然,张彩碚,赖祖涵.材料研究学报,2000;14:218)
[13]Li Y,Yang X Y,Chen H.J Hubei Univ Technol,1995; 10(1):1 (李尧,杨贤镛,陈洪.湖北工学院学报,1995;10(1):1)
[14]Li Y,Song Z K.Shanghai Nonferrous Met,1996;17(3): 103 (李尧,宋子凯.上海有色金属,1996;17(3):103)
[15]Li G,Zhu X C.J Chongqing Polytechnic College,2005; 15(2):30 (李钢,朱新才.重庆工业高等专科学校校报,2005;15(2):30)
[16]Song Y Q,Song J W,Guan X F.Chin Pat,ZL 200610017268.1,2006 (宋玉泉,朱家旺,管晓芳.中国发明号利,ZL 200610017268.1,2006)
[17]Song Y Q,Cheng Y C.Chin Pat,ZL 00117802.4,2000 (宋玉泉,程永春.中国发明专利,ZL 00117802.4,2000)?
[1] JIANG He, NAI Qiliang, XU Chao, ZHAO Xiao, YAO Zhihao, DONG Jianxin. Sensitive Temperature and Reason of Rapid Fatigue Crack Propagation in Nickel-Based Superalloy[J]. 金属学报, 2023, 59(9): 1190-1200.
[2] WANG Lei, LIU Mengya, LIU Yang, SONG Xiu, MENG Fanqiang. Research Progress on Surface Impact Strengthening Mechanisms and Application of Nickel-Based Superalloys[J]. 金属学报, 2023, 59(9): 1173-1189.
[3] SUN Rongrong, YAO Meiyi, WANG Haoyu, ZHANG Wenhuai, HU Lijuan, QIU Yunlong, LIN Xiaodong, XIE Yaoping, YANG Jian, DONG Jianxin, CHENG Guoguang. High-Temperature Steam Oxidation Behavior of Fe22Cr5Al3Mo-xY Alloy Under Simulated LOCA Condition[J]. 金属学报, 2023, 59(7): 915-925.
[4] WANG Fa, JIANG He, DONG Jianxin. Evolution Behavior of Complex Precipitation Phases in Highly Alloyed GH4151 Superalloy[J]. 金属学报, 2023, 59(6): 787-796.
[5] LIU Manping, XUE Zhoulei, PENG Zhen, CHEN Yulin, DING Lipeng, JIA Zhihong. Effect of Post-Aging on Microstructure and Mechanical Properties of an Ultrafine-Grained 6061 Aluminum Alloy[J]. 金属学报, 2023, 59(5): 657-667.
[6] CHENG Yuanyao, ZHAO Gang, XU Deming, MAO Xinping, LI Guangqiang. Effect of Austenitizing Temperature on Microstructures and Mechanical Properties of Si-Mn Hot-Rolled Plate After Quenching and Partitioning Treatment[J]. 金属学报, 2023, 59(3): 413-423.
[7] SHEN Zhao, WANG Zhipeng, HU Bo, LI Dejiang, ZENG Xiaoqin, DING Wenjiang. Research Progress on the Mechanisms Controlling High-Temperature Oxidation Resistance of Mg Alloys[J]. 金属学报, 2023, 59(3): 371-386.
[8] WANG Di, HE Lili, WANG Dong, WANG Li, ZHANG Siqian, DONG Jiasheng, CHEN Lijia, ZHANG Jian. Influence of Pt-Al Coating on Tensile Properties of DD413 Alloy at High Temperatures[J]. 金属学报, 2023, 59(3): 424-434.
[9] WANG Kai, JIN Xi, JIAO Zhiming, QIAO Junwei. Mechanical Behaviors and Deformation Constitutive Equations of CrFeNi Medium-Entropy Alloys Under Tensile Conditions from 77 K to 1073 K[J]. 金属学报, 2023, 59(2): 277-288.
[10] MIAO Junwei, WANG Mingliang, ZHANG Aijun, LU Yiping, WANG Tongmin, LI Tingju. Tribological Properties and Wear Mechanism of AlCr1.3TiNi2 Eutectic High-Entropy Alloy at Elevated Temperature[J]. 金属学报, 2023, 59(2): 267-276.
[11] ZHANG Limin, LI Ning, ZHU Longfei, YIN Pengfei, WANG Jianyuan, WU Hongjing. Macrosegregation Mechanism of Primary Silicon Phase in Cast Hypereutectic Al-Si Alloys Under Alternating Electropulsing[J]. 金属学报, 2023, 59(12): 1624-1632.
[12] XU Wenguo, HAO Wenjiang, LI Yingju, ZHAO Qingbin, LU Bingyu, GUO Heyi, LIU Tianyu, FENG Xiaohui, YANG Yuansheng. Effects of Trace Aluminum and Titanium on High Temper-ature Oxidation Behavior of Inconel 690 Alloy[J]. 金属学报, 2023, 59(12): 1547-1558.
[13] SU Zhenqi, ZHANG Congjiang, YUAN Xiaotan, HU Xingjin, LU Keke, REN Weili, DING Biao, ZHENG Tianxiang, SHEN Zhe, ZHONG Yunbo, WANG Hui, WANG Qiuliang. Formation and Evolution of Stray Grains on Remelted Interface in the Seed Crystal During the Directional Solidification of Single-Crystal Superalloys Assisted by Vertical Static Magnetic Field[J]. 金属学报, 2023, 59(12): 1568-1580.
[14] CHEN Jilin, FENG Guanghong, MA Honglei, YANG Dong, LIU Wei. Microstructure, Mechanical Properties, and Strengthening Mechanism of Cr-Mo Microalloy Cold Heading Steel[J]. 金属学报, 2022, 58(9): 1189-1198.
[15] XIE Leipeng, SUN Wenyao, CHEN Minghui, WANG Jinlong, WANG Fuhui. Effects of Processing on Microstructures and Properties of FGH4097 Superalloy[J]. 金属学报, 2022, 58(8): 992-1002.
No Suggested Reading articles found!